# US 2023/0272278 A1 · Etching composition for etching molybdenum film and method of manufacturing integrated circuit device using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272278 A1
- Document ID: US20230272278A1
- Status: Published application
- Kind: A1
- Application number: 18/081,899
- Filed: 2022-12-15
- Published: 2023-08-31
- Earliest claimed: 2022-02-25
- Assignees: Soulbrain Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Changjun PARK; Jaesung LEE; Junghun LIM; Mihyun PARK; Sangwon BAE; Jungmin OH; Hyosan LEE
- Web page: https://patentgrep.com/patent/US20230272278A1

## CPC

- C09K 13/06: with organic material
- C23F 1/30: for etching other metallic material
- C23F 11/04: in markedly acid liquids
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10D 64/665: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. tungsten or molybdenum (having lateral variation H10D64/671)}
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P 50/667: {by liquid etching only}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An etching composition for etching a molybdenum film, the etching composition includes about 0.1 wt % to about 5 wt % of an oxidant; about 10 wt % to about 40 wt % of a chelate agent, the chelate agent including a mineral acid; about 0.01 wt % to about 3 wt % of a corrosion inhibitor, the corrosion inhibitor including an ammonium salt, an amine compound, or a combination thereof; and an organic solvent, all wt % being based on a total weight of the etching composition.

## Claims

### Claim 1

An etching composition for etching a molybdenum film, the etching composition comprising:
about 0.1 wt % to about 5 wt % of an oxidant;
about 10 wt % to about 40 wt % of a chelate agent, the chelate agent including a mineral acid;
about 0.01 wt % to about 3 wt % of a corrosion inhibitor, the corrosion inhibitor including an ammonium salt, an amine compound, or a combination thereof; and
an organic solvent, all wt % being based on a total weight of the etching composition.

### Claim 2 (depends on 1)

The etching composition as claimed in claim 1, wherein the oxidant includes nitric acid, sulfuric acid, perchloric acid, ammonium persulfate, methanesulfonic acid, paratoluenesulfonic acid, or a combination thereof.

### Claim 3 (depends on 1)

The etching composition as claimed in claim 1, wherein the chelate agent includes phosphoric acid, a phosphoric acid salt, phosphonic acid, a phosphonic acid salt, or a combination thereof.

### Claim 4 (depends on 1)

The etching composition as claimed in claim 1, wherein:
the ammonium salt includes monoammonium phosphate, diammonium phosphate, triammonium phosphate, ammonium chloride, ammonium acetate, ammonium carbonate, ammonium nitrate, ammonium sulfate, or a combination thereof, and
the amine compound includes a C1-C8 aliphatic amine compound or a 5-membered to 8-membered cyclic amine compound.

### Claim 5 (depends on 1)

The etching composition as claimed in claim 1, wherein the organic solvent is a non-aqueous organic solvent, the non-aqueous organic solvent including a C1-C5 carboxylic acid compound, a C1-C5 alcohol compound, a C1-C5 carbonic acid ester compound, or a combination thereof.

### Claim 6 (depends on 1)

The etching composition as claimed in claim 1, further comprising greater than about 0 wt % and less than about 1 wt % of water, based on the total weight of the etching composition.

### Claim 7

A method of manufacturing an integrated circuit device, the method comprising:
forming, on a substrate, an insulating film structure defining a plurality of spaces arranged apart from each other;
forming a molybdenum film filling the plurality of spaces and covering the insulating film structure; and
removing a part of the molybdenum film from outside of the plurality of spaces by using an etching composition to obtain a plurality of molybdenum patterns filling the plurality of spaces and spaced apart from each other,
wherein the etching composition includes:
about 0.1 wt % to about 5 wt % of an oxidant;
about 10 wt % to about 40 wt % of a chelate agent, the chelate agent including a mineral acid;
about 0.01 wt % to about 3 wt % of a corrosion inhibitor, the corrosion inhibitor including an ammonium salt, an amine compound, or a combination thereof; and
an organic solvent, all wt % being based on a total weight of the etching composition.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein removing the part of the molybdenum film includes etching the molybdenum film at an etching speed of less than about 10 Å/min.

### Claim 9 (depends on 7)

The method as claimed in claim 7, wherein removing the part of the molybdenum film is performed at a temperature ranging from about 10° C. to about 30° C.

### Claim 10 (depends on 7)

The method as claimed in claim 7, wherein the plurality of spaces extend in a direction parallel with a main surface of the substrate and overlap each other in a direction perpendicular to the main surface of the substrate.

### Claim 11 (depends on 7)

The method as claimed in claim 7, wherein the oxidant in the etching composition includes nitric acid, sulfuric acid, perchloric acid, ammonium persulfate, methanesulfonic acid, paratoluenesulfonic acid, or a combination thereof.

### Claim 12 (depends on 7)

The method as claimed in claim 7, wherein the chelate agent in the etching composition includes phosphoric acid, a phosphoric acid salt, phosphonic acid, a phosphonic acid salt, or a combination thereof.

### Claim 13 (depends on 7)

The method as claimed in claim 7, wherein:
the ammonium salt includes monoammonium phosphate, diammonium phosphate, triammonium phosphate, ammonium chloride, ammonium acetate, ammonium carbonate, ammonium nitrate, ammonium sulfate, or a combination thereof, and
the amine compound includes a C1-C8 aliphatic amine compound or a 5-membered to 8-membered cyclic amine compound.

### Claim 14 (depends on 7)

The method as claimed in claim 7, wherein the organic solvent is a non-aqueous organic solvent, the non-aqueous organic solvent including a C1-C5 carboxylic acid compound, a C1-05 alcohol compound, a C1-C5 carbonic acid ester compound, or a combination thereof.

### Claim 15 (depends on 7)

The method as claimed in claim 7, wherein the etching composition further includes greater than about 0 wt % and less than about 1 wt % of water, based on the total weight of the etching composition.

### Claim 16

A method of manufacturing an integrated circuit device, the method comprising:
forming, on a substrate, a structure in which a plurality of first films and a plurality of second films are stacked alternately one by one;
forming a channel hole penetrating the structure in a vertical direction;
forming a channel structure in the channel hole;
forming a word line cut area penetrating the structure in the vertical direction and extending in a shape of a line in a first horizontal direction;
forming a plurality of word line spaces by removing the plurality of first films exposed in the word line cut area;
forming a molybdenum film filling the plurality of word line spaces and covering surfaces of the plurality of second films exposed in the word line cut area; and
removing a part of the molybdenum film by applying an etching composition through the word line cut area to obtain a plurality of word lines including a plurality of molybdenum patterns filling the plurality of word line spaces and arranged apart from each other,
wherein the etching composition includes:
about 0.1 wt % to about 5 wt % of an oxidant;
about 10 wt % to about 40 wt % of a chelate agent, the chelate agent including a mineral acid;
about 0.01 wt % to about 3 wt % of a corrosion inhibitor, the corrosion inhibitor including an ammonium salt, an amine compound, or a combination thereof; and
an organic solvent, all wt % being based on a total weight of the etching composition.

### Claim 17 (depends on 16)

The method as claimed in claim 16, further comprising, after forming the plurality of word line spaces and before the forming of the molybdenum film, forming a dielectric thin film conformally covering the surfaces of the plurality of second films and a surface of the channel structure, which are exposed in the plurality of word line spaces and the word line cut area,
wherein:
forming the molybdenum film includes forming the molybdenum film to fill spaces limited by the dielectric thin film, of the plurality of word line spaces, and after removing the part of the molybdenum film, parts of the dielectric thin film which cover the surfaces of the plurality of second films in the word line cut area are exposed.

### Claim 18 (depends on 16)

The method as claimed in claim 16, wherein removing the part of the molybdenum film includes etching the molybdenum film at an etching speed of less than about 10 Å/min.

### Claim 19 (depends on 16)

The method as claimed in claim 16, wherein:
the oxidant includes nitric acid,
the chelate agent includes phosphoric anhydride,
the corrosion inhibitor includes an aliphatic polyamine, and
the organic solvent is a non-aqueous organic solvent, the non-aqueous organic solvent including a C1-C5 carboxylic acid compound.

### Claim 20 (depends on 16)

The method as claimed in claim 16, wherein the etching composition further includes greater than about 0 wt % and less than about 1 wt % of water, based on the total weight of the etching composition.