# US 2023/0272540 A1 · Electrolysis process for making lithium hydroxide from lithium chloride and sodium chloride

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272540 A1
- Document ID: US20230272540A1
- Status: Published application
- Kind: A1
- Application number: 18/312,343
- Filed: 2023-05-04
- Published: 2023-08-31
- Earliest claimed: 2020-04-17
- Assignees: Polaris Lithium, LLC
- Applicants: Polaris Lithium, LLC
- Inventors: Mukul M. Sharma; Stoney Brett Barton
- Web page: https://patentgrep.com/patent/US20230272540A1

## CPC

- C25B 1/20: Hydroxides
- C25B 1/46: in diaphragm cells
- C25B 9/19: with diaphragms
- C25B 9/65: Means for supplying current; Electrode connections; Electric inter-cell connections
- C25B 11/037: Electrodes made of particles
- C25B 11/052: Electrodes comprising one or more electrocatalytic coatings on a substrate
- C25B 11/073: characterised by the electrocatalyst material
- C25B 13/00: Diaphragms; Spacing elements
- C25B 15/021: of heating or cooling
- C25B 1/02: Hydrogen or oxygen
- C25B 1/26: Chlorine; Compounds thereof (by simultaneous production of alkali metal hydroxides and chlorine, oxyacids or salts of chlorine C25B1/34)
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Systems and methods are described for producing lithium hydroxide from lithium chloride and sodium chloride through an electrolysis process. A solution of lithium hydroxide and sodium hydroxide may be produced through electrolysis of a lithium chloride and sodium chloride solution. Lithium hydroxide in the produced solution may then be crystallized and filtered out to produce substantially pure lithium hydroxide crystals.

## Claims

### Claim 1

A method for making lithium hydroxide and sodium hydroxide, comprising:
providing a mixture of lithium chloride, sodium chloride, and water to an electrolysis reaction chamber, wherein the electrolysis reaction chamber includes:
a first volume separated from a second volume by an ion-selective membrane, wherein the ion-selective membrane selectively allows lithium and sodium ions to pass through the membrane while inhibiting hydroxide ions and chloride ions from passing through the membrane;
an anode positioned in the first volume; and
a cathode positioned in the second volume;
wherein the mixture is provided to the first volume;
providing water or an aqueous solution of lithium hydroxide and sodium hydroxide to the second volume;
providing a selected voltage to the anode and the cathode from a power supply, producing chlorine gas from the first volume;
producing hydrogen gas from the second volume; and
producing a solution of lithium hydroxide and sodium hydroxide from the second volume.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ion-selective membrane has a selectivity for lithium ions determined by at least one of the ion exchange capacity of the membrane, the degree of hydration of the membrane, or a pore size in the membrane.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ion-selective membrane has a selectivity for sodium ions determined by at least one of the ion exchange capacity of the membrane, the degree of hydration of the membrane, or a pore size in the membrane.

### Claim 4 (depends on 1)

The method of claim 1, wherein the ion-selective membrane has a selectivity for lithium ions that is comparable to the selectivity for sodium ions in a chloralkali process.

### Claim 5 (depends on 1)

The method of claim 1, further comprising producing a diluted mixture of lithium chloride, sodium chloride, and water from the first volume, wherein the diluted mixture has a lower volume percentage of lithium chloride and sodium chloride than the mixture provided to the first volume.

### Claim 6 (depends on 1)

The method of claim 1, wherein the cathode has a coating of at least one of inert metal compounds or transition metal compounds.

### Claim 7 (depends on 6)

The method of claim 6, wherein the coating is applied to the cathode as at least one of using nanoparticles, using a solution, or by electroplating.

### Claim 8 (depends on 1)

The method of claim 1, wherein the anode has a coating of at least one of inert metal compounds or transition metal compounds.

### Claim 9 (depends on 8)

The method of claim 8, wherein the coating is applied to the cathode as at least one of using nanoparticles, using a solution, or by electroplating.

### Claim 10 (depends on 1)

The method of claim 1, further comprising pretreating the mixture to increase a percentage of lithium chloride in the mixture.

### Claim 11 (depends on 1)

The method of claim 1, further comprising removing divalent ions from the mixture of lithium chloride, sodium chloride, and water before providing the mixture to the first volume.

### Claim 12

A method for making lithium hydroxide, comprising:
providing a mixture of lithium chloride, sodium chloride, and water to an electrolysis reaction chamber, wherein the electrolysis reaction chamber includes:
a first volume separated from a second volume by an ion-selective membrane, wherein the ion-selective membrane selectively allows lithium and sodium ions to pass through the membrane while inhibiting hydroxide ions and chloride ions from passing through the membrane;
an anode positioned in the first volume; and
a cathode positioned in the second volume;
wherein the mixture is provided to the first volume;
providing water or an aqueous solution of lithium hydroxide and sodium hydroxide to the second volume;
providing a selected voltage to the anode and the cathode from a power supply, producing a solution of lithium hydroxide and sodium hydroxide from the second volume;
cooling the produced solution of lithium hydroxide and sodium hydroxide; and
removing crystallized lithium hydroxide from the cooled solution.

### Claim 13 (depends on 12)

The method of claim 12, further comprising recirculating a portion of the cooled solution into the electrolysis reaction chamber after removing the crystallized lithium hydroxide.

### Claim 14 (depends on 12)

The method of claim 12, wherein removing the crystallized lithium hydroxide from the cooled solution includes filtering out the crystallized lithium hydroxide from the cooled solution.

### Claim 15 (depends on 12)

The method of claim 12, wherein the produced solution is cooled to a temperature below the crystallization temperature of lithium hydroxide and above the crystallization temperature of the sodium hydroxide.

### Claim 16

A system for making lithium hydroxide, comprising:
an electrolysis reaction chamber, wherein the electrolysis reaction chamber includes:
an ion-selective membrane separating a first volume from a second volume in the chamber, wherein the ion-selective membrane selectively allows lithium and sodium ions to pass through the membrane while inhibiting hydroxide ions and chloride ions from passing through the membrane;
an anode positioned in the first volume; and
a cathode positioned in the second volume;
a mixture feed coupled to the first volume, wherein the mixture feed is configured to provide lithium chloride, sodium chloride, and water to the first volume;
a water feed coupled to the second volume;
a power supply coupled to the anode and the cathode, wherein the power supply is configured to provide a selected voltage to the anode and the cathode a first gas outlet coupled to the first volume, wherein the first gas outlet is configured to output chlorine gas from the first volume;
a second gas outlet coupled to the second volume, wherein the second gas outlet is configured to output hydrogen gas from the second volume; and
a first liquid outlet coupled to the first volume, wherein the first liquid outlet is configured to output lithium chloride, sodium chloride, and water with a lower volume percentage of lithium chloride and sodium chloride than the mixture feed; and
a second liquid outlet coupled to the second volume, wherein the second liquid outlet is configured to output lithium hydroxide, sodium hydroxide, and water with a higher percentage of lithium hydroxide and sodium hydroxide than the mixture feed from the second volume.

### Claim 17 (depends on 16)

The system of claim 16, wherein the ion-selective membrane has a selectivity for lithium and sodium ions determined by at least one of the ion exchange capacity of the membrane, the degree of hydration of the membrane, or a pore size in the membrane.

### Claim 18 (depends on 16)

The system of claim 16, wherein the cathode has a coating of inert metal compounds or transition metal compounds.

### Claim 19 (depends on 16)

The system of claim 16, wherein the anode has a coating of inert metal compounds or transition metal compounds.

### Claim 20 (depends on 16)

The system of claim 16, further comprising:
a cooling tank coupled to the second liquid outlet, wherein the cooling tank is configured to cool a solution of lithium hydroxide, sodium hydroxide, and water to a temperature below the crystallization temperature of lithium hydroxide and above the crystallization temperature of the sodium hydroxide; and
a filter coupled to the cooling tank, wherein the filter is configured to remove crystallized lithium hydroxide from the solution of lithium hydroxide, sodium hydroxide, and water.