# US 2023/0272207 A1 · Thermoplastic Resin Composition and Molded Article Produced Therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272207 A1
- Document ID: US20230272207A1
- Status: Published application
- Kind: A1
- Application number: 17/802,232
- Filed: 2021-02-22
- Published: 2023-08-31
- Earliest claimed: 2020-02-28
- Assignees: Lotte Chemical Corporation
- Applicants: Lotte Chemical Corporation
- Inventors: Sanghyun HONG; Hanna KIM; Bongjun SONG; Youngsub JIN; Wonyoung CHOI
- Web page: https://patentgrep.com/patent/US20230272207A1

## CPC

- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08F 222/06: Maleic anhydride
- C08G 65/08: Saturated oxiranes
- C08G 69/14: Lactams
- C08G 69/44: Polyester-amides
- C08L 25/12: with unsaturated nitriles
- C08L 71/12: Polyphenylene oxides
- C08L 77/02: Polyamides derived from omega-amino carboxylic acids or from lactams thereof (C08L77/10 takes precedence)
- C08G 69/08: derived from amino-carboxylic acids
- C08G 69/40: Polyamides containing oxygen in the form of ether groups (C08G69/12, C08G69/32 take precedence)
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/53: Core-shell polymer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The present invention relates to a thermoplastic resin composition and a molded article produced therefrom, the thermoplastic resin composition including, based on 100 parts by weight of a base resin including (A1) 20 to 40 wt% of a butadiene-based rubber-modified aromatic vinyl-vinyl cyanide graft copolymer, (A2) 30 to 75 wt% of an aromatic vinyl-vinyl cyanide copolymer, and (B) 5 to 40 wt% of a polyamide resin, (C) 1 to 15 parts by weight of a polyether ester amide block copolymer, and (D) 0.5 to 10 parts by weight of a maleic anhydride-aromatic vinyl-vinyl cyanide copolymer.

## Claims

### Claim 1

A thermoplastic resin composition, comprising:
based on 100 parts by weight of a base resin including (A1) 20 to 40 wt% of a butadiene-based rubber-modified aromatic vinyl-vinyl cyanide graft copolymer;
(A2) 30 to 75 wt% of an aromatic vinyl-vinyl cyanide copolymer; and
(B) 5 to 40 wt% of a polyamide resin;
(C) 1 to 15 parts by weight of a polyether ester amide block copolymer; and
(D) 0.5 to 10 parts by weight of a maleic anhydride-aromatic vinyl-vinyl cyanide copolymer.

### Claim 2 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (A1) butadiene-based rubber-modified aromatic vinyl-vinyl cyanide graft copolymer has a core-shell structure including
a core of a butadiene-based rubbery polymer, and
a shell formed by graft polymerization of an aromatic vinyl compound and a vinyl cyanide compound.

### Claim 3 (depends on 2)

The thermoplastic resin composition of claim 2, wherein
in the (A1) butadiene-based rubber-modified aromatic vinyl-vinyl cyanide graft copolymer, an average particle diameter of the butadiene-based rubbery polymer is 0.2 to 1.0 µm.

### Claim 4 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (A1) butadiene-based rubber-modified aromatic vinyl-vinyl cyanide graft copolymer is an acrylonitrile-butadiene-styrene copolymer.

### Claim 5 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (A2) aromatic vinyl-vinyl cyanide copolymer includes 55 to 80 wt% of a component derived from an aromatic vinyl compound and 20 to 45 wt% of a component derived from a vinyl cyanide compound based on 100 wt%.

### Claim 6 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (A2) aromatic vinyl-vinyl cyanide copolymer has a weight average molecular weight of 80,000 to 300,000 g/mol.

### Claim 7 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (A2) aromatic vinyl-vinyl cyanide copolymer is a styrene-acrylonitrile copolymer.

### Claim 8 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (B) polyamide resin includes polyamide 6, polyamide 66, polyamide 46, polyamide 11, polyamide 12, polyamide 610, polyamide 612, polyamide 6I, polyamide 6T, polyamide 4T, polyamide 410, polyamide 510, polyamide 1010, polyamide 1012, polyamide 10T, polyamide 1212, polyamide 12T, polyamide MXD6, or a combination thereof.

### Claim 9 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (C) polyether ester amide block copolymer is a reaction mixture of an aminocarboxylic acid, lactam, or a diamine-dicarboxylic acid salt having 6 or more carbon atoms; polyalkylene glycol; and a dicarboxylic acid having 4 to 20 carbon atoms.

### Claim 10 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the (D) maleic anhydride-aromatic vinyl-vinyl cyanide copolymer is a maleic anhydride-styrene-acrylonitrile copolymer.

### Claim 11 (depends on 1)

The thermoplastic resin composition of claim 1, wherein
the thermoplastic resin composition further includes at least one additive selected from a nucleating agent, a coupling agent, a filler, a plasticizer, a lubricant, a mold release agent, an antibacterial agent, a heat stabilizer, an antioxidant, an ultraviolet stabilizer, a flame retardant, a colorant, and an impact modifier.

### Claim 12 (depends on 1)

A molded article produced from the thermoplastic resin composition of claim 1.

### Claim 13 (depends on 12)

The molded article of claim 12, wherein
the molded article has a notched Izod impact strength of a ¼″-thick specimen according to ASTM D256 ranging from 20 to 60 kgf·cm/cm.

### Claim 14 (depends on 12)

The molded article of claim 12, wherein
the molded article has surface resistance of less than or equal to 1012.0 Ω/sq measured for a 100 mm x 100 mm x 20 mm specimen using a surface resistance measuring device (manufacturer: SIMCO-ION, model name: Worksurface Tester ST-4).

### Claim 15 (depends on 12)

The molded article of claim 12, wherein
the molded article has a heat deflection temperature (HDT) of 80 to 100° C. according to ASTM D648.