# US 2023/0272548 A1 · Alloy member, apparatus, and method for manufacturing alloy member

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272548 A1
- Document ID: US20230272548A1
- Status: Published application
- Kind: A1
- Application number: 18/172,903
- Filed: 2023-02-22
- Published: 2023-08-31
- Earliest claimed: 2022-02-28
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: HIROTOMO TAMIYA; JUN-ICHI SAKAMOTO; KEIICHI ISHIZUKA
- Web page: https://patentgrep.com/patent/US20230272548A1

## CPC

- C25D 11/30: of magnesium or alloys based thereon
- C22C 23/00: Alloys based on magnesium
- C22C 23/02: with aluminium as the next major constituent
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An alloy member includes a base material that includes a surface layer and is a magnesium-lithium alloy (Mg—Li alloy) having an α-phase and a β-phase, and an anticorrosive film is able to be formed on the surface layer. A degree of orientation in a (110) plane of the β-phase of the Mg—Li alloy is more than or equal to 70%. An average grain size of the Mg—Li alloy is less than or equal to 50 μm. A Li concentration of the surface layer is lower than a Li concentration of inside of the base material.

## Claims

### Claim 1

An alloy member comprising:
a base material that includes a surface layer and is a Mg—Li alloy having an α-phase and a β-phase,
wherein an anticorrosive film is able to be formed on the surface layer,
wherein a degree of orientation in a (110) plane of the β-phase of the Mg—Li alloy is more than or equal to 70 percent (%),
wherein an average grain size of the Mg—Li alloy is less than or equal to 50 micrometres (μm), and
wherein a Li concentration of the surface layer is lower than a Li concentration of an inside of the base material.

### Claim 2 (depends on 1)

The alloy member according to claim 1, wherein a thickness of the surface layer is more than or equal to 10 μm.

### Claim 3 (depends on 1)

The alloy member according to claim 1, wherein a thickness of the surface layer is more than or equal to 30 μm.

### Claim 4 (depends on 1)

The alloy member according to claim 1, wherein a crystal shape of the α-phase of the Mg—Li alloy is a needle shape.

### Claim 5 (depends on 4)

The alloy member according to claim 4, wherein an average grain size in the α-phase of the Mg—Li alloy is less than or equal to 30 μm.

### Claim 6 (depends on 1)

The alloy member according to claim 1, further comprising:
a Li compound,
wherein after a lapse of two hours from cutting of the alloy member in a lamination direction, the Li compound is deposited from the base material.

### Claim 7 (depends on 6)

The alloy member according to claim 6, wherein the Li compound is at least one of lithium carbonate or lithium oxide.

### Claim 8 (depends on 6)

The alloy member according to claim 6, wherein a Li compound deposited from the surface layer is less than the Li compound deposited from the base material.

### Claim 9 (depends on 1)

The alloy member according to claim 1, further comprising:
an anticorrosive film formed on the surface layer,
wherein the anticorrosive film includes an inorganic fluoride.

### Claim 10 (depends on 9)

The alloy member according to claim 9, wherein the inorganic fluoride comprises magnesium fluoride (MgF2), the proportion of the magnesium fluoride (MgF2) of the inorganic fluoride is more than or equal to 90% By volume.

### Claim 11 (depends on 9)

The alloy member according to claim 9, wherein a thickness of the anticorrosive film is more than or equal to 2 μm.

### Claim 12 (depends on 1)

The alloy member according to claim 1, wherein the Mg—Li alloy has a Li content of more than or equal to 5% by mass and less than or equal to 11% by mass.

### Claim 13 (depends on 1)

The alloy member according to claim 1,
wherein the Mg—Li alloy further contains one or more elements selected from the group consisting of aluminum (Al), zinc (Zn), manganese (Mn), silicon (Si), calcium (Ca), germanium (Ge), and beryllium (Be), and
wherein a content of a sum of the one or more elements is less than or equal to 10% by mass.

### Claim 14 (depends on 13)

The alloy member according to claim 13,
wherein the content of Al is less than or equal to 10% by mass,
wherein the content of Zn is less than or equal to 3% by mass,
wherein the content of Mn is less than or equal to 0.3% by mass,
wherein the content of Si is less than or equal to 0.2% by mass,
wherein the content of Ca is less than or equal to 1.0% by mass,
wherein the content of Ge is less than or equal to 1% by mass, and
wherein the content of Be is less than or equal to 3% by mass.

### Claim 15 (depends on 9)

The alloy member according to claim 9,
wherein a surface of the anticorrosive film on a side opposite to a surface which is in contact with the surface layer has an average surface roughness Ra of more than or equal to 0.19 μm and less than or equal to 0.9 μm and a maximum roughness Rz of less than or equal to 15 μm.

### Claim 16 (depends on 15)

The alloy member according to claim 15, wherein the anticorrosive film has a porous structure.

### Claim 17 (depends on 1)

An apparatus comprising:
a housing; and
a component provided in the housing,
wherein the housing includes the alloy member according claim 1.

### Claim 18

A method for manufacturing an alloy member, comprising:
preparing a base material that is molded using die-cast molding and is an Mg—Li alloy having an α-phase and a β-phase; and
forming a surface layer on the base material by performing an anodization process on the base material to obtain the surface layer having a Li concentration lower than a Li concentration of inside of the base material.

### Claim 19 (depends on 18)

The method for manufacturing the alloy member according to claim 18, wherein in the forming, the surface layer and an anticorrosive film on the surface layer are formed.

### Claim 20 (depends on 18)

The method for manufacturing the alloy member according to claim 18, wherein in the preparing, a molten alloy raw material is die-cast molded under application of pressure to obtain the base material of the Mg—Li alloy.

### Claim 21 (depends on 18)

The method for manufacturing the alloy member according to claim 18, wherein the forming includes
placing a base material as a cathode and the base material of the Mg—Li alloy as an anode in a neutral ammonium fluoride aqueous solution, and
applying a voltage between the anode and the cathode.

### Claim 22 (depends on 18)

The method for manufacturing the alloy member according to claim 18, further comprising heating the base material between the preparing and the forming.