# US 2023/0272159 A1 · Resorbable complex shape memory poly(propylene fumarate) star scaffolds for 4d printing applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272159 A1
- Document ID: US20230272159A1
- Status: Published application
- Kind: A1
- Application number: 18/005,643
- Filed: 2021-07-15
- Published: 2023-08-31
- Earliest claimed: 2020-07-15
- Assignees: The University of Akron
- Inventors: Matthew Becker; Garrett Fredric Bass
- Web page: https://patentgrep.com/patent/US20230272159A1

## CPC

- C08G 63/52: Polycarboxylic acids or polyhydroxy compounds in which at least one of the two components contains aliphatic unsaturation
- C08G 63/83: Alkali metals, alkaline earth metals, beryllium, magnesium, copper, silver, gold, zinc, cadmium, mercury, manganese, or compounds thereof {(C08G63/823 takes precedence)}
- C08G 63/918: {Polycarboxylic acids and polyhydroxy compounds in which at least one of the two components contains aliphatic unsaturation}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

In one or more embodiments, the present invention provides am method of making a poly(propylene fumarate-co-succinate) (PPFS) copolymer containing a random incorporation of succinate groups and targetable reduction profiles without the need for three or more monomer units. To achieve this, a time-dependent sonication-promoted zinc/acetic acid reduction of the PPM unsaturated double bonds has been used to create a random PPMS copolymer which may be isomerized into the PPFS equivalent. By changing the sonication time as well as the ratios of acetic acid, zinc, and PPM unsaturated alkenes, partial reduction of the PPM alkenes has been shown to give PPMS products containing varying compositions of succinic and maleate units, which may then be isomerized to the PPFS product.

## Claims

### Claim 1

A method for making poly(propylene fumarate-co-succinate) polymer comprising the time-dependent partial reduction of poly(propylene maleate) double bonds by sonication mediated by zinc and acetic acid to form a poly(propylene maleate-co-succinate) intermediate, followed by isomerization of the poly(propylene maleate-co-succinate) intermediate using an organic base to produce the poly(propylene fumarate-co-succinate) polymer.

### Claim 2 (depends on 1)

The method for producing a poly(propylene fumarate-co-succinate) polymer of claim 1 comprising:
A) obtaining or synthesizing poly(propylene maleate) and dissolving it in acetic acid or a solvent combination comprising acetic acid;
B) adding zinc to the poly(propylene maleate) solution;
C) sonicating the combination of step B to reduce at least some of the maleate groups in the poly(propylene maleate) to succinate groups to form a poly(propylene maleate-co-succinate) intermediate; and
D) dissolving the poly(propylene maleate-co-succinate) intermediate in a suitable solvent and isomerizing it with an organic base to produce a poly(propylene fumarate-co-succinate) polymer.

### Claim 3 (depends on 2)

The method of claim 2 wherein the acetic acid is glacial acetic acid.

### Claim 4 (depends on 2)

The method of claim 2 wherein the solvent combination comprising acetic acid in step A comprises glacial acetic acid and a solvent selected from the group consisting of dichloromethane, chloroform, toluene, and combinations thereof.

### Claim 5 (depends on 2)

The method of claim 2 wherein the solvent combination comprising acetic acid in step A is a co-solvent solution of glacial acetic acid and toluene.

### Claim 6 (depends on 2)

The method of claim 2 wherein the solvent combination comprising acetic acid in step A is a co-solvent solution of glacial acetic acid and one of dichloromethane, chloroform, or both dichloromethane and chloroform.

### Claim 7 (depends on 2)

The method of claim 2 wherein the step of combining (step B) comprises adding an amount of zinc that is from about 0.5 to about 5.0 equivalents relative to the alkene bonds in the PPM polymer.

### Claim 8 (depends on 2)

The method of claim 2 wherein the step of adding zinc (step B) comprises adding an amount of zinc that is from about 0.5 to about 3.0 equivalents relative to the alkene bonds in the PPM polymer.

### Claim 9 (depends on 2)

The method of claim 2 wherein the step of sonication comprises sonicating the combination of step C for from about 1 to about 60 minutes.

### Claim 10 (depends on 2)

The method of claim 2 wherein the step of sonication comprises sonicating the combination of step C until a desired mole percent of succinate groups is present in the poly(propylene maleate-co-succinate) polymer produced.

### Claim 11 (depends on 2)

The method of claim 2 wherein the suitable solvent in the step of dissolving (step D) is an organic solvent.

### Claim 12 (depends on 2)

The method of claim 2 wherein the suitable solvent in the step of dissolving (step D) is selected from the group consisting of chloroform, dichloromethane and combinations thereof.

### Claim 13 (depends on 1)

The method of claim 1 wherein the organic base is selected from the group consisting of diethylamine, trimethylamine, pyridine, and combinations thereof.

### Claim 14 (depends on 2)

The method of claim 2 wherein the organic base in step D is selected from the group consisting of diethylamine, trimethylamine, pyridine, and combinations thereof.

### Claim 15

A method for making a poly(propylene fumarate-co-succinate) polymer comprising the time-dependent partial reduction of poly(propylene fumarate) double bonds by sonication mediated by zinc and acetic acid.

### Claim 16 (depends on 15)

The method for producing poly(propylene fumarate-co-succinate) polymer of claim 15 comprising:
A) obtaining or synthesizing poly(propylene fumarate), dissolving it in acetic acid or a solvent combination comprising acetic acid, and adding zinc; and
B) sonicating the poly(propylene fumarate) solution of step A to reduce at least some of the fumarate groups in the poly(propylene fumarate) to succinate groups to form the poly(propylene fumarate-co-succinate) polymer.

### Claim 17 (depends on 16)

The method of claim 16 wherein the solvent combination comprising acetic acid in step A is a co-solvent solution of glacial acetic acid and one of dichloromethane, chloroform, and both dichloromethane and chloroform.

### Claim 18 (depends on 16)

The method of claim 16 wherein the suitable solvent in step A is a co-solvent solution of glacial acetic acid and toluene.

### Claim 19 (depends on 16)

The method of claim 16 wherein the step of sonication (step B) comprises sonicating the solution of step A for from about 1 to about 60 minutes.

### Claim 20 (depends on 16)

The method of claim 16 wherein the step of sonication (step B) comprises sonicating the solution of step A until a desired mole percent of succinate groups is present in the poly(propylene fumarate-co-succinate) polymer produced.

### Claim 21 (depends on 16)

The method of claim 16 wherein the step of adding (step A) comprises adding an amount of zinc that is from about 0.5 to about 5.0 equivalents relative to the alkene bonds in the PPF polymer.

### Claim 22 (depends on 16)

The method of claim 16 wherein the step of adding (step A) comprises adding an amount of zinc that is from about 0.5 to about 3.0 equivalents relative to the alkene bonds in the PPF polymer.

### Claim 23 (depends on 1)

A poly(propylene fumarate-co-succinate) polymer made according to the method of claim 1.

### Claim 24 (depends on 23)

The poly(propylene fumarate-co-succinate) polymer of claim 23 having at least one of a reduced viscosity and a reduced molar extinction coefficient when compared to a poly(propylene fumarate-co-succinate) polymer of comparable size and succinate content formed by the ring opening copolymerization of propylene oxide, maleic anhydride, and succinic anhydride.