# US 2023/0291072 A1 · Large-dimension, flexible, ultrathin high-conductivity polymer-based composite solid-state electrolyte membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0291072 A1
- Document ID: US20230291072A1
- Status: Published application
- Kind: A1
- Application number: 18/198,238
- Filed: 2023-05-16
- Published: 2023-09-14
- Earliest claimed: 2021-07-30
- Assignees: Solid Energies Inc.
- Applicants: Solid Energies Inc.
- Inventors: Zhigang Lin; Tianyu Meng
- Web page: https://patentgrep.com/patent/US20230291072A1

## CPC

- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 50/211: adapted for pouch cells
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 50/491: Porosity
- H01M 50/105: Pouches or flexible bags
- H01M 50/417: Polyolefins
- H01M 2300/0065: Solid electrolytes
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Fabricating a composite solid-state electrolyte (SSE) membrane by infiltrating a porous polymer substrate with a mixture which comprises: (i) polymer precursor, (ii) ceramic nanoparticles with diameters that range from 10 to 2000 nm, (iii) plasticizer and (iv) lithium salt. Curing the mixture yields a solid-state electrolyte which is formed within pores of the substrate. A continuous roll-to-roll system for manufacturing of large-dimension, flexible, ultrathin, high ionic conductivity (SSE) membrane advances a porous polymer substrate through a coating module, multifunctional module for post-treatment curing and calendar unit. The SSE membrane is used in all solid-state lithium-ion electrochemical pouch cells. The SSE membrane exhibits high ionic conductivity over wide temperature range, especially high value in low temperature (−40° C.).

## Claims

### Claim 1

A composite solid-state electrolyte membrane which comprises a porous polymer substrate which is formed of a first polymer and has a porosity of 30 to 70% and has a solid-state electrolyte formed in pores of the substrate wherein the solid-state electrolyte comprises a polymer network formed of a second polymer with ceramic nanoparticles and lithium salt distributed in the network.

### Claim 2 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 wherein the substrate has an average pore size of about 0.01 μm to 0.3 μm.

### Claim 3 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 wherein the first polymer is polyethylene, polypropylene, or a composite of polyethylene and polypropylene.

### Claim 4 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 wherein the second polymer is PEGDA or p(VDF-HFP).

### Claim 5 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 wherein porous polymer substrate has a first planar surface and a second planar surface and wherein the solid-state electrolyte defines a first exposed layer that extends from the first planar surface and a second exposed layer that extends from the second planar surface.

### Claim 6 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 which is fabricated by a method that comprises:
(a) providing a porous polymer substrate having pores;
(b) infiltrating the pores of the porous polymer substrate with a solid electrolyte precursor mixture which comprises: (i) a polymer precursor, (ii) ceramic nanoparticles with diameters that range from 10 to 2000 nm, (iii) a plasticizer and (iv) a lithium salt; and
(c) curing the mixture to yield a solid-state electrolyte which is formed within pores of the substrate.

### Claim 7 (depends on 6)

The composite solid-state electrolyte membrane of claim 6 wherein the solid-electrolyte precursor mixture includes PEGDA and a photoinitiator and step (c) comprises exposing the mixture to ultra-violet radiation to crosslink the PEGDA to form a polymer network in the solid-state electrolyte.

### Claim 8 (depends on 6)

The composite solid-state electrolyte membrane of claim 6 wherein the solid-electrolyte precursor mixture includes P(VDF-HFP) and step (c) comprises heating the mixture to vaporize excess plasticizer to form a polymer network in the solid-state electrolyte.

### Claim 9 (depends on 6)

The composite solid-state electrolyte membrane of claim 6 wherein the ceramic nanoparticles are selected from the group consisting of ceramic materials having the basic formula Li7La3Zr2O12 (LLZO) and derivatives thereof wherein at least one of Al, Ta, or Nb is substituted in Zr sites of the Li7La3Zr2O12.

### Claim 10 (depends on 6)

The composite solid-state electrolyte membrane of claim 6 wherein the porous polymer substrate comprises a porous polymer membrane having a porosity of 30 to 70%.

### Claim 11 (depends on 1)

The composite solid-state electrolyte membrane of claim 1 wherein the membrane exhibits an ionic conductivity of above 0.6 mS/cm at a temperature range of 20° C. to 90° C. and an ionic conductivity of above 0.01 mS/cm at a temperature range of −40° C. to 10° C.

### Claim 12

An electrochemical cell which comprises one or more unit cells, wherein each unit cells comprises: an anode; a cathode; and interposed therebetween a solid-electrolyte which comprises a composite solid-state electrolyte membrane which comprises a porous polymer substrate which is formed of a first polymer and has a porosity of 30 to 70% and has a solid-state electrolyte formed in pores of the substrate wherein the solid-state electrolyte comprises a polymer network formed of a second polymer with ceramic nanoparticles and lithium salt distributed in the network.

### Claim 13 (depends on 12)

The electrochemical cell of claim 12 wherein the one or more unit cells are connected to an anode electrode tab and a cathode electrode tab and are enclosed in a flexible shell in the form of a pouch.

### Claim 14 (depends on 13)

The electrochemical cell of claim 13 comprising a plurality of unit cells that are stacked together in tandem.

### Claim 15 (depends on 12)

The electrochemical cell of claim 12 wherein the composite solid-state electrolyte membrane is fabricated by a method that comprises:
(a) providing a porous polymer substrate having pores;
(b) infiltrating the pores of the porous polymer substrate with a solid electrolyte precursor mixture which comprises: (i) a polymer precursor, (ii) ceramic nanoparticles with diameters that range from 10 to 2000 nm, (iii) a plasticizer and (iv) a lithium salt; and
(c) curing the mixture to yield a solid-state electrolyte which is formed within pores of the substrate.

### Claim 16 (depends on 15)

The electrochemical cell of claim 15 wherein the solid-electrolyte precursor mixture includes PEGDA and a photoinitiator and step (c) comprises exposing the mixture to ultra-violet radiation to crosslink the PEGDA to form a polymer network in the solid-state electrolyte.

### Claim 17 (depends on 15)

The electrochemical cell of claim 15 wherein the solid-electrolyte precursor mixture includes P(VDF-HFP) and step (c) comprises heating the mixture to vaporize excess plasticizer to form a polymer network in the solid-state electrolyte.

### Claim 18 (depends on 15)

The electrochemical cell of claim 15 wherein the ceramic nanoparticles are selected from the group consisting of ceramic materials having the basic formula Li7La3Zr2O12 (LLZO) and derivatives thereof wherein at least one of Al, Ta, or Nb is substituted in Zr sites of the Li7La3Zr2O12.

### Claim 19 (depends on 15)

The electrochemical cell of claim 15 wherein the porous polymer substrate comprises a porous polymer membrane having a porosity of 30 to 70%.

### Claim 20 (depends on 12)

The electrochemical cell of claim 12 wherein the membrane exhibits an ionic conductivity of above 0.6 mS/cm at a temperature range of 20° C. to 90° C. and an ionic conductivity of above 0.01 mS/cm at a temperature range of −40° C. to 10° C.