# US 2023/0272160 A1 · Process for producing polyester comprising 2,5-furandicarboxylate units

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272160 A1
- Document ID: US20230272160A1
- Status: Published application
- Kind: A1
- Application number: 18/017,874
- Filed: 2021-08-27
- Published: 2023-08-31
- Earliest claimed: 2020-08-27
- Applicants: Furanix Technologies B.V.
- Inventors: Matheus Adrianus Dam; Bing Wang; Hendawy Elfeki
- Web page: https://patentgrep.com/patent/US20230272160A1

## CPC

- C08G 63/863: {Germanium or compounds thereof}
- C08G 63/181: Acids containing aromatic rings
- C08G 63/80: Solid-state polycondensation
- C08G 63/88: Post-polymerisation treatment
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A process for producing a polyester having 2,5-furandicarboxylate units includes: a) providing or producing a starting composition including 2,5-furandicarboxylic acid, an aliphatic diol and a suppressant for suppressing ether formation between the aliphatic diol molecules, b) subjecting the starting composition to esterification conditions to produce an ester composition, and c) contacting the ester composition with a germanium containing catalyst at polycondensation conditions to produce a polyester including 2,5-furandicarboxylate units, where the suppressant includes amines and lithium hydroxide.

## Claims

### Claim 1

A process for producing a polyester comprising 2,5-furandicarboxylate units, which process comprises:
a) providing or producing a starting composition comprising 2,5-furandicarboxylic acid, an aliphatic diol and a suppressant for suppressing ether formation between the aliphatic diol molecules,
b) subjecting the starting composition to esterification conditions to produce an ester composition, and
c) contacting the ester composition with a germanium containing catalyst at polycondensation conditions to produce a polyester comprising 2,5-furandicarboxylate units,
wherein the suppressant is selected from the group consisting of amines and lithium hydroxide.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the aliphatic diol comprises 2 to 8 carbon atoms.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the molar ratio of the aliphatic diol to 2,5-furandicarboxylic acid of the starting composition is in the range of 1.01 to 1.80.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the esterification conditions comprise a temperature in the range of 180 to 260° C. and wherein the polycondensation conditions comprise a temperature in the range of 240 to 300° C.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the starting composition is subjected to esterification conditions in the presence of the germanium containing catalyst.

### Claim 6 (depends on 1)

The process according to claim 1, wherein the germanium containing catalyst is added to the esterification and/or polycondensation as a germanium salt, preferably an organic germanium salt or germanium oxide or a mixture thereof.

### Claim 7 (depends on 1)

The process according to claim 1, wherein the suppressant is selected from the group consisting of primary amines, tertiary amines and lithium hydroxide, more preferably selected from the group consisting of 2-(diethylamino)ethanol, N,N-dimethyldodecylamine, 3-aminocrotonic acid ester with butanediol and lithium hydroxide.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the amount of decarboxylated end groups in the polyester comprising 2,5-furandicarboxylate units after polycondensation determined by 1H-NMR is less than 7 eq/t, preferably less than 6 eq/t, most preferably less than 5 eq/t.

### Claim 9 (depends on 1)

The process according to claim 1, further comprising the steps:
d) crystallizing the polyester comprising 2,5-furandicarboxylate units obtained in step c) to obtain a crystallized polyester comprising 2,5-furandicarboxylate units, and
e) subjecting the crystallized polyester comprising 2,5-furandicarboxylate units produced in step d) to a solid state polymerization for increasing the molecular weight.

### Claim 10 (depends on 9)

The process according to claim 9, wherein the solid state polymerization is conducted at an elevated temperature in the range of Tm−80° C. to Tm−20° C., wherein Tm is the melting point of the polyester comprising 2,5-furandicarboxylate units in ° C. determined in accordance with ISO11357-3.

### Claim 11 (depends on 9)

The process according to claim 9, wherein the crystallization is conducted in an atmosphere with reduced oxygen concentration, preferably under inert gas atmosphere.

### Claim 12 (depends on 1)

A catalyst system for use in a process according to claim 1, comprising a germanium compound, preferably germanium oxide, as a polycondensation catalyst and one or more suppressants, selected from the group consisting of 2-(diethylamino)ethanol, N,N-dimethyldodecylamine, 3-aminocrotonic acid ester with butanediol and lithium hydroxide.

### Claim 13 (depends on 1)

A method comprising:
utilizing a catalyst system comprising a germanium compound, preferably germanium oxide, as a polycondensation catalyst and one or more suppressants, selected from the group consisting of 2-(diethylamino)ethanol, N,N-dimethyldodecylamine, 3-aminocrotonic acid ester with butanediol and lithium hydroxide in a process according to claim 1.

### Claim 14

A polyester comprising 2,5-furandicarboxylate units having a weight average molecular weight after polycondensation of 40 kg/mol or more, determined by gel permeation chromatography with hexafluorisopropanol and 0.05 M potassiumtrifluoroacetate as eluent and calibrated using polymethylmethacrylate standard, wherein the amount of decarboxylated end groups in the polyester is less than 7 eq/t as determined by 1H-NMR using TCE-d2.