# US 2023/0275049 A1 · Semiconductor devices having conductive pad structures with multi-barrier films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0275049 A1
- Document ID: US20230275049A1
- Status: Published application
- Kind: A1
- Application number: 18/314,923
- Filed: 2023-05-10
- Published: 2023-08-31
- Earliest claimed: 2018-07-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Po-Hsun HUANG; Po-Han WANG; Ing-Ju LEE; Chao-Lung CHEN; Cheng-Ming WU
- Web page: https://patentgrep.com/patent/US20230275049A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10W 72/019: {of bond pads}
- H10F 39/011: {Manufacture or treatment of image sensors covered by group H10F39/12}
- H10F 39/8053: {Colour filters}
- H10F 39/8063: {Microlenses}
- H10F 39/811: {Interconnections}
- H10P 14/44: Physical vapour deposition [PVD]
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 72/90: Bond pads, in general
- H10W 72/01223: {in liquid form, e.g. by dispensing droplets or by screen printing}
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01238: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01953: {by etching}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/59: Bond pads specially adapted therefor
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Semiconductor devices are provided. The semiconductor device includes a substrate, an interconnect structure, and a conductive pad structure. The interconnect structure is over the substrate and includes a top metal layer. The conductive pad structure is over the interconnect structure and includes a lower barrier film, an upper barrier film, and an aluminum-containing layer. The lower barrier film is on the top metal layer. The upper barrier film is on the lower barrier film and has an amorphous structure. The aluminum-containing layer is on the upper barrier film. The lower barrier film and the upper barrier film are made of a same material, and a nitrogen atomic percentage of the upper barrier film is higher than a nitrogen atomic percentage of the lower barrier film.

## Claims

### Claim 1

A semiconductor device, comprising:
a substrate;
an interconnect structure over the substrate and comprising a top metal layer; and
a conductive pad structure over the interconnect structure and comprising:
a lower barrier film on the top metal layer;
an upper barrier film on the lower barrier film and having an amorphous structure; and
an aluminum-containing layer on the upper barrier film,
wherein the lower barrier film and the upper barrier film are made of a same material, and a nitrogen (N) atomic percentage of the upper barrier film is higher than a nitrogen (N) atomic percentage of the lower barrier film.

### Claim 2 (depends on 1)

The semiconductor device as claimed in claim 1, wherein the N atomic percentage of the upper barrier film is in a range from about 2.5 times to about 5 times greater than the N atomic percentage of the lower barrier film.

### Claim 3 (depends on 1)

The semiconductor device as claimed in claim 1, wherein the lower barrier film and the upper barrier film are made of tantalum nitride (TaN).

### Claim 4 (depends on 1)

The semiconductor device as claimed in claim 1, wherein the top metal layer is made of copper (Cu), and the aluminum-containing layer is made of aluminum-copper (AlCu) alloy.

### Claim 5 (depends on 1)

The semiconductor device as claimed in claim 1, wherein a thickness of the lower barrier film is greater than a thickness of the upper barrier film.

### Claim 6 (depends on 5)

The semiconductor device as claimed in claim 5, wherein the thickness of the lower barrier film is in a range from about 2.5 times to about 70 times greater than the thickness of the upper barrier film.

### Claim 7 (depends on 1)

The semiconductor device as claimed in claim 1, further comprising a passivation layer between the lower barrier film and the top metal layer and surrounding bottom portions of the lower barrier film, the upper barrier film, and the aluminum-containing layer.

### Claim 8 (depends on 7)

The semiconductor device as claimed in claim 7, further comprising a conductive bump over the aluminum-containing layer and partially surrounded by the aluminum-containing layer.

### Claim 9

A semiconductor device, comprising:
a substrate comprising electronic elements;
an interconnect structure over the substrate and electrically coupled to the electronic elements; and
a conductive pad structure over the interconnect structure and comprising:
a crystalline tantalum-nitride (TaN) film;
an amorphous tantalum-nitride (TaN) film on the crystalline TaN film; and
an aluminum-containing layer on the amorphous TaN film.

### Claim 10 (depends on 9)

The semiconductor device as claimed in claim 9, wherein a nitrogen (N) atomic percentage of the amorphous TaN film is higher than a nitrogen (N) atomic percentage of the crystalline TaN film.

### Claim 11 (depends on 9)

The semiconductor device as claimed in claim 9, wherein the crystalline TaN film has an atomic ratio of N to TaN in a range from about 0.19 to about 0.31, and the amorphous TaN film has an atomic ratio of N to TaN in a range from about 0.86 to about 0.93.

### Claim 12 (depends on 9)

The semiconductor device as claimed in claim 9, wherein the amorphous TaN film has a higher compressive stress than that of the crystalline TaN film.

### Claim 13 (depends on 9)

The semiconductor device as claimed in claim 9, wherein the aluminum-containing layer is made of aluminum-copper (AlCu) alloy and has a tensile stress.

### Claim 14 (depends on 9)

The semiconductor device as claimed in claim 9, wherein a thickness of the crystalline TaN film is greater than a thickness of the amorphous TaN film.

### Claim 15 (depends on 14)

The semiconductor device as claimed in claim 14, wherein a thickness of the aluminum-containing layer is greater than the thickness of the amorphous TaN film.

### Claim 16

A semiconductor device, comprising:
a substrate having a front side surface and a back side surface opposite to the front side surface;
an interconnect structure under the front side surface of the substrate; and
a conductive pad structure in the substrate and comprising:
a first tantalum-nitride (TaN) film;
a second tantalum-nitride (TaN) film on the first TaN film, wherein the second TaN film has a higher compressive stress than that of the first TaN film; and
an aluminum-containing layer on the second TaN film.

### Claim 17 (depends on 16)

The semiconductor device as claimed in claim 16, wherein the first TaN film is on the front side surface of the substrate and in contact with a top layer of the interconnect structure.

### Claim 18 (depends on 17)

The semiconductor device as claimed in claim 17, wherein the top layer of the interconnect structure is made of copper (Cu), and the aluminum-containing layer is made of aluminum-copper (AlCu) alloy.

### Claim 19 (depends on 16)

The semiconductor device as claimed in claim 16, further comprising an opening extending from the back side surface of the substrate and exposing the aluminum-containing layer.

### Claim 20 (depends on 16)

The semiconductor device as claimed in claim 16, further comprising:
multiple photo-sensing elements in the substrate; and