# US 2023/0275203 A1 · All-solid-state battery having protective layer comprising metal sulfide and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0275203 A1
- Document ID: US20230275203A1
- Status: Published application
- Kind: A1
- Application number: 18/078,773
- Filed: 2022-12-09
- Published: 2023-08-31
- Earliest claimed: 2022-02-25
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Ga Hyeon Im; Seung Ho Choi; Sang Heon Lee; Yun Sung Kim
- Web page: https://patentgrep.com/patent/US20230275203A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/66: Selection of materials
- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/366: {as layered products}
- H01M 4/38: of elements or alloys
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- H01M 4/5815: {Sulfides}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2300/0065: Solid electrolytes
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are an all-solid-state battery having a protective layer including a composite including a metal sulfide and a carbon component, and a method for manufacturing the same. The all-solid-state battery includes an anode current collector, the protective layer disposed on the anode current collector, a solid electrolyte layer disposed on the protective layer, a cathode active material layer disposed on the solid electrolyte layer, and a cathode current collector disposed on the cathode active material layer, and the protective layer includes a matrix comprising the composite including the metal sulfide and the carbon component, and a metal component distributed in the matrix and capable of alloying with lithium.

## Claims

### Claim 1

An all-solid-state battery comprising:
an anode current collector;
a protective layer disposed on the anode current collector;
a solid electrolyte layer disposed on the protective layer;
a cathode active material layer disposed on the solid electrolyte layer; and
a cathode current collector disposed on the cathode active material layer,
wherein the protective layer comprises:
a matrix comprising a composite comprising a metal sulfide and a carbon component; and
a metal component distributed in the matrix and capable of alloying with lithium.

### Claim 2 (depends on 1)

The all-solid-state battery of claim 1, wherein the metal sulfide comprises a compound represented by MxSy, wherein M comprises one or more of Mo, W, Cu, Co, Ti, Ni, and Fe, 1≤x≤3 and 0.5≤y≤4.

### Claim 3 (depends on 1)

The all-solid-state battery of claim 1, wherein the carbon component comprises spherical particles having a particle size D50 of about 10 nm to 100 nm, or linear particles having a cross-sectional diameter of about 10 nm to 300 nm.

### Claim 4 (depends on 1)

The all-solid-state battery of claim 1, wherein the carbon component comprises one or more of carbon black, carbon nanotubes, carbon fiber, vapor-grown carbon fiber (VGCF) or any combination thereof.

### Claim 5 (depends on 1)

The all-solid-state battery of claim 1, wherein a particle size D50 of the composite ranges from about 10 nm to 1 μm.

### Claim 6 (depends on 1)

The all-solid-state battery of claim 1, wherein the composite comprises the metal sulfide and the carbon component at a mass ratio of about 2:8 to 5:5.

### Claim 7

The all-solid-state battery of claim I, wherein the metal component comprises one or more of Ag, Zn, Mg, Bi, and Sn.

### Claim 8 (depends on 1)

The all-solid-state battery of claim 1, wherein a particle size D50 of the metal component ranges from about 30 nm to 500 nm.

### Claim 9 (depends on 1)

The all-solid-state battery of claim 1 wherein the protective layer comprises an amount of about 50% to 80% by weight of the matrix and an amount of about 20% to 50% by weight of the metal component, based on the total weight of the protective layer, and has a thickness of about 1 μm to 20 μm.

### Claim 10 (depends on 1)

The all-solid-state battery of claim 1, wherein the metal sulfide reacts with lithium ions to produce lithium sulfide (Li2S) and a metal during charging and discharging of the all-solid-state battery, and lithium is stored between the anode current collector and the protective layer.

### Claim 11

A method for manufacturing an all-solid-state battery, comprising:
preparing a composite comprising a metal sulfide and a carbon component by performing mechanical milling;
preparing a slurry comprising the composite and a metal component capable of alloying with lithium;
forming a protective layer by applying the slurry to a substrate; and
preparing a stack comprising an anode current collector, the protective layer disposed on the anode current collector, a solid electrolyte layer disposed on the protective layer, a cathode active material layer disposed on the solid electrolyte layer, and a cathode current collector disposed on the cathode active material layer,
wherein the protective layer comprises:
a matrix comprising the composite comprising the metal sulfide and the carbon component; and
the metal component distributed in the matrix and capable of alloying with lithium.

### Claim 12 (depends on 11)

The method of claim 11, wherein the metal sulfide comprises a compound represented by MxSy, wherein M comprises one or more of Mo, W, Cu, Co, Ti, Ni, and Fe, 1≤x≤3 and 0.5≤y≤4.

### Claim 13 (depends on 11)

The method of claim 11, wherein a particle size D50 of the metal sulfide ranges from about 10 nm to 50 μm.

### Claim 14 (depends on 11)

The method of claim 11, wherein the carbon component comprises spherical particles having a particle size D50 of about 10 nm to 100 nm, or linear particles having a cross-sectional diameter of about 10 nm to 300 nm.

### Claim 15 (depends on 11)

The method of claim 11, wherein the carbon component comprises one or more of carbon black, carbon nanotubes, carbon fiber, and vapor-grown carbon fiber (VGCF).

### Claim 16 (depends on 11)

The method of claim 11, wherein a particle size D50 of the composite ranges from about 10 nm to 1 μm.

### Claim 17 (depends on 11)

The method of claim 11, wherein the composite comprises the metal sulfide and the carbon component at a mass ratio of about 2:8 to 5:5.

### Claim 18 (depends on 11)

The method of claim 11, wherein the metal component comprises one or more of Ag, Zn, Mg, Bi, and Sn.

### Claim 19 (depends on 11)

The method of claim 11, wherein a particle size D50 of the metal component ranges from about 30 nm to 500 nm.

### Claim 20 (depends on 11)

The method of claim 11, wherein the protective layer comprises an amount of about 50% to 80% by weight of the matrix and an amount of about 20% to 50% by weight of the metal component, based on the total weight of the protective layer, and has a thickness of about 1 μm to 20 μm.