# US 2023/0272500 A1 · High-strength steel sheet having excellent formability and method for manufacturing thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272500 A1
- Document ID: US20230272500A1
- Status: Published application
- Kind: A1
- Application number: 18/010,041
- Filed: 2021-06-16
- Published: 2023-08-31
- Earliest claimed: 2020-06-17
- Assignees: Posco
- Applicants: Posco
- Inventors: Sung-Kyu KIM; Jun-Ho PARK; Chang-Hyo SEO; Eul-Yong CHOI; Sang-Ho HAN
- Web page: https://patentgrep.com/patent/US20230272500A1

## CPC

- C21D 9/46: for sheet metals
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/19: by interrupted quenching
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/005: {containing Mn}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/562: {Details}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a high-strength steel sheet suitable for automobile structural members, etc., and a method for manufacturing same, wherein the high-strength steel sheet has a low yield ratio and high strength and has excellent formability through improvement of ductility that may prevent processing defects such as cracks, wrinkles, or the like, during press forming.

## Claims

### Claim 1

A high-strength steel sheet having excellent formability comprising, by weight %:
0.05 to 0.15% of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 2.0 to 3.0% of manganese (Mn), 0.2% or less (excluding 0%) of titanium (Ti), 0.1% or less (excluding 0%) of niobium (Nb), 0.2% or less (excluding 0%) of vanadium (V), 0.5% or less (excluding 0%) of molybdenum (Mo), 0.1% or less of phosphorus (P), 0.01% or less of sulfur (S), and a remainder of Fe and other unavoidable impurities,
wherein a microstructure is composed of ferrite with an area fraction of 20 to 45%, and a remainder of martensite and bainite, and
a fraction of non-recrystallized ferrite, among the ferrite is 25 area% or less, and an average aspect ratio thereof (major axis: minor axis) is 1.1 to 2:1.

### Claim 2 (depends on 1)

The high-strength steel sheet having excellent formability of claim 1, wherein the martensite is contained in an area fraction of 10% or less (excluding 0%).

### Claim 3 (depends on 1)

The high-strength steel sheet having excellent formability of claim 1, wherein the steel sheet has a tensile strength of 980 MPa or more, a yield strength of 680 MPa or less, and an elongation of 13% or more.

### Claim 4 (depends on 1)

The high-strength steel sheet having excellent formability of claim 1, wherein the steel sheet has a yield ratio of 0.8 or less.

### Claim 5

A method for manufacturing a high-strength steel sheet having excellent formability, comprising:
an operation of heating a steel slab including, by wt%:
0.05 to 0.15% of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 2.0 to 3.0% of manganese (Mn), 0.2% or less (excluding 0%) of titanium (Ti), 0.1% or less (excluding 0%) of niobium (Nb), 0.2% or less (excluding 0%) of vanadium (V), 0.5% or less (excluding 0%) of molybdenum (Mo), 0.1% or less of phosphorus (P), 0.01% or less of sulfur (S), and a remainder of Fe and other unavoidable impurities,
an operation of manufacturing a hot-rolled steel sheet by finishing hot rolling the heated slab at an outlet temperature of Ar3 or higher to 1000° C. or lower;
an operation of coiling the hot-rolled steel sheet in a temperature range of 400 to 700° C.;
an operation of cooling the hot-rolled steel sheet to room temperature after the coiling operation;
an operation of manufacturing a cold-rolled steel sheet by cold rolling the hot-rolled steel sheet at a reduction ratio of 40 to 70% after the cooling operation;
an operation of continuous annealing of the cold-rolled steel sheet;
an operation of primary cooling the cold-rolled steel sheet to a temperature range of 650 to 700° C. after the continuous annealing operation; and
an operation of secondary cooling the cold-rolled steel sheet to a temperature range of 300 to 580° C. after the primary cooling operation,
wherein the continuous annealing operation is performed in a facility equipped with a heating section, a soaking section, and a cooling section, and an end temperature in the heating section is higher than an end temperature in the soaking section by 10° C. or higher.

### Claim 6 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5,
wherein the end temperatures of the heating section and the soaking section satisfies the following relational expression, [Relational Expression]
10
≤
End temperature in heating section - End
temperature in soaking section
°
C
≤
40.
.

### Claim 7 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5, wherein the end temperature in the heating section is 790 to 830° C., and the end temperature in the soaking section is 760 to 790° C.

### Claim 8 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5, wherein the operation of heating the steel slab is performed in a temperature range of 1100 to 1300° C.

### Claim 9 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5, wherein the operation of cooling after the coiling operation is performed at an average cooling rate of 0.1° C./s or less (excluding 0° C./s).

### Claim 10 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5, wherein the primary cooling operation is performed at an average cooling rate of 1 to 10° C./s, and
the secondary cooling operation is performed at an average cooling rate of 5 to 50° C./s.

### Claim 11 (depends on 5)

The method for manufacturing a high-strength steel sheet having excellent formability of claim 5, further comprising:
an operation of performing over-aging treatment after performing the secondary cooling operation,
wherein the over-aging treatment is performed for 200 to 800 seconds.