# US 2023/0272501 A1 · Welding base metal for recycling railway wheel and method for recycling railway wheel using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272501 A1
- Document ID: US20230272501A1
- Status: Published application
- Kind: A1
- Application number: 18/120,222
- Filed: 2023-03-10
- Published: 2023-08-31
- Earliest claimed: 2019-11-26
- Assignees: Asiatech Co., Ltd.
- Applicants: Asiatech Co., Ltd.
- Inventors: Young Jin LEE
- Web page: https://patentgrep.com/patent/US20230272501A1

## CPC

- C21D 9/50: for welded joints
- B60B 17/0006: {Construction of wheel bodies, e.g. disc wheels (B60B17/0003 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C22C 38/02: containing silicon
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- B60B 17/00: Wheels characterised by rail-engaging elements ({wheel-axle combinations B60B37/00;} of model railways A63H19/22)
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B60B: VEHICLE WHEELS (making wheels or wheel parts by rolling B21H1/00, by forging, hammering or pressing B21K1/28); CASTORS; AXLES FOR WHEELS OR CASTORS; INCREASING WHEEL ADHESION
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure relates to a welding base metal for recycling a railway wheel and a method for recycling a railway wheel using the same, which can overlay-weld a railway wheel with a welding base metal suitable for overlay-welding a railway wheel through a heat treatment, form a surface hardened layer, and strengthen the metal structure of the railway wheel, in order to recycle the railway wheel. The welding base metal for recycling a railway wheel may be used as a surface hardened layer of a railway wheel because the welding base metal has high hardness while exhibiting a similar property to the railway wheel. Furthermore, the welding base metal can change the metal structure of the recycled railway wheel, and thus delay the initial wear time of the recycled railway wheel. The method for recycling a railway wheel may overlay-weld the damaged railway wheel to its original size, form a surface hardened layer, and change the metal structure of the railway wheel by changing the composition of the welding base metal and performing the pre-heat treatment and the post heat treatment, thereby minimizing the occurrence of damage to the recycled railway wheel.

## Claims

### Claim 1

A method for recycling a railway wheel, comprising:
a railway wheel overlay-welding step of overlay-welding a worn railway wheel by welding the worn railway wheel with a first welding base metal; and
a surface hardened layer forming step of forming a surface hardened layer by welding the overlay-welded railway wheel with a second welding base metal,
wherein the first welding base metal contains carbon of 0.05 to 0.15 wt %, silicon 0.2 to 1.0 wt %, manganese 1.0 to 2.0 wt %, chromium 0.6 to 1.2 wt %, inevitable impurities and the remainder of iron,
wherein the second welding base metal contains carbon of 0.1 to 0.25 wt %, silicon 1.0 to 2.0 wt %, manganese of 2.2 to 3.3 wt %, nickel 0.45 to 0.65 wt %, chromium 0.85 to 2.45 wt %, molybdenum 0.01 to 0.4 wt %, titanium 0.01 to 0.05 wt %, vanadium 0.03 to 0.1 wt %, niobium 0.01 to 0.1 wt %, inevitable impurities and the remainder of iron,
wherein the railway wheel is a railway wheel of any one of a freight car, a passenger car, an urban railway train and a subway train.

### Claim 2 (depends on 1)

The method of claim 1, wherein the welding in the railway wheel overlay-welding step and the surface hardened layer forming step is performed by any one of gas shield welding, open arc welding, submerged arc welding and automatic welding.

### Claim 3 (depends on 1)

The method of claim 1, further comprising a railway wheel pre-heating step of pre-heating the worn railway wheel, before the railway wheel overlay-welding step.

### Claim 4 (depends on 3)

The method of claim 3, wherein the railway wheel pre-heating step is performed in a temperature range of 250° C. to 300° C.

### Claim 5 (depends on 1)

The method of claim 1, further comprising a railway wheel post heat treatment step of post heat-treating the welded railway wheel, after the surface hardened layer forming step.

### Claim 6 (depends on 5)

The method of claim 5, wherein the railway wheel post heat treatment step is performed in a temperature range of 240° C. to 260° C. for four hours.

### Claim 7 (depends on 6)

The method of claim 6, further comprising, after the railway wheel post heat treatment step is performed in a temperature range of 240° C. to 260° C. for four hours:
slowly cooling the railway wheel at a temperature of 260° C. at a speed of 40° C. per hour for four hours until the temperature of the railway wheel becomes 100° C.; and
slowing cooling the railway wheel under the atmospheric condition while the temperature is maintained at 100° C. or less.

### Claim 8 (depends on 7)

The method of claim 7, further comprising a railway wheel processing step of cutting or grinding the heat-treated railway wheel, after the railway wheel post heat treatment step.

### Claim 9 (depends on 8)

The method of claim 8, wherein the cutting or grinding process is performed by a CNC turning machine.