# US 2023/0278909 A1 · Copper ion-doped polychromatic fluorescent glass and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0278909 A1
- Document ID: US20230278909A1
- Status: Published application
- Kind: A1
- Application number: 17/780,525
- Filed: 2021-06-29
- Published: 2023-09-07
- Earliest claimed: 2021-05-11
- Assignees: Sun Yat-Sen University
- Applicants: Sun Yat-Sen University
- Inventors: Jing WANG; Shuaichen SI; Weijiang GAN
- Web page: https://patentgrep.com/patent/US20230278909A1

## CPC

- C03C 3/062: with less than 40% silica by weight
- C03B 5/06: in pot furnaces {(C03B5/02 takes precedence)}
- C03B 5/16: Special features of the melting process; Auxiliary means specially adapted for glass-melting furnaces
- C03B 11/122: {Heating}
- C03C 4/12: for luminescent glass; for fluorescent glass
- C09K 11/58: containing copper, silver or gold
- H10H 20/8512: {Wavelength conversion materials}
- H10H 20/0361: {of wavelength conversion means}
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

A copper ion-doped polychromatic fluorescent glass and a preparation method and use thereof are provided. The fluorescent glass has a chemical formula shown as the following: aP2O5-bSiO2-cZnO-dCs2CO3-eNaCl-fCuCl, wherein a, b, c, d, e, and f in the formula represent the molar coefficients of compounds, wherein a is 45 to 65, b is 10 to 30, c is 1 to 5, d is 5 to 20, e is 5 to 20, f is 0.1 to 5. The fluorescent can achieve blue, orange and near-infrared photoluminescence under the UV light with higher fluorescent quantum yield.

## Claims

### Claim 1

A copper ion-doped polychromatic fluorescent glass, wherein it has a chemical formula shown as the following:
aP2O5-bSiO2-cZnO-dCs2CO3-eNaCl-fCuCl,
wherein a, b, c, d, e, and f in the formula represent the molar coefficients of compounds, wherein a is 45 to 65, b is 10 to 30, c is 1 to 5, d is 5 to 20, e is 5 to 20, f is 0.1 to 5.

### Claim 2 (depends on 1)

The copper ion-doped polychromatic fluorescent glass according to claim 1, wherein in the fluorescent glass, d is 5 to 10, f is 0.1 to 0.5, or d is 8 to 15, f is 2 to 3, or d is 10 to 20, f is 0.3 to 1.

### Claim 3 (depends on 1)

A preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 1, wherein the preparation method comprises the following steps:
step S1, weighing P2O5, SiO2, ZnO, Cs2CO3, NaCl, CuCl and a reductant, and sufficiently grinding and mixing to form a mixture;
step S2, under a reducing atmosphere, melting the mixture at 1000° C. to 1300° C. for 5 to 60 minutes; and
step S3, pouring the melted mixture into a preheated mold, then annealing, cooling, cutting and polishing, thus obtaining the copper ion-doped polychromatic fluorescent glass.

### Claim 4 (depends on 3)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 3, wherein in step S2, temperature of the melting is 1050° C. to 1200° C.

### Claim 5 (depends on 3)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 3, wherein in step S2, the melting lasts for 10 to 30 minutes.

### Claim 6 (depends on 3)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 3, wherein in step S2, the reducing atmosphere is provided by carbon blocks.

### Claim 7 (depends on 3)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 3, wherein in step S3, temperature of the annealing is 320° C. to 450° C.

### Claim 8 (depends on 1)

Use of the copper ion-doped polychromatic fluorescent glass according to claim 1 in luminescence conversion materials.

### Claim 9 (depends on 8)

The use according to claim 8, wherein the use of the copper ion-doped polychromatic fluorescent glass in single host white-light illumination, near-infrared venography, infrared night-vision scope or food testing.

### Claim 10 (depends on 1)

A LED device, comprising a photoconverter and a LED chip, wherein the photoconverter comprises the copper ion-doped polychromatic fluorescent glass according to claim 1.

### Claim 11 (depends on 2)

A preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 2, wherein the preparation method comprises the following steps:
step S1, weighing P2O5, SiO2, ZnO, Cs2CO3, NaCl, CuCl and a reductant, and sufficiently grinding and mixing to form a mixture;
step S2, under a reducing atmosphere, melting the mixture at 1000° C. to 1300° C. for 5 to 60 minutes; and
step S3, pouring the melted mixture into a preheated mold, then annealing, cooling, cutting and polishing, thus obtaining the copper ion-doped polychromatic fluorescent glass.

### Claim 12 (depends on 11)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 11, wherein in step S2, temperature of the melting is 1050° C. to 1200° C.

### Claim 13 (depends on 11)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 11, wherein in step S2, the melting lasts for 10 to 30 minutes.

### Claim 14 (depends on 11)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 11, wherein in step S2, the reducing atmosphere is provided by carbon blocks.

### Claim 15 (depends on 11)

The preparation method for the copper ion-doped polychromatic fluorescent glass according to claim 11, wherein in step S3, temperature of the annealing is 320° C. to 450° C.

### Claim 16 (depends on 2)

Use of the copper ion-doped polychromatic fluorescent glass according to claim 2 in luminescence conversion materials.

### Claim 17 (depends on 16)

The use according to claim 16, wherein the use of the copper ion-doped polychromatic fluorescent glass in single host white-light illumination, near-infrared venography, infrared night-vision scope or food testing.

### Claim 18 (depends on 2)

A LED device, comprising a photoconverter and a LED chip, wherein the photoconverter comprises the copper ion-doped polychromatic fluorescent glass according to claim 2.