- Inventors: Yong-Hee Kang; Ji-Hoon Ryu; Yeo-Min Yoon; Jae-Won Lee; Jung-Hoon Lee; Bum-Young Jung
- Web page: https://patentgrep.com/patent/US20230275267A1

## CPC

- H01M 10/052: Li-accumulators
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/058: Construction or manufacture
- H01M 10/446: {Initial charging measures}
- H01M 10/52: Removing gases inside the secondary cell, e.g. by absorption (vent plugs or other mechanical arrangements for facilitating escape of gases H01M50/30)
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- H01M 2300/0082: Organic polymers
- H01M 2300/0085: Immobilising or gelification of electrolyte
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing a gel polymer electrolyte battery, the method comprising two steps of pressurization carried out before and after a formation step, is provided. The method provides a gel polymer electrolyte battery having a small gap between a separator and an electrode, high binding force, reduced thickness, improved shape stability and stiffness, and thus provides the gel polymer electrolyte battery having increased initial capacity, reduced initial resistance, and improved characteristics, such as cycle characteristics, high-temperature safety, overcharge safety and penetration safety.

## Claims

### Claim 1

A method for manufacturing a gel polymer electrolyte battery, the method comprising:
(S1) a pre-aging step which includes accommodating a stack cell in a battery housing, injecting an electrolyte precursor thereto, and gelling the electrolyte precursor to form a gel polymer electrolyte;
(S2) a first pressurization step of pressurizing the product of step (S1);
(S3) a formation step of carrying out charge/discharge of the product of step (S2);
(S4) an aging step of allowing the product of step (S3) to stand for a predetermined time; and
(S5) a second pressurization step of pressurizing the product of (S4),
wherein step (S5) is carried out under a pressure higher than that of step (S2).

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first pressurization step is carried out at 3 kgf/cm2 or less.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the electrolyte precursor comprises an organic solvent, a lithium salt, a crosslinkable polymer and/or oligomer, and a crosslinking initiator.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the crosslinkable polymer comprises a polyvinylidene fluoride (PVDF)-based polymer containing a vinylidene fluoride unit; and/or an acrylic polymer having a crosslinkable functional group.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the step of gelling the electrolyte precursor is carried out at a temperature at which crosslinking of the crosslinkable polymer and/or oligomer is accomplished.

### Claim 6 (depends on 1)

The method according to claim 1, wherein step (S2) is carried out for a time of 1 hour or less.

### Claim 7 (depends on 1)

The method according to claim 1, wherein step (S3) is carried out under the same pressure as that of step (S2), while not releasing the pressure applied in step (S2).

### Claim 8 (depends on 1)

The method according to claim 1, wherein step (S3) is carried out by charging to 30-100% capacity of the gel polymer electrolyte battery.

### Claim 9 (depends on 1)

The method according to claim 1, wherein step (S5) is carried out at a temperature equal to or higher than the that of step (S2).

### Claim 10 (depends on 1)

The method according to claim 1, wherein step (S5) is carried out at a temperature higher than the that of step (S2).

### Claim 11 (depends on 1)

The method according to claim 1, wherein step (S2) is carried out at a temperature of 30-70° C.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising a degassing step carried out after step (S5).