# US 2023/0274890 A1 · Electrode foil for electrolytic capacitor, and electrolytic capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0274890 A1
- Document ID: US20230274890A1
- Status: Published application
- Kind: A1
- Application number: 18/003,692
- Filed: 2021-07-15
- Published: 2023-08-31
- Earliest claimed: 2020-07-31
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: MIWA OGAWA; NAOMI KURIHARA; MITSUHISA YOSHIMURA
- Web page: https://patentgrep.com/patent/US20230274890A1

## CPC

- H01G 9/048: characterised by their structure (H01G11/22 takes precedence)
- H01G 9/055: Etched foil electrodes
- H01G 9/042: characterised by the material (H01G11/22 takes precedence)
- H01G 9/045: based on aluminium
- H01G 9/07: Dielectric layers
- H01G 2009/05: {consisting of tantalum, niobium, or sintered material; Combinations of such electrodes with solid semiconductive electrolytes, e.g. manganese dioxide}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

An electrode foil for an electrolytic capacitor includes a base material containing a valve metal and a dissimilar metal composite layer covering a surface of the base material. The dissimilar metal composite layer includes a mixed region in which a first metal and a second metal are mixed. The second metal is different from the first metal. The mixed region constitutes at least 50% of the dissimilar metal composite layer in a thickness-wise direction of the dissimilar metal composite layer. Each of a content M1 of the first metal and a content M2 of the second metal with respect to all metals in the mixed region is 1 atomic % or more.

## Claims

### Claim 1

An electrode foil for an electrolytic capacitor, the electrode foil comprising:
a base material that contains a valve metal; and
a dissimilar metal composite layer that covers a surface of the base material, wherein:
the dissimilar metal composite layer includes a mixed region where a first metal and a second metal are mixed, the second metal being different from the first metal,
the mixed region constitutes at least 50% of the dissimilar metal composite layer in a thickness-wise direction of the dissimilar metal composite layer,
a content M1 of the first metal with respect to all metals in the mixed region is 1 atomic % or more, and
a content M2 of the second metal with respect to all metals in the mixed region is 1 atomic % or more.

### Claim 2 (depends on 1)

The electrode foil according to claim 1, wherein
the content M1 of the first metal with respect to all metals in the mixed region is 1 atomic % or more and 99 atomic % or less, and
the content M2 of the second metal with respect to all metals in the mixed region is 1 atomic % or more and 99 atomic % or less.

### Claim 3 (depends on 1)

The electrode foil according to claim 1, wherein,
when three regions obtained by equally dividing the mixed region are defined as a region A1, a region A2, and a region A3 that are arranged in a stated order from a side close to the surface of the dissimilar metal composite layer in the thickness-wise direction of the dissimilar metal composite layer,
0.8≤RA2/RA1≤1.2 and 0.8≤RA3/RA2≤1.2 are satisfied,
where RA1 denotes an atomic ratio of the first metal to the second metal in the region A1,
RA2 denotes an atomic ratio of the first metal to the second metal in the region A2, and
RA3 denotes an atomic ratio of the first metal to the second metal in the region A3.

### Claim 4 (depends on 3)

The electrode foil according to claim 3, wherein
0.9≤M1A2/M1A1≤1.1, 0.9≤M1A3/M1A2≤1.1, 1≤M1A1, 1≤M1A2, and 1≤M1A3 are satisfied,
where M1A1 denotes a content in atomic % of the first metal with respect to all metals in the region A1,
M1A2 denotes a content in atomic % of the first metal with respect to all metals in the region A2, and
M1A3 denotes a content in atomic % of the first metal with respect to all metals in the region A3.

### Claim 5 (depends on 3)

The electrode foil according to claim 3, wherein
0.9≤M2A2/M2A1≤1.1, 0.9≤M2A3/M2A2≤1.1, 1≤M2A1, 1≤M2A2, and 1≤M2A3 are satisfied,
where M2A1 denotes a content in atomic % of the second metal with respect to all metals in the region A1,
M2A2 denotes a content in atomic % of the second metal with respect to all metals in the region A2, and
M2A3 denotes a content in atomic % of the second metal with respect to all metals in the region A3.

### Claim 6 (depends on 1)

The electrode foil according to claim 1, wherein:
the base material includes a porous portion and a core portion continuous with the porous portion,
the dissimilar metal composite layer covers a surface of the porous portion, and
when three regions obtained by equally dividing the porous portion are defined as a region B1, a region B2, and a region B3 that are arranged in a stated order from a side opposite to the core portion in the thickness-wise direction of the porous portion,
RB3<RB2<RB1 is satisfied,
where RB1 denotes an atomic ratio of the first metal to the second metal in the region B1,
RB2 denotes an atomic ratio of the first metal to the second metal in the region B2, and
RB3 denotes an atomic ratio of the first metal to the second metal in the region B3.

### Claim 7 (depends on 6)

The electrode foil according to claim 6, wherein
M1B3<M1B2<M1B1 is satisfied,
where M1B1 denotes a content in atomic % of the first metal with respect to all metals in the region B1,
M1B1 denotes a content in atomic % of the first metal with respect to all metals in the region B2, and
M1B3 denotes a content in atomic % of the first metal with respect to all metals in the region B3.

### Claim 8 (depends on 6)

The electrode foil according to claim 6, wherein
M2B1<M2B2<M2B3 is satisfied,
where M2B1 denotes a content in atomic % of the second metal with respect to all metals in the region B1,
M2B2 denotes a content in atomic % of the second metal with respect to all metals in the region B2, and
M2B3 denotes a content in atomic % of the second metal with respect to all metals in the region B3.

### Claim 9 (depends on 1)

The electrode foil according to claim 1, wherein:
the first metal includes at least one selected from the group consisting of titanium, tantalum, hafnium, zirconium, and zinc, and
the second metal includes at least one selected from the group consisting of silicon and aluminum.

### Claim 10 (depends on 1)

The electrode foil according to claim 1, wherein:
the first metal is titanium and the second metal is silicon, and
a content of the silicon with respect to all metals in the mixed region is 1 atomic % or more and 70 atomic % or less.

### Claim 11 (depends on 1)

The electrode foil according to claim 1, wherein:
the first metal is titanium and the second metal is aluminum, and
a content of the aluminum with respect to all metals in the mixed region is 1 atomic % or more and 55 atomic % or less.

### Claim 12 (depends on 1)

The electrode foil according to claim 1, wherein the dissimilar metal composite layer is an oxide layer.

### Claim 13 (depends on 12)

The electrode foil according to claim 12, wherein:
the mixed region contains an impurity,
the impurity is at least one selected from the group consisting of hydrogen, carbon, and nitrogen, and
a content of the impurity in the mixed region is 25 atomic % or less with respect to a total of all metals and the impurity in the mixed region.

### Claim 14 (depends on 13)

The electrode foil according to claim 13, wherein a content of the hydrogen in the mixed region is 10 atomic % or less with respect to the total of all metals and the impurity in the mixed region.

### Claim 15 (depends on 1)

The electrode foil according to claim 1, wherein the dissimilar metal composite layer contains a conductive carbon.

### Claim 16 (depends on 1)

The electrode foil according to claim 1, further comprising a layer containing an oxide of the valve metal between the base material and the dissimilar metal composite layer.

### Claim 17 (depends on 1)

An electrolytic capacitor comprising the electrode foil according to claim 1.