# US 2023/0275209 A1 · Positive Electrode Active Material for Lithium Secondary Battery, Method of Preparing the Same, and Positive Electrode for Lithium Secondary Battery and Lithium Secondary Battery Which Include the Positive Electrode Active Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0275209 A1
- Document ID: US20230275209A1
- Status: Published application
- Kind: A1
- Application number: 18/195,089
- Filed: 2023-05-09
- Published: 2023-08-31
- Earliest claimed: 2018-04-06
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Tae Gu Yoo; Young Uk Park; Jin Tae Hwang; Wang Mo Jung; Sung Bin Park
- Web page: https://patentgrep.com/patent/US20230275209A1

## CPC

- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/66: containing alkaline earth metals, e.g. SrNiO3 or SrNiO2
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode active material includes a lithium transition metal oxide, which is doped with doping element M2, wherein M2 includes at least one of Al, Ti, Mg, Zr, W, Y, Sr, Co, F, Si, Na, Cu, Fe, Ca, S, or B, and contains nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium, wherein the lithium transition metal oxide has a single particle form, and includes a center portion having a layered structure and a surface portion having a rock-salt structure, and the doping element M2 is included in an amount of 3,580 ppm to 7,620 ppm based on a total weight of the positive electrode active material.

## Claims

### Claim 1

A positive electrode active material comprising:
a lithium transition metal oxide doped with doping element M2,
wherein M2 includes at least one of aluminum (Al), titanium (Ti), magnesium (Mg), zirconium (Zr), tungsten (W), yttrium (Y), strontium (Sr), fluorine (F), silicon (Si), sodium (Na), copper (Cu), iron (Fe), calcium (Ca), sulfur (S), or boron (B), and
wherein the lithium transition metal oxide contains nickel in an amount of 60 mol % or more based on a total number of moles of transition metals excluding lithium,
wherein the lithium transition metal oxide has a single particle form and comprises a center portion having a layered structure and a surface portion having a rock-salt structure, and
the doping element M2 is included in an amount of 3,580 ppm to 7,620 ppm based on a total weight of the positive electrode active material.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein a grain size of the positive electrode active material is in a range of 180 nm to 300 nm.

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein the doping element M2 comprises Sr.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the surface portion is a region located within 100 nm from a surface toward a center of a particle.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein the lithium transition metal oxide is represented by Formula 1:
Li1+a[NixCoyM1zM2w]1−aO2 [Formula 1]
wherein, in Formula 1,
0≤a≤0.2, 0.6≤x<1, 0<y≤0.4, 0<z≤0.4, 0<w≤0.1, and x+y+z+w=1,
M1 comprises manganese (Mn) or Al, and
M2 comprises at least one of Al, Ti, Mg, Zr, W, Y, Sr, F, Si, Na, Cu, Fe, Ca, S, or B.

### Claim 6 (depends on 1)

The positive electrode active material of claim 1, further comprising a coating element M3-containing coating layer formed on a surface of the lithium transition metal oxide, wherein M3 comprises at least one of Al, Ti, Mg, Zr, W, Y, Sr, Co, F, Si, Na, Cu, Fe, Ca, S, or B.

### Claim 7 (depends on 6)

The positive electrode active material of claim 6, wherein a total amount of the doping element M2 and the coating element M3 is in a range of 4,580 ppm to 9,120 ppm based on the total weight of the positive electrode active material.

### Claim 8 (depends on 1)

The positive electrode active material of claim 1, wherein the positive electrode active material has an average particle diameter of 3.5 μm to 7 μm.

### Claim 9

A method of preparing a positive electrode active material, comprising:
mixing a transition metal precursor containing nickel in an amount of 60 mol % or more based on a total number of moles of transition metals, a lithium raw material, and a doping element M2-containing raw material, wherein M2 includes at least one of aluminum (Al), titanium (Ti), magnesium (Mg), zirconium (Zr), tungsten (W), yttrium (Y), strontium (Sr), fluorine (F), silicon (Si), sodium (Na), copper (Cu), iron (Fe), calcium (Ca), sulfur (S), or boron (B), and
sintering the mixture at 800° C. to 1,000° C. to prepare a lithium transition metal oxide having a single particle form,
wherein the doping element M2-containing raw material is mixed such that an amount of the doping element M2 is in a range of 3,580 ppm to 7,620 ppm based on a total weight of the positive electrode active material.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
forming a coating layer on a surface of the positive electrode active material by mixing the positive electrode active material and a coating element M3-containing raw material, wherein M3 comprises at least one of Al, Ti, Mg, Zr, W, Y, Sr, Co, F, Si, Na, Cu, Fe, Ca, S, or B, and performing a heat treatment.

### Claim 11 (depends on 10)

The method of claim 10, wherein the heat treatment is performed at 350° C. to 800° C.

### Claim 12 (depends on 10)

The method of claim 10, wherein the doping element M2-containing raw material and the coating element M3-containing raw material are mixed such that a total amount of the doping element M2 and the coating element M3 is in a range of 4,580 ppm to 9,120 ppm based on the total weight of the positive electrode active material.

### Claim 13 (depends on 1)

A positive electrode for a lithium secondary battery, the positive electrode comprising the positive electrode active material of claim 1.

### Claim 14 (depends on 13)

A lithium secondary battery comprising the positive electrode of claim 13.