# US 2023/0272499 A1 · Process for manufacturing high strength steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272499 A1
- Document ID: US20230272499A1
- Status: Published application
- Kind: A1
- Application number: 17/993,700
- Filed: 2022-11-23
- Published: 2023-08-31
- Earliest claimed: 2021-11-24
- Assignees: United States Steel Corporation
- Applicants: United States Steel Corporation
- Inventors: Matthew J. Merwin
- Web page: https://patentgrep.com/patent/US20230272499A1

## CPC

- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 9/46: for sheet metals
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 1/19: by interrupted quenching
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/26: Methods of annealing
- C21D 6/02: Hardening by precipitation
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/021: involving particular fabrication steps or treatments of ingots or slabs
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/002: Bainite
- C21D 2211/004: Dispersions; Precipitations
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method of making high strength steel sheet with a tensile strength of 800 to 1000 MPa and a hole expansion ratio of at least 50%, comprising the steps of reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3; hot rolling the slab to final desired thickness; cooling the steel sheet at a rate of 50° C. per second to a temperature less than 400° C.; and winding the steel sheet into a coil.

## Claims

### Claim 1

A method of making high strength steel sheet with a tensile strength of 800 to 1100 MPa and a hole expansion ratio of at least 50%, comprising the steps of:
reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3;
hot rolling the slab to final desired thickness; cooling the steel sheet at a rate of 50° C. per second to a temperature less than 400° C.; and
winding the steel sheet into a coil.

### Claim 2 (depends on 1)

The method of making high strength steel according to claim 1, wherein the temperature Ar3 is a temperature greater than the austenite-to-ferrite transformation temperature.

### Claim 3 (depends on 1)

The method of making high strength steel according to claim 1, further comprising cooling the steel sheet to an acicular ferrite structure.

### Claim 4 (depends on 1)

The method of making high strength steel according to claim 1, further comprising cooling the steel sheet to a bainitic structure.

### Claim 5 (depends on 1)

The method of making high strength steel according to claim 1, further comprising the application of a secondary treatment to the steel sheet to promote precipitation reactions for strength preservation or an increase in strength.

### Claim 6 (depends on 5)

The method of making high strength steel according to claim 5, further comprising reheating the steel coil to a temperature below Ac1.

### Claim 7 (depends on 6)

The method of making high strength steel according to claim 6, wherein the temperature Ac1 is a temperature above 500° C. and below the ferrite-to-austenite phase transformation temperature.

### Claim 8 (depends on 6)

The method of making high strength steel according to claim 6, wherein the temperature depends on a time duration anticipated for a process employed.

### Claim 9 (depends on 6)

The method of making high strength steel according to claim 6, further comprising continuous annealing of the steel sheet to achieve reduced heating times.

### Claim 10 (depends on 9)

The method of making high strength steel according to claim 9, wherein the reduced duration of the heating time during the continuous annealing allows for the steel sheet to approach a temperature Ac1 temperature while achieving the desired properties.

### Claim 11

A method of making high strength steel sheet having a tensile strength of approximately 800 MPa and a composition of 0.06 weight percent of Carbon, 1.0 weight percent of Mn and 0.1 weight percent of Si, 0.03 weight percent of Ti and 0.0020 weight percent of boron, comprising the steps of:
reheating a previously cast slab, or retaining the heat from a directly cast slab, above Ar3;
than 400° C.; and
hot rolling the slab to final desired thickness;
cooling the steel sheet at a rate of 50° C. per second to a temperature less winding the steel sheet into a coil.

### Claim 12 (depends on 11)

The method of making high strength steel according to claim 11, further comprising cooling the steel sheet to an acicular ferrite.

### Claim 13 (depends on 11)

The method of making high strength steel according to claim 11, further comprising a applying a secondary treatment to the steel sheet to promote precipitation reactions for strength preservation or an increase in strength.

### Claim 14 (depends on 13)

The method of making high strength steel according to claim 13, further comprising reheating the steel coil to a temperature below Act.

### Claim 15 (depends on 14)

The method of making high strength steel according to claim 14, wherein the temperature Ac1 is a temperature above 500° C. and below the ferrite-to-austenite phase transformation temperature.

### Claim 16 (depends on 11)

The method of making high strength steel according to claim 11, wherein the temperature depends on a time duration anticipated for a process employed.

### Claim 17 (depends on 11)

The method of making high strength steel according to claim 11, further comprising continuous annealing of the steel sheet to achieve reduced heating times.

### Claim 18 (depends on 17)

The method of making high strength steel according to claim 17, wherein the reduced duration of the heating time during the continuous annealing allows for the steel sheet to approach a temperature Ac1 temperature while achieving the desired properties.

### Claim 19

A method of making high strength steel sheet a tensile strength of approximately 1000 MPa and a composition 0.06 weight percent of C, 1.0 weight percent of Mn, 0.1 weight percent of Si, 0.03 weight percent of Ti and 0.0020 weight percent of B, comprising the steps of:
slab, above Ar3;
than 400° C.; and
reheating a previously cast slab, or retaining the heat from a directly cast hot rolling the slab to final desired thickness;
cooling the steel sheet at a rate of 50° C. per second to a temperature less winding the steel sheet into a coil.