# US 2023/0272184 A1 · Ultra-Low Wear Magnetic Polymer Composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272184 A1
- Document ID: US20230272184A1
- Status: Published application
- Kind: A1
- Application number: 18/133,826
- Filed: 2023-04-12
- Published: 2023-08-31
- Earliest claimed: 2022-04-12
- Assignees: National Technology & Engineering Solutions of Sandia, LLC
- Applicants: National Technology & Engineering Solutions of Sandia, LLC; Lehigh University
- Inventors: Tomas Farley Babuska; Andrew Kustas; Tomas Grejtak
- Web page: https://patentgrep.com/patent/US20230272184A1

## CPC

- C08K 3/11: Compounds containing metals of Groups 4 to 10 or of Groups 14 to 16 of the Periodic Table
- C08F 114/26: Tetrafluoroethene
- C08K 3/08: Metals
- C08K 2003/0856: {Iron}
- C08K 2201/01: Magnetic additives
- C08K 2201/011: Nanostructured additives
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Polytetrafluoroethylene filled with FeCo microparticles provides an ultralow wear, magnetic, multifunctional tribological material. For example, PTFE filled with an 5 wt. % of equiatomic, prealloyed FeCo powder resulted in steady state wear rates of 2.7×10−7 mm3/Nm, approaching that of PTFE-filled alumina. Comparable wear rates were not recovered for PTFE filled with just iron or cobalt microparticles.

## Claims

### Claim 1

A low-wear magnetic polymer composite, comprising magnetic alloy particles dispersed in a perfluoropolymer matrix.

### Claim 2 (depends on 1)

The low-wear magnetic polymer composite of claim 1, wherein the magnetic alloy has a yield strength of less than 300 MPa and a strain-to-failure of less than 6%.

### Claim 3 (depends on 1)

The low-wear magnetic polymer composite of claim 1, wherein the magnetic alloy comprises an iron-cobalt intermetallic alloy.

### Claim 4 (depends on 3)

The low-wear magnetic polymer composite of claim 3, wherein the iron-cobalt intermetallic alloy further comprises vanadium, chromium, niobium, molybdenum, and/or nickel.

### Claim 5 (depends on 1)

The low-wear magnetic polymer composite of claim 1, wherein magnetic polymer composite comprises between 1 and 50 wt. % magnetic alloy particles.

### Claim 6 (depends on 1)

The low-wear magnetic polymer composite of claim 1, where the size of the magnetic alloy particles are greater than 100 nm and less than 100 μm.

### Claim 7 (depends on 1)

The low-wear magnetic polymer composite of claim 1, where the perfluoropolymer comprises polytetrafluoroethylene, perfluoroalkoxy alkane, fluorinated ethylene-propylene, or polychlorotrifluoroethylene.

### Claim 8 (depends on 1)

The low-wear magnetic polymer composite of claim 1, wherein the magnetic polymer composite has a steady-state wear rate of less than 1×10−6 mm3/Nm.