# US 2023/0311272 A1 · Grinding method using nanolayer-lubricated diamond grinding wheel based on shock wave cavitation effect

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0311272 A1
- Document ID: US20230311272A1
- Status: Published application
- Kind: A1
- Application number: 18/119,297
- Filed: 2023-03-09
- Published: 2023-10-05
- Earliest claimed: 2020-09-14
- Assignees: Hunan Institute of Science and Technology
- Applicants: Hunan Institute of Science and Technology
- Inventors: CHAO LI; XIAOHONG ZHANG; ZHAOYAO SHI; YUEJIAO DING; LIWEI NING; XIAOHONG TANG; SONGHUI ZHANG; WEI LI; WANYI TIAN
- Web page: https://patentgrep.com/patent/US20230311272A1

## CPC

- B24B 55/03: designed as a complete equipment for feeding or clarifying coolant
- B24C 5/08: Devices for generating abrasive blasts non-mechanically, e.g. of metallic abrasives by means of a magnetic field {or by detonating cords}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL

## Abstract

The present invention provides a nanolayer-lubricated diamond grinding wheel grinding method based on a shock wave cavitation effect. In the method, after a gas pressure regulation valve is turned on, a shock wave generated by an acceleration tube pushes nanoparticles to move forward, and the nanoparticles are then accelerated by a small de Laval nozzle to acquire a high initial velocity. One wave source of a shock wave speed-increase module generates a high-frequency high-strength shock wave, to impact nanoparticles with an initial velocity, to enable the nanoparticles to be continuously accelerated downward in an axial direction of a large de Laval nozzle, until the nanoparticles are embedded on a grinding wheel surface at a maximum speed to form a nanolayer. The other wave source is used to clean impurities on the grinding wheel surface. In a processing process, the nanoparticles of the nanolayer are autonomously released in a core grinding region, to implement self-lubrication and cooling inside the grinding region. This method significantly enhances lubrication and cooling effects and satisfies the green development idea.

## Claims

### Claim 1

A grinding method using nanolayer-lubricated diamond grinding wheel based on a shock wave cavitation effect, wherein the method includes:
step S1. generating compressed gas and storing the compressed gas in a gas tank;
step S2. inputting the compressed gas into a gas acceleration tube, which has a push plate, a high pressure chamber and a low pressure chamber; inputting nanoparticles into the low pressure chamber and inputting compressed gas into the high pressure chamber, in which the compressed gas is further pressurized by the push plate until pressure of the compressed gas reaches a first preset threshold;
Step S3. Opening the high pressure chamber, so that the compressed gas is delivered to the low pressure chamber with a streamline tightening structure to push the nanoparticles therein to a second wave focusing device;
Step S4. setting two shock wave sources, a first shock wave source and a second shock wave source, which are both facing towards the grind wheel;
Step S5. generating shock waves in sequence with the two shock wave sources, wherein the first shock wave source generates shock waves and enhance the shock waves using a first wave focusing device in front of the second shock wave source, and the second shock wave source generates shock waves and brings the nanoparticles in the second wave focusing device to impact the grind wheel;
Step S6. forming a uniformly distributed nanolayer on the grinding wheel surface by using the shock waves.

### Claim 2 (depends on 1)

The grinding method of claim 1,
wherein step 51 includes: turning on a gas pump to suck gas after a workpiece to be grinded is fixed at a workpiece fixing plate of a workbench, wherein the gas is compressed into a gas tank through a gas-guide tube, and when a gas pressure detector detects that gas pressure in the gas tank satisfies the first preset threshold, the gas pump is stopped, or else, the gas pump goes on working; and after the gas pump and the gas tank start to work, turning on a powder delivery switch, so that nanoparticles stored in a detachable sealed powder delivery box is delivered into the low-pressure chamber.

### Claim 3 (depends on 2)

The grinding method of claim 2, wherein step S2 includes: turning on a gas pressure regulation valve, so that the compressed gas in the gas tank enters a movable chamber in an acceleration tube through a gas inlet tube, to push a push plate to compress a gas in a high-pressure chamber; and turning on a gas pressure sensing switch after sensing that a gas pressure of the high-pressure chamber satisfies a second preset threshold, so that the compressed gas in the high-pressure chamber enters the low-pressure chamber to generate a shock wave.

### Claim 4 (depends on 3)

The grinding method of claim 3, wherein step S3 includes: turning on a movable switch so that the generated shock wave passes through a streamlined narrowing structure of the low-pressure chamber to form a pulse enhanced shock wave to push the nanoparticles to move forward, and then the nanoparticles is further accelerated by a small de Laval nozzle, so that the nanoparticles acquire an initial velocity.

### Claim 5 (depends on 4)

The grinding method of claim 4, wherein step S4 includes: connecting an electromagnetic coil to a bipolar high-pressure pulse current to enable the electromagnetic coil to generate a bidirectional electromagnetic force, to push an impact ball to start to reciprocate in a semicircular annular pipe, and to strike back and forth on the impact heads at two ends of the semicircular annular pipe at a high speed to generate high-frequency ballistic shock waves at each end, thus forming the two shock wave sources, a first shock wave source and a second shock wave source,
wherein strength of the shock waves is then improved under the action of a wave focusing device; and when the impact ball strikes the impact heads at two ends of the semicircular annular pipe back and forth, making a heat sink start to operate.

### Claim 6 (depends on 5)

The grinding method of claim 5, wherein step S5 includes: generating shock wave continually, wherein a shock wave of the first shock wave source directly impacts a grinding wheel surface to generate a cavitation effect to clean impurities on the grinding wheel surface, and also provides a condition for subsequent formation of a nanolayer; a shock wave of the second shock wave source impacts the nanoparticles with a high initial velocity, to provide the nanoparticles with a higher speed; and subsequent shock waves continuously increase speed of the nanoparticles, so that the nanoparticles are continuously accelerated downward in an axial direction of the large de Laval nozzle by using a Laval effect of a large de Laval nozzle, until the nanoparticles impact the grinding wheel surface at a maximum speed.

### Claim 7 (depends on 1)

The grinding method of claim 1, wherein the grinding method uses a diamond grinding wheel with a metal binder layer thereon, wherein the metal binder is a bronze binder and the nanoparticles are metal nanoparticles.

### Claim 8 (depends on 7)

The grinding method of claim 7, wherein the metal nanoparticles includes ferric oxide magnetic nanoparticles, with sizes ranging from 50 nm to 100 nm.

### Claim 9 (depends on 1)

The grinding method of claim 1, wherein the compressed gas in the gas tank is air, and the first preset threshold ranges from 2.0 MPa to 8.0 MPa; and the structure of the acceleration tube in the acceleration module is of a streamlined narrowing type to enhance the generated shock wave, and a gas flow rate of the acceleration tube ranges from 320 m/s to 1200 m/s, to ensure that the nanoparticles acquire the high initial velocity.

### Claim 10 (depends on 9)

The grinding method of claim 9, wherein the method includes: adjusting the positions of the two wave focusing device, inducing that the first shock wave source generates low-strength high-frequency shock waves, to directly impact the grinding wheel surface to generate a cavitation effect to clean the impurities on the grinding wheel surface, and using the second shock wave source to form a high-strength high-frequency shock wave, to continuously increase the speed of the nanoparticles, until the nanoparticles impact the grinding wheel surface at a final speed ranging from 4200 m/s to 6800 m/s to form the nanolayer, wherein the thickness of the nanolayer ranges from 5 μm to 15 μm.