# US 2023/0273098 A1 · Method for Preparing TEM Sample

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0273098 A1
- Document ID: US20230273098A1
- Status: Published application
- Kind: A1
- Application number: 18/151,045
- Filed: 2023-01-06
- Published: 2023-08-31
- Earliest claimed: 2022-02-28
- Assignees: Shanghai Huali Integrated Circuit Corporation
- Applicants: Shanghai Huali Integrated Circuit Corporation
- Inventors: Qiang Chen; Yanrong Qiu; Jinde Gao
- Web page: https://patentgrep.com/patent/US20230273098A1

## CPC

- G01N 1/286: {involving mechanical work, e.g. chopping, disintegrating, compacting, homogenising (microtomes G01N1/06; pulverising in general B02C; mixing in general B01F)}
- G01N 1/32: Polishing; Etching
- H01J 37/31: for cutting or drilling
- G01N 2001/2873: {Cutting or cleaving}
- H01J 2237/31745: for preparing specimen to be viewed in microscopes or analyzed in microanalysers
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

The present application discloses a method for preparing a TEM sample, comprising: step 1, forming a first protective layer to non-full fill a deep trench; step 2, performing a first time of front and rear side cutting using a FIB, so as to form the TEM sample having a first thickness, and a via in the deep trench is exposed from the front side and the rear side of the TEM sample; step 3, forming a second material layer, which fully fills the exposed via from the front side and the rear side of the TEM sample; and step 4, performing a second time of front and rear side cutting of a target area on the chip sample using the FIB, so as to reduce the thickness of the TEM sample to a target thickness.

## Claims

### Claim 1

A method for preparing a transmission electron microscope (TEM) sample, comprising the following steps:
step 1, providing a chip sample having a deep trench, and forming a first protective layer, the first protective layer filling the deep trench from a top of the chip sample, and the first protective layer further extending to a top surface of the chip sample outside the deep trench, wherein
a first value is a maximum aspect ratio of a trench fully filled with the first protective layer, an aspect ratio of the deep trench is greater than the first value, the first protective layer does not fully fill the deep trench, and a via produced by non-full filling is formed in the deep trench;
step 2, performing, using a focused ion beam (FIB), a first time of front and rear side cutting of a target area on the chip sample for forming the TEM sample, so as to form the TEM sample having a first thickness, the first thickness being greater than a target thickness, wherein a front side and a rear side of the TEM sample both intersect with an extension direction of the deep trench, and the via in the deep trench is exposed from the front side and the rear side of the TEM sample;
step 3, forming a second material layer, the second material layer fully filling the exposed via from the front side and the rear side of the TEM sample; and
step 4, performing a second time of front and rear side cutting of the target area on the chip sample using the FIB, so as to reduce a thickness of the TEM sample to the target thickness.

### Claim 2 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein the chip sample comprises a semiconductor substrate and a semiconductor device layer formed on a front side of the semiconductor substrate, and the deep trench is located on the semiconductor device layer.

### Claim 3 (depends on 2)

The method for preparing the TEM sample according to claim 2, wherein the chip sample comprises a plurality of deep trenches, and all of the deep trenches are arranged in parallel.

### Claim 4 (depends on 3)

The method for preparing the TEM sample according to claim 3, wherein, in the semiconductor device layer, a structure having the deep trench comprises:
deep trench isolation;
an arrangement structure of polysilicon wires;
an arrangement structure of fins; and
an arrangement structure of metal wires.

### Claim 5 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein, in step 1, the first protective layer is formed by means of an electron beam assisted deposition process or a colloid coating process.

### Claim 6 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein, in step 2, the front side and the rear side of the TEM sample both perpendicularly intersect with the extension direction of the deep trench.

### Claim 7 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein, in step 2, a cutting direction of the first time of front and rear side cutting is a direction from the top surface to a bottom surface of the chip sample.

### Claim 8 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein the first thickness is 100-300 nm.

### Claim 9 (depends on 8)

The method for preparing the TEM sample according to claim 8, wherein the target thickness is 30-80 nm.

### Claim 10 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein, in step 3, the second material layer is formed by means of an electron beam assisted deposition process.

### Claim 11 (depends on 2)

The method for preparing the TEM sample according to claim 2, wherein the semiconductor substrate comprises a silicon substrate.

### Claim 12 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein a material of the first protective layer comprises a metal material.

### Claim 13 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein a material of the second material layer comprises a metal material.

### Claim 14 (depends on 1)

The method for preparing the TEM sample according to claim 1, wherein, in step 1, a thickness of the chip sample is greater than 500 nm.

### Claim 15 (depends on 14)

The method for preparing the TEM sample according to claim 14, wherein the chip sample is obtained by cutting and thinning a wafer composed of a semiconductor substrate.