# US 2023/0272200 A1 · Polymer composition with improved flowability and falling weight impact resistance at low temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272200 A1
- Document ID: US20230272200A1
- Status: Published application
- Kind: A1
- Application number: 18/013,467
- Filed: 2021-06-28
- Published: 2023-08-31
- Earliest claimed: 2020-06-29
- Assignees: Sabic Global Technologies B.V.
- Applicants: Sabic Global Technologies B.V.
- Inventors: Ting Huang; Christelle Marie, Helene GREIN; Chaodong JIANG; Weisong GAO
- Web page: https://patentgrep.com/patent/US20230272200A1

## CPC

- C08L 23/12: Polypropene
- H01Q 1/42: Housings not intimately mechanically associated with radiating elements, e.g. radome
- B29B 7/002: {Methods (chemical aspects C08J3/00)}
- B29B 7/726: {Measuring properties of mixture, e.g. temperature or density (B29B7/724 takes precedence)}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- B29B 9/14: fibre-reinforced
- B29C 45/0001: {characterised by the choice of material}
- B29C 45/0005: {using fibre reinforcements}
- C08K 7/14: Glass
- B29B 9/06: in the form of filamentary material, e.g. combined with extrusion
- B29K 2021/003: {Thermoplastic elastomers}
- B29K 2023/08: {Copolymers of ethylene (B29K2023/16 takes precedence)}
- B29K 2023/10: {Polymers of propylene}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29L 2031/3456: {Antennas, e.g. radomes}
- C08L 2203/206: use in coating or encapsulating of electronic parts
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C08L 2207/064: VLDPE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01Q: ANTENNAS, i.e. RADIO AERIALS (radiators or antennas for microwave heating H05B6/72)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The present invention relates to a polymer composition comprising a polypropylene, an ethylene based elastomer, a grafted polypropylene and glass fiber. The polymer composition according to the present invention has improved flowability and falling weight impact resistance at low temperature.

## Claims

### Claim 1

A polymer composition comprising a polypropylene, an ethylene based elastomer, a grafted polypropylene and glass fiber, wherein the polypropylene has a melt flow index (MFI) in the range from 17 to 68 dg/min as measured according to ISO1133-1:2011 at 230° C./ 2.16 kg,wherein the amount of the ethylene based elastomer is in the range from 15.5 to 28.3 wt% based on the total amount of the polymer composition, wherein the MFI of the ethylene based elastomer is in the range of 0.8 to 36 dg/min as measured according to ISO1133-1:2011 at 190° C./2.16 kg wherein amount of grafted polypropylene is in the range from 1.2 to 2.9 wt%
based on the total amount of the polymer composition.

### Claim 2 (depends on 1)

The polymer composition according to claim 1, wherein the MFI of the polypropylene is in the range from 23 to 59 dg/min, as measured according to ISO1133-1:2011 at 230° C./2.16 kg.

### Claim 3 (depends on 1)

The polymer composition according to claim 1, wherein the polypropylene comprises an ethylene-α-olefin copolymer, wherein the amount of the ethylene α-olefin copolymer is in the range from 13 to 28 wt% based on the total amount of the polypropylene.

### Claim 4 (depends on 1)

The polymer composition according to claim 1, wherein the ethylene based elastomer is selected from the group consisting of ethylene-butene copolymer, ethylene- hexene copolymer, ethylene-octene copolymer and a combination thereof.

### Claim 5 (depends on 1)

The polymer composition according to claim 1, wherein the shore A hardness of the ethylene based elastomer is in the range from 35 to 90, as measured according to ASTM D2240-15, 1 s.

### Claim 6 (depends on 1)

The polymer composition according to claim 1, wherein the grafted polypropylene is a maleic anhydrate grafted polypropylene.

### Claim 7 (depends on 1)

The polymer composition according to claim 1, wherein the diameter of the glass fibers is in the range from 5 to 50 microns.

### Claim 8 (depends on 1)

The polymer composition according to claim 1, wherein the amount of the glass fiber is in the range from 16 to 42 wt%, based on the total amount of the polymer composition.

### Claim 9 (depends on 1)

The polymer composition according to claim 1, wherein the amount of the polypropylene is in the range from 26 to 76 wt%, based on the total amount of the polymer composition.

### Claim 10 (depends on 1)

The polymer composition according to claim 1, wherein the density of the ethylene based elastomer is in the range from 0.845 to 0.883 g/cm3, as measured according to ASTM D792-13.

### Claim 11 (depends on 1)

The polymer composition according to claim 1, wherein the MFI of the ethylene based elastomer is in the range from 0.9 to 23 dg/min, as measured according to ISO1133-1:2011 at 190° C./2.16 kg.

### Claim 12 (depends on 1)

The polymer composition according to claim 1, wherein the grafted polypropylene has an MFI in the range from 150 to 600 dg/min, as measured according to ISO1133-1:2011 at 230° C./2.16 kg.

### Claim 13 (depends on 1)

An antenna housing comprising the polymer composition of claim 1, wherein the amount of the polymer composition is at least 95 wt%, of the total amount of the antenna housing.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

A process for the preparation of an antenna housing comprising the following sequential steps:
providing the polymer composition of any one of claims 1 to 12 in pellet form; and
injection moulding the polymer composition from the previous step into an antenna housing.

### Claim 15

(canceled)

### Claim 16 (depends on 1)

The polymer composition according to claim 1, wherein the polyolefin based elastomer is an ethylene-octene copolymer.