# US 2023/0278874 A1 · Carbonized upgraded coal, graphite, and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0278874 A1
- Document ID: US20230278874A1
- Status: Published application
- Kind: A1
- Application number: 18/309,339
- Filed: 2023-04-28
- Published: 2023-09-07
- Earliest claimed: 2020-08-28
- Applicants: Energy and Environmental Research Center Foundation
- Inventors: Alexander Azenkeng; Jason D. Laumb
- Web page: https://patentgrep.com/patent/US20230278874A1

## CPC

- C01B 32/205: Preparation
- C10B 53/04: of powdered coal
- C10B 57/08: Non-mechanical pretreatment of the charge (C10L9/00 takes precedence), {e.g. desulfurization}
- C10L 5/04: Raw material {of mineral origin} to be used; Pretreatment thereof {(pretreatment of fuels of non-mineral origin C10L5/40)}
- C10L 9/06: by oxidation
- H01M 4/587: for inserting or intercalating light metals
- C01B 2204/04: Specific amount of layers or specific thickness
- C01B 2204/06: Graphene nanoribbons
- C10L 2290/08: Drying or removing water
- C10L 2290/544: Extraction for separating fractions, components or impurities during preparation or upgrading of a fuel
- C10L 2290/545: Washing, scrubbing, stripping, scavenging for separating fractions, components or impurities during preparation or upgrading of a fuel
- C10L 2290/60: Measuring or analysing fractions, components or impurities or process conditions during preparation or upgrading of a fuel
- C25B 11/043: Carbon, e.g. diamond or graphene
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C10B: DESTRUCTIVE DISTILLATION OF CARBONACEOUS MATERIALS FOR PRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS (cracking oils C10G; underground gasification of minerals E21B43/295)
- C10L: FUELS NOT OTHERWISE PROVIDED FOR; NATURAL GAS; SYNTHETIC NATURAL GAS OBTAINED BY PROCESSES NOT COVERED BY SUBCLASSES C10G OR C10K; LIQUIFIED PETROLEUM GAS; USE OF ADDITIVES TO FUELS OR FIRES; FIRE-LIGHTERS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

A method of forming graphite includes carbonizing an upgraded coal, to form a carbonized upgraded coal. The method also includes graphitizing the carbonized upgraded coal, to form the graphite.

## Claims

### Claim 1

A method of carbonizing an upgraded coal, the method comprising:
heating the upgraded coal in an inert environment, to form a carbonized upgraded coal.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heating comprises heating to a temperature of 500° C. to 2,000° C. for a duration of 10 min to 6 h.

### Claim 3 (depends on 1)

The method of claim 1, wherein the upgraded coal comprises an upgraded lignite coal, an upgraded subbituminous coal, an upgraded anthracite coal, an upgraded crushed coal, an upgraded particulate coal, an upgraded coal waste, or a combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the method includes allowing the carbonized upgraded coal to cool to a temperature of 0° C. to 1000° C. over a duration of 1 h to 4 h.

### Claim 5 (depends on 1)

The method of claim 1, wherein the upgraded coal comprises:
an ash content of 2 wt% to 12 wt%;
an oxygen concentration of 10 wt% to 25 wt%; and
a carbon concentration of 40 wt% to 75 wt%.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carbonized upgraded coal has a fixed carbon (FC) content of 80 wt% to 99 wt%.

### Claim 7 (depends on 1)

The method of claim 1, further comprising forming the upgraded coal, comprising
cleaning coal to form a cleaned coal residue; and
at least one of
reacting the cleaned coal residue with an oxidizable inorganic metallic agent, and
reacting the cleaned coal residue with a reducing agent,
to form the upgraded coal.

### Claim 8 (depends on 7)

The method of claim 7, wherein the method comprises:
cleaning coal having a largest dimension of 25 mm or less using a strong mineral acid at a temperature of 30° C. to 100° C. to form a cleaned coal residue; and
at least one of
reacting the cleaned coal residue at 100° C. to 500° C. under an inert gas with an oxidizable inorganic metallic agent comprising iron (II) sulfate heptahydrate (FeSO4·7H2O), iron (II) chloride tetrahydrate (FeCl-4H2O), or a combination thereof, and
reacting the cleaned coal residue at 0° C. to 50° C. in an organic solvent with a reducing agent comprising lithium aluminum hydride (LAH), sodium borohydride (NAH), or a combination thereof,
to form the upgraded coal; wherein
the upgraded coal has a lower ash content, as compared to the coal used to form the upgraded coal, and
the upgraded coal has at least one of a lower oxygen concentration, a lower sulfur concentration, a lower nitrogen concentration, and a higher carbon concentration, as compared to the naturally-sourced coal used to form the upgraded coal.

### Claim 9 (depends on 1)

A carbonized upgraded coal formed by the method of claim 1.

### Claim 10 (depends on 1)

The method of claim 1, wherein the method is a method of forming graphite, the method further comprising:
graphitizing the carbonized upgraded coal, to form the graphite.

### Claim 11 (depends on 10)

The method of claim 10, wherein the graphitizing comprises heating the carbonized upgraded coal in an inert environment to a graphitization temperature in the range of 2500° C. to 3500° C. for a graphitization duration of 10 min to 10 h, to form the graphite, and wherein the method further includes allowing the graphite to cool to 0° C. to 1000° C. over a duration of 1 h to 4 h.

### Claim 12 (depends on 10)

The method of claim 10, wherein the graphite comprises croissant graphite that comprises a croissant-like texture and shape, the croissant graphite comprising 2D-graphene sheets spiral-wound or folded into ribbon-like structures.

### Claim 13 (depends on 10)

The method of claim 10, wherein the graphite comprises
3D graphene stacks comprising internal longitudinal hollow channels,
graphulerenite that comprises a spherical external geometry, a plurality of approximately flat sides, and a solid fill, or
a combination thereof.

### Claim 14 (depends on 10)

The method of claim 10, further comprising controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 0 wt% to <7 wt%, wherein in the graphite a weight ratio of croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels to graphulerenite is equal to or greater than 100:1.

### Claim 15 (depends on 10)

The method of claim 10, further comprising controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 5.6 wt% to 20 wt%, wherein in the graphite a weight ratio of graphulerenite to croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels is equal to or greater than 100:1.

### Claim 16 (depends on 10)

The method of claim 10, wherein the graphite has a degree of graphitization of 70% to 95%.

### Claim 17

A method of forming graphite, the method comprising:
cleaning coal to form a cleaned coal residue;
at least one of
reacting the cleaned coal residue with an oxidizable inorganic metallic agent, and
reacting the cleaned coal residue with a reducing agent,
to form an upgraded coal;
heating the upgraded coal to a temperature of 500° C. to 2,000° C. in an inert environment, to form a carbonized upgraded coal;
controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 0 wt% to <7 wt%; and
heating the carbonized upgraded coal to a graphitization temperature in the range of 2500° C. to 3500° C. for a graphitization duration of 10 min to 10 h, to form the graphite, wherein in the graphite a weight ratio of croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels to graphulerenite is equal to or greater than 100:1.

### Claim 18

A method of forming graphite, the method comprising:
cleaning coal to form a cleaned coal residue;
at least one of
reacting the cleaned coal residue with an oxidizable inorganic metallic agent, and
reacting the cleaned coal residue with a reducing agent,
to form an upgraded coal;
heating the upgraded coal to a temperature of 500° C. to 2,000° C. in an inert environment, to form a carbonized upgraded coal;
controlling the cleaning and/or the reacting of the cleaned coal residue with the oxidizable inorganic metallic agent and/or the reacting of the cleaned coal residue with the reducing agent, such that the ash content of the carbonized upgraded coal is 5.6 wt% to 20 wt%; and
heating the carbonized upgraded coal to a graphitization temperature in the range of 2500° C. to 3500° C. for a graphitization duration of 10 min to 10 h, to form the graphite, wherein in the graphite a weight ratio of graphulerenite to croissant graphite and/or 3D graphene stacks comprising internal longitudinal hollow channels is equal to or greater than 100:1.

### Claim 19 (depends on 10)

A graphite formed from the method of claim 10.

### Claim 20 (depends on 19)

An electrochemical cell comprising:
a cathode; and
an anode comprising the graphite of claim 19.