# US 2023/0282424 A1 · Controlled heating rate baking protocol for the synthesis of bismuth vanadate thin films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0282424 A1
- Document ID: US20230282424A1
- Status: Published application
- Kind: A1
- Application number: 18/176,786
- Filed: 2023-03-01
- Published: 2023-09-07
- Earliest claimed: 2022-03-02
- Assignees: City University of Hong Kong
- Applicants: City University of Hong Kong
- Inventors: Ruiqin Zhang; Rafiqat Ui Rasool
- Web page: https://patentgrep.com/patent/US20230282424A1

## CPC

- H01G 9/0029: {Processes of manufacture}
- H01G 9/2027: {comprising an oxide semiconductor electrode}
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- C23C 18/1245: {Inorganic substrates other than metallic}
- C23C 18/127: {Preformed particles}
- C23C 18/1283: {Control of temperature, e.g. gradual temperature increase, modulation of temperature}
- H01G 9/2004: {characterised by the electrolyte, e.g. comprising an organic electrolyte}
- H01G 9/205: {comprising a semiconductor electrode comprising AIII-BV compounds with or without impurities, e.g. doping materials}
- C23C 18/1254: {Sol or sol-gel processing}
- Y02E 10/542: Dye sensitized solar cells
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for fabricating a film on a substrate and a method for controlling the heating rate of a plurality of nanoparticles to transform the plurality of nanoparticles into a plurality of nanorods and nano-cone structures includes the steps of providing a sol precursor, providing a substrate, depositing the sol precursor onto the substrate via a sol-gel technique, annealing the sol precursor under ambient pressure at a controlled heating rate, and cooling down the sol precursor to form a film.

## Claims

### Claim 1

A method for fabricating a film on a substrate comprising the steps of,
(a) providing a sol precursor;
(b) providing a substrate;
(c) depositing the sol precursor onto the substrate via a sol-gel technique;
(d) annealing the sol precursor under ambient pressure at a controlled heating rate; and
(e) cooling down the sol precursor to form the film.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the precursor comprises a metal oxide, wherein the metal oxide is selected from the group consisting essentially of bismuth vanadate, zinc oxide, iron oxide, and a combination thereof.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the substrate comprises an adhesive base, wherein the adhesive base is selected from the group consisting essentially of FTO glass, ITO glass, plain glass, and a combination thereof.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the sol-gel technique comprises a coating step, wherein the coating step is selected from the group consisting essentially of spin coating, dip coating, and a combination thereof.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the annealing step occurs in a muffle furnace at a temperature of from about 400° C. to about 550° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the annealing step takes from about 0.5 hours to about 5 hours.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the controlled heating rate is from about 10° C./min to about 70° C./min.

### Claim 8 (depends on 1)

A photoelectrode comprising a film and a substrate, wherein the film is fabricated according to the method of claim 1.

### Claim 9 (depends on 9)

The photoelectrode according to claim 9, wherein the film comprises a nanostructure, preferably selected from the group consisting essentially of a nanorod, a nano-cone structure, and a combination thereof.

### Claim 10

A method for controlling the heating rate of a plurality of nanoparticles to transform the plurality of nanoparticles into a plurality of nanorod and nano-cone structures comprising the steps of,
(a) providing a sol precursor comprising a plurality of nanoparticles;
(b) providing a substrate;
(c) depositing the sol precursor onto the substrate via a sol-gel technique to form a plurality of densely stacked nanoparticles;
(d) annealing the sol precursor at a controlled heating rate, wherein the controlled heating rate is from about 10° C./min to about 70° C./min, or about 60° C./min; and
(e) cooling down the sol precursor to form a plurality of nanorod and nano-cone structures.