# US 2023/0313455 A1 · Process for production of cellulose nanofibers from miscanthus x. giganteus and composites therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0313455 A1
- Document ID: US20230313455A1
- Status: Published application
- Kind: A1
- Application number: 17/291,803
- Filed: 2019-10-31
- Published: 2023-10-05
- Earliest claimed: 2018-04-18
- Assignees: The University of Chicago
- Applicants: The University of Chicago
- Inventors: Stuart J. ROWAN; Han YANG
- Web page: https://patentgrep.com/patent/US20230313455A1

## CPC

- D21C 9/004: {inorganic compounds}
- D21C 3/022: {in presence of S-containing compounds}
- D21C 9/06: in filters {; Washing of concentrated pulp, e.g. pulp mats, on filtering surfaces}
- D21C 9/1047: {Conserving the bleached pulp}
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR

## Abstract

A process for the isolation of cellulose nanofibers, in particular carboxylic acid functionalized cellulose nanofibers (MxG-CNF-CO2H) from the sustainable grass hybrid Miscanthus x. giganteus (MxG). The process includes the steps of performing bleach treatment on a quantity of MxG followed by ammonium persulfate oxidation. The resulting MxG-CNF-CO2Hs have good dispersibility in aqueous and polar organic solvents. They are also able to form gels at relatively low concentrations. The MxG-CNF-CO2H show significantly higher reinforcement effect when compared to carboxylic acid functionalized cellulose nanocrystals at the same weight percent in a composite composition.

## Claims

### Claim 1

A process for preparing cellulose nanofibers from Miscanthus x. giganteus (MxG), comprising the steps of:
performing a bleaching step on a quantity of the MxG; and
thereafter subjecting a solid material obtained from the bleaching step to ammonium persulfate oxidation and obtaining carboxylic acid functionalized cellulose nanofibers, MxG-CNF-CO2H.

### Claim 2 (depends on 1)

The process according to claim 1, further including the step of obtaining the quantity of the MxG and reducing a particle size thereof to a smaller average particle size.

### Claim 3 (depends on 2)

The process according to claim 2, wherein the reduced average particle size is less than 500 μm.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the bleaching step comprises contacting the MxG with a bleaching solution comprising an oxidizing agent and one or more of an acid and an acid liberating agent.

### Claim 5 (depends on 4)

The process according to claim 4, wherein the oxidizing agent comprises one or more of sodium chlorite, sodium hypochlorite, calcium hypochlorite and hydrogen peroxide.

### Claim 6 (depends on 5)

The process according to claim 5, wherein the concentration of the oxidizing agent ranges from about 2 wt. % to about 4 wt. % based on the total weight of the bleaching solution.

### Claim 7 (depends on 4)

The process according to claim 4, wherein the pH of the bleaching solution is between about 4 and about 6.

### Claim 8 (depends on 6)

The process according to claim 6, wherein the bleaching step is performed at a temperature between 60° C. and 80° C. for an amount of time sufficient to convert lignins present in the MxG.

### Claim 9 (depends on 1)

The process according to claim 1, wherein after the bleaching step has been performed, the MxG-containing bleaching solution is filtered, washed and dried prior to subjecting the solid material obtained from the bleaching step to ammonium persulfate oxidation.

### Claim 10 (depends on 1)

The process according to claim 1, wherein the ammonium persulfate oxidation step includes contacting the solid material obtained from the bleaching step with an ammonium persulfate solution having a concentration from about 0.5 M to about 2.0 M.

### Claim 11 (depends on 10)

The process according to claim 10, wherein the ammonium persulfate solution containing the solid material is mixed fora suitable period of time in order to oxidize the solid material to form the MxG-CNF-CO2H.

### Claim 12 (depends on 11)

The process according to claim 11, wherein the mixing is performed at a temperature between about 50° C. to about 90° C.

### Claim 13 (depends on 12)

The process according to claim 12, wherein the oxidation process is performed for about 8 hours to about 24 hours.