# US 2023/0279164 A1 · Polymerization Method Of Ultra High Molecular Weight Polyethylene And Method For Preparing Catalyst Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0279164 A1
- Document ID: US20230279164A1
- Status: Published application
- Kind: A1
- Application number: 18/098,178
- Filed: 2023-01-18
- Published: 2023-09-07
- Earliest claimed: 2022-01-18
- Assignees: Hanwha Totalenergies Petrochemical Co., Ltd.
- Applicants: Hanwha Totalenergies Petrochemical Co., Ltd.
- Inventors: Seung Yeop LEE; Jin Woo LEE
- Web page: https://patentgrep.com/patent/US20230279164A1

## CPC

- C08F 110/02: Ethene
- C08F 4/6026: {containing aluminium}
- C08F 4/6226: {containing aluminium}
- C08F 2410/03: Multinuclear procatalyst, i.e. containing two or more metals, being different or not
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present disclosure provides a method for polymerizing ultra-high molecular weight polyethylene and a method for preparing the catalyst thereof by reacting a main catalyst, a cocatalyst mixed with two or more types of organoaluminum, and an organosilane compound in the polymerization of ultra-high molecular weight polyethylene to have high activity, high bulk density, and high molecular weight while simultaneously having low particle agglomeration.

## Claims

### Claim 1

A method for polymerizing ultra-high molecular weight polyethylene, the method comprising: reacting a main catalyst including a titanium active site, an organoaluminum cocatalyst mixed with two or more types of organoaluminum, and an organosilane compound to polymerize ultra-high molecular weight polyethylene.

### Claim 2 (depends on 1)

The method for polymerizing ultra-high molecular weight polyethylene of claim 1, wherein the main catalyst is a Ziegler-Natta-based catalyst in which titanium is supported on magnesium dichloride (MgCl2).

### Claim 3 (depends on 2)

The method for polymerizing ultra-high molecular weight polyethylene of claim 2, wherein the main catalyst is prepared by the following method comprising:
a first step of preparing a magnesium compound solution by reacting the magnesium dichloride (MgCl2) with an alcohol;
a second step of preparing a precursor by reacting the magnesium compound solution with titanium tetrachloride; and
a third step of preparing a catalyst by primary-reacting the precursor with titanium tetrachloride, and then reacting the result with a diester compound represented by the following Formula 1;
R1OOCR2COOR3 [Formula 1]
wherein R1 and R3 are a linear or branched alkyl group having 1 to 10 carbon atoms, and R2 is a hydrocarbon having 1 to 20 carbon atoms.

### Claim 4 (depends on 1)

The method for polymerizing ultra-high molecular weight polyethylene of claim 1, wherein a solvent used for polymerizing the ultra-high molecular weight polyethylene is one of linear, branched and cyclic saturated hydrocarbons.

### Claim 5 (depends on 1)

The method for polymerizing ultra-high molecular weight polyethylene of claim 1, wherein the organoaluminum cocatalyst used for polymerizing the ultra-high molecular weight polyethylene includes a mixture of two or more having a structure represented by AlRnX3-n (n is 1 to 3, R is a linear or branched alkyl group having 1 to 8 carbon atoms, and X is a halogen atom such as F, Cl, and Br, or a hydrogen atom).

### Claim 6 (depends on 5)

The method for polymerizing ultra-high molecular weight polyethylene of claim 5, wherein the amount of the organoaluminum cocatalyst is 0.1 to 100 moles of aluminum atoms of the cocatalyst per mole of titanium atoms of the main catalyst.

### Claim 7 (depends on 1)

The method for polymerizing ultra-high molecular weight polyethylene of claim 1, wherein the organosilane compound used for polymerizing the ultra-high molecular weight polyethylene is a compound represented by the following Formula 2:
wherein R4, R5, R6, and R7 are each independently a linear, branched and cyclic alkyl group having 1 to 20 carbon atoms, alkoxy group having 1 to 20 carbon atoms, aryl group having 6 to 20 carbon atoms, and alkyl group having 1 to 20 carbon atoms including a hetero atom.

### Claim 8 (depends on 7)

The method for polymerizing ultra-high molecular weight polyethylene of claim 7, wherein the amount of the organosilane compound is 0.2 to 50 moles per mole of titanium atoms of the main catalyst.

### Claim 9 (depends on 1)

The method for polymerizing ultra-high molecular weight polyethylene of claim 1, wherein the polymerization reaction during polymerizing the ultra-high molecular weight polyethylene is performed under a pressure condition of 1 to 60 kg/cm2 G and a temperature condition of 60 to 95° C. for the residence time of the reactant of 1 to 4 hours.

### Claim 10

A method for preparing a main catalyst for ultra-high molecular weight polyethylene polymerization by reacting a main catalyst including a titanium active site, an organoaluminum cocatalyst mixed with two or more types of organoaluminum, and an organosilane compound, the method comprising:
a first step of preparing a magnesium compound solution by reacting the magnesium dichloride (MgCl2) with an alcohol;
a second step of preparing a precursor by reacting the magnesium compound solution with titanium tetrachloride; and
a third step of preparing a catalyst by primary-reacting the precursor with titanium tetrachloride, and then reacting the result with a diester compound represented by the following Formula 1;
R1OOCR2COOR3 [Formula 1]
wherein R1 and R3 are a linear or branched alkyl group having 1 to 10 carbon atoms, and R2 is a hydrocarbon having 1 to 20 carbon atoms.

### Claim 11

An ultra-high molecular weight polyethylene having polymerization activity of 5 to 40 kg-PE/g-catalyst, the viscosity average molecular weight of 2.0 to 10.0×106 g/ml, the bulk density of 0.30 to 0.50 g/ml, and particle aggregation having 1 μm or more of 8.0 wt % or less.

### Claim 12 (depends on 11)

The ultra-high molecular weight polyethylene of claim 11, wherein the average particle size is 100 to 150 μm.