# US 2023/0274938 A1 · Method of manufacturing semiconductor devices and semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0274938 A1
- Document ID: US20230274938A1
- Status: Published application
- Kind: A1
- Application number: 17/837,848
- Filed: 2022-06-10
- Published: 2023-08-31
- Earliest claimed: 2022-02-25
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Hao-Ming TANG; Shu-Han CHEN; Yun-San CHIEN; Da-Yuan LEE; Chi On CHUI; Tsung-Ju CHEN; Yi-Hsin TING; Han-Shen WANG
- Web page: https://patentgrep.com/patent/US20230274938A1

## CPC

- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10D 84/0167: {Manufacturing their channels}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In a method of manufacturing a semiconductor device, a fin structure is formed by patterning a semiconductor layer, an isolation insulating layer is formed such that an upper portion of the fin structure protrudes from the isolation insulating layer, a gate dielectric layer is formed by a deposition process, a nitridation operation is performed on the gate dielectric layer, and a gate electrode layer is formed over the gate dielectric layer. The gate dielectric layer as formed includes silicon oxide, and the nitridation operation comprises a plasma nitridation operation using a N2 gas and a NH3 gas.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising:
forming a fin structure by patterning a semiconductor layer;
forming an isolation insulating layer such that an upper portion of the fin structure protrudes from the isolation insulating layer;
forming a gate dielectric layer by a deposition process;
after the gate dielectric layer is formed, introducing nitrogen into the gate dielectric layer; and
forming a gate electrode layer over the gate dielectric layer,
wherein the gate dielectric layer as formed is silicon oxide.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the introducing the nitrogen comprises a plasma nitridation operation using a N2 gas and a NH3 gas, and
a flow ratio NH3/(N2+NH3) is in a range from 0.1 to 0.3.

### Claim 3 (depends on 2)

The method of claim 2, wherein a part of the gate dielectric layer formed on a sidewall of the upper portion of the fin structure includes no nitrogen or includes nitrogen in an amount of less than 3 atomic %.

### Claim 4 (depends on 3)

The method of claim 3, wherein a top part of the gate dielectric layer formed on a top of the upper portion of the fin structure and a side part of the gate dielectric layer continuous from the top part to a distance below the top of the upper portion of the fin structure include nitrogen in an amount of 20 to 40 atomic %, the distance being 15% of a height of the upper portion of the fin structure from an upper surface of the isolation insulating layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein an angle between an interface between a nitridated portion of the gate dielectric layer and a non-nitridated portion of the gate dielectric layer and a sidewall of the gate dielectric layer is 1 degree to 5 degrees.

### Claim 6 (depends on 2)

The method of claim 2, wherein a nitrogen concentration at an interface between the gate dielectric layer and the upper portion of the fin structure after the nitridation operation is less than 3 atomic %.

### Claim 7 (depends on 2)

The method of claim 2, wherein a part of the gate dielectric layer formed on the isolation insulating layer is also nitridated.

### Claim 8 (depends on 1)

The method of claim 1, wherein a process temperature of the nitridation operation is in a range from 50° C. to 450° C.

### Claim 9 (depends on 8)

The method of claim 8, wherein a process duration of the nitridation operation is in a range from 20 sec to 150 sec.

### Claim 10

A method for manufacturing a semiconductor device, the method comprising:
forming a fin structure by patterning a semiconductor layer;
forming an isolation insulating layer such that an upper portion of the fin structure protrudes from the isolation insulating layer;
forming a gate dielectric layer over the fin structure by a deposition process;
performing a nitridation operation on the gate dielectric layer; and
forming a gate electrode layer over the gate dielectric layer, wherein:
the gate dielectric layer as formed includes silicon oxide,
the nitridation operation comprises a plasma nitridation operation using one or more of N2 gas and NH3 gas, and
a flow ratio NH3/(N2+NH3) is in a range from 0.4 to 1.0.

### Claim 11 (depends on 10)

The method of claim 10, wherein the flow ratio is in a range from 0.8 to 0.95.

### Claim 12 (depends on 10)

The method of claim 10, wherein an entire outer surface of the gate dielectric layer is nitridated.

### Claim 13 (depends on 10)

The method of claim 10, wherein a nitrogen concentration of the gate dielectric layer after the nitridation operation at a top region of the gate dielectric layer is greater than a nitrogen concentration at a bottom region of the gate dielectric layer.

### Claim 14 (depends on 10)

The method of claim 10, wherein a nitrogen concentration at an interface between the gate dielectric layer and the upper portion of the fin structure after the nitridation operation is less than 3 atomic %.

### Claim 15 (depends on 10)

The method of claim 10, wherein a depth of a nitridated portion of the gate dielectric layer formed on a sidewall of the upper portion of the fin structure is 20% to 80% of a thickness of the gate dielectric layer formed on the sidewall of the upper portion of the fin structure.

### Claim 16 (depends on 10)

The method of claim 10, wherein the gate dielectric layer after the nitridation process is a single layer in which a nitrogen concentration varies along a thickness direction.

### Claim 17

A semiconductor device, comprising:
a semiconductor fin structure disposed over a substrate and including a channel region;
an isolation insulating layer from which the channel region protrudes;
a gate dielectric layer disposed over the channel region; and
a gate electrode disposed over the gate dielectric layer, wherein:
the gate dielectric layer includes silicon oxide that is only partially nitridated.

### Claim 18 (depends on 17)

The semiconductor device of claim 17, wherein a part of the gate dielectric layer formed on a sidewall of the channel region includes no nitrogen or includes nitrogen in an amount of less than 3 atomic %.

### Claim 19 (depends on 18)

The semiconductor device of claim 18, wherein a top part of the gate dielectric layer formed on a top of the channel region and an upper side part of the gate dielectric layer continuous from the top part to a distance below the top of the channel region include nitrogen in an amount of 20 to 40 atomic %, the distance being 15% of a height of the channel region from an upper surface of the isolation insulating layer.

### Claim 20 (depends on 19)

The semiconductor device of claim 19, wherein an angle between an interface between a nitridated portion of the gate dielectric layer and a non-nitridated portion of the gate dielectric layer and a sidewall of the gate dielectric layer is 1 degree to 5 degrees.