# US 2023/0275236 A1 · Current collector and preparation method thereof, secondary battery, and apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0275236 A1
- Document ID: US20230275236A1
- Status: Published application
- Kind: A1
- Application number: 18/311,363
- Filed: 2023-05-03
- Published: 2023-08-31
- Earliest claimed: 2021-04-01
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Bobing HU; Shengyuan HUANG; Chengyong LIU; Jiawei FU; Xiaoning HE; Jieliang ZOU; Chengbin ZHONG
- Web page: https://patentgrep.com/patent/US20230275236A1

## CPC

- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/70: characterised by shape or form
- H01M 4/66: Selection of materials
- H01M 10/052: Li-accumulators
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A current collector includes a current collector body and a lithiophilic layer applied on a surface of the current collector body. The lithiophilic layer has lithium affinity and comprises a lithiophilic material. The lithiophilic material comprises an internal structure and an external structure, and the internal structure is a cavity.

## Claims

### Claim 1

A current collector, comprising:
a current collector body; and
a lithiophilic layer applied on a surface of the current collector body, wherein the lithiophilic layer has lithium affinity and comprises a lithiophilic material, the lithiophilic material comprises an internal structure and an external structure, and the internal structure is a cavity.

### Claim 2 (depends on 1)

The current collector according to claim 1, wherein morphology of the external structure of the lithiophilic material comprises one or more selected from granular structure, linear structure, plate structure, spherical shape, and near-spherical shape.

### Claim 3 (depends on 1)

The current collector according to claim 1, wherein an average thickness of the external structure of the lithiophilic material is 0.05-2 μm.

### Claim 4 (depends on 3)

The current collector according to claim 3, wherein the average thickness of the external structure of the lithiophilic material is 0.1-1 μm.

### Claim 5 (depends on 1)

The current collector according to claim 1, wherein a material of the external structure of the lithiophilic material comprises at least one of metal or metal oxide with lithium affinity.

### Claim 6 (depends on 5)

The current collector according to claim 5, wherein the material of the external structure of the lithiophilic material comprises at least one of gold, silver, platinum, or silver oxide.

### Claim 7 (depends on 1)

The current collector according to claim 1, wherein a thickness of the lithiophilic layer is 1-500 μm.

### Claim 8 (depends on 7)

The current collector according to claim 7, wherein the thickness of the lithiophilic layer is 10-100 μm.

### Claim 9 (depends on 1)

The current collector according to claim 1, wherein the current collector body comprises a metal foil.

### Claim 10 (depends on 9)

The current collector according to claim 9, wherein the current collector body comprises a copper foil.

### Claim 11

A preparation method of a current collector, comprising:
providing a material with composite structure, wherein:
a material of an internal structure of the material with composite structure comprises a first metal, and a material of an external structure of the material with composite structure comprises at least one of a second metal or an oxide of the second metal with lithium affinity; and
the first metal is copper or a metal having an oxidation potential lower than an oxidation potential of copper, and the second metal comprises a metal having an oxidation potential is higher than an oxidation potential the first metal;
reacting the material with composite structure with an acid solution to form a lithiophilic material with lithium affinity, wherein the lithiophilic material comprises an internal structure and an external structure, and the internal structure of the lithiophilic material is a cavity; and
applying the lithiophilic material to a surface of a current collector body.

### Claim 12 (depends on 11)

The preparation method according to claim 11, wherein the first metal comprises at least one of tin, zinc, iron, aluminum, or copper, and the second metal comprises at least one of gold, silver, or platinum.

### Claim 13 (depends on 12)

The preparation method according to claim 12, wherein the material with composite structure comprises at least one of silver-coated tin powder, silver-coated zinc powder, silver-coated iron powder, silver-coated aluminum powder, silver-coated copper powder, gold-coated tin powder, gold-coated zinc powder, gold-coated iron powder, gold-coated aluminum powder, gold-coated copper powder, platinum-coated tin powder, platinum-coated zinc powder, platinum-coated iron powder, platinum-coated aluminum powder, or platinum-coated copper powder.

### Claim 14 (depends on 11)

The preparation method according to claim 11, wherein based on a total weight of the material with composite structure, an amount of the second metal is 1 wt % to 10 wt %.

### Claim 15 (depends on 11)

The preparation method according to claim 11, wherein a potential of the acid solution is between a potential of the internal structure of the material with composite structure and a potential of the external structure of the material with composite structure.

### Claim 16 (depends on 15)

The preparation method according to claim 15, wherein the acid solution comprises at least one of sulfuric acid or hydrochloric acid.

### Claim 17 (depends on 11)

A secondary battery, comprising the current collector prepared by the preparation method according to claim 11.

### Claim 18 (depends on 17)

An apparatus, comprising the secondary battery according to claim 17.

### Claim 19

A secondary battery, comprising:
a current collector, comprising:
a current collector body; and
a lithiophilic layer applied on a surface of the current collector body, wherein the lithiophilic layer has lithium affinity and comprises a lithiophilic material, the lithiophilic material comprises an internal structure and an external structure, and the internal structure is a cavity.

### Claim 20 (depends on 19)

An apparatus, comprising the secondary battery according to claim 19.