# US 2023/0275207 A1 · Method of manufacturing anode for lithium secondary battery including pre-litigation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0275207 A1
- Document ID: US20230275207A1
- Status: Published application
- Kind: A1
- Application number: 17/992,250
- Filed: 2022-11-22
- Published: 2023-08-31
- Earliest claimed: 2022-02-28
- Assignees: Hyundai Motor Company; Kia Corporation; Korea Institute of Science and Technology
- Applicants: Hyundai Motor Company; Kia Corporation; Korea Institute of Science and Technology
- Inventors: Young Jin Nam; Dae Yang Oh; Soon Chul Byun; Jae Min Lim; Hong Suk Choi; Min Ah Lee; Ji Hyun Hong; In Yeong Kang; Ju Young Jang
- Web page: https://patentgrep.com/patent/US20230275207A1

## CPC

- H01M 4/0459: {Electrochemical doping, intercalation, occlusion or alloying}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/044: {Activating, forming or electrochemical attack of the supporting material}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/38: of elements or alloys
- H01M 4/587: for inserting or intercalating light metals
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Proposed is a method of manufacturing an anode for a lithium secondary battery, including a pre-lithiation step.

## Claims

### Claim 1

A method of manufacturing an anode for a lithium secondary battery, the method comprising:
preparing an anode comprising an anode current collector, and a coating layer disposed on the anode current collector and comprising a carbon material;
immersing the anode in a pre-lithiation solution; and
immersing the anode in a stabilizing solution, wherein the pre-lithiation solution comprises a pre-lithiated compound comprising lithium and a biphenyl-based compound,
wherein the stabilizing solution comprises at least one of fluoroethylene carbonate (FEC), vinylene carbonate (VC), vinyl ethylene carbonate (VEC), methyl vinylene carbonate (meVC), ethylene carbonate (EC), or any combination thereof, and
wherein a lithium doping amount of the anode is about 1 mAh/cm2 or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the coating layer comprises the carbon material and a metal capable of alloying with the lithium.

### Claim 3 (depends on 2)

The method of claim 2, wherein the metal capable of alloying with the lithium comprises at least one of silver (Ag), magnesium (Mg), aluminum (Al), gallium (Ga), zinc (Zn), bismuth (Bi), tin (Sn), indium (In), antimony (Sb), lead (Pb), silicon (Si), germanium (Ge), or any combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein a concentration of the pre-lithiation compound is about 0.1 M to 1 M.

### Claim 5 (depends on 1)

The method of claim 1, wherein a molar ratio of the lithium and the biphenyl-based compound is about 0.5:1 to 6:1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the biphenyl-based compound is represented by the following Formula 1.
wherein, in Formula 1, R1 to R10 each comprises an alkyl group having 1 to 3 of carbon atoms.

### Claim 7 (depends on 1)

The method of claim 1,
wherein the pre-lithiation solution further comprises a solvent, and
wherein the solvent comprises at least one of dimethyl ether (DME), 2-methyl tetrahydrofuran, tetrahydropyranyl, or any combination thereof

### Claim 8 (depends on 1)

The method of claim 1, wherein the anode is immersed in the pre-lithiation solution at a temperature of about 25° C. to 60° C. for about 10 seconds to 30 minutes.

### Claim 9 (depends on 1)

The method of claim 1, wherein the anode is immersed in the stabilizing solution to form a film on the anode, and the film comprises a C—O bond, a C═O bond, and an R—CO—R′ bond.

### Claim 10 (depends on 9)

The method of claim 9, wherein a thickness of the film is about 200 nm or less.

### Claim 11 (depends on 1)

The method of claim 1, wherein the anode is immersed in the stabilizing solution for about 10 to 60 minutes.

### Claim 12

An anode for a lithium secondary battery, the anode comprising:
an anode current collector; and
a coating layer disposed on the anode current collector.

### Claim 13 (depends on 12)

The anode of claim 12, wherein the coating layer comprises a carbon material and a metal capable of alloying with lithium.

### Claim 14 (depends on 13)

The anode of claim 13, wherein the metal capable of alloying with the lithium comprises at least one of silver (Ag), magnesium (Mg), aluminum (Al), gallium (Ga), zinc (Zn), bismuth (Bi), tin (Sn), indium (In), antimony (Sb), lead (Pb), silicon (Si), germanium (Ge), or any combination thereof.