# US 2023/0272145 A1 · Composite fiber and fiber structure containing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272145 A1
- Document ID: US20230272145A1
- Status: Published application
- Kind: A1
- Application number: 18/248,845
- Filed: 2021-10-04
- Published: 2023-08-31
- Earliest claimed: 2020-10-14
- Assignees: Kuraray Trading Co., Ltd.
- Applicants: Kuraray Trading Co., Ltd.
- Inventors: Kohei YAMASAKI; Hitoshi NAKATSUKA; Takayuki IKEDA; Shoji ONOGI
- Web page: https://patentgrep.com/patent/US20230272145A1

## CPC

- C08F 293/00: Macromolecular compounds obtained by polymerisation on to a macromolecule having groups capable of inducing the formation of new polymer chains bound exclusively at one or both ends of the starting macromolecule (on to polymers modified by introduction of unsaturated end groups C08F290/02)
- D01F 8/04: from synthetic polymers
- D01F 8/06: with at least one polyolefin as constituent
- D01F 8/10: with at least one other macromolecular compound obtained by reactions only involving carbon-to-carbon unsaturated bonds as constituent
- D01F 8/12: with at least one polyamide as constituent
- D01F 8/14: with at least one polyester as constituent
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

A composite fiber contains a component A as a core component and a component B at least partially covering the component A. The component A contains a vibration damping elastomer having a peak top intensity of tan δ of 0.5 or more. The component B contains a thermoplastic elastomer having a peak top intensity of tan δ of less than 0.5. The component B covers 70% or more of the cross-sectional perimeter of the component A in the fiber cross-section.

## Claims

### Claim 1

A composite fiber, comprising:
component A as a core component, and
component B at least partially covering the component A,
wherein
the component A comprises a vibration damping elastomer having a peak top intensity of tan δ of 0.5 or more, and the component B comprises a thermoplastic elastomer having a peak top intensity of tan δ of less than 0.5, and
the component B covers 70% or more of the cross-sectional perimeter of the component A in the fiber cross-section.

### Claim 2 (depends on 1)

The composite fiber according to claim 1, wherein a difference between the peak top temperature of tan δ of the component A and the peak top temperature of tan d of the component B is between 0° C. and 85° C., inclusive.

### Claim 3 (depends on 1)

The composite fiber according to claim 1, wherein the peak top of tan δ of the component A is located in the temperature range between −30° C. and 70° C., inclusive.

### Claim at position 4 (depends on 1)

The composite fiber according to claim 1, wherein the peak top intensity of tan δ of the composite fiber is 0.15 or more.

### Claim 5 (depends on 1)

The composite fiber according to claim 1, wherein the vibration damping elastomer is
a block copolymer comprising
a polymer block (a) mainly composed of a vinyl aromatic compound, and
a polymer block (b) mainly composed of a conjugated diene-based compound, and/or
a hydrogenated product thereof.

### Claim 6 (depends on 5)

The composite fiber according to claim 5, satisfying the following (1) and (2):
(1) the content of the polymer block (a) in the block copolymer and/or the hydrogenated product thereof is 1 to 30% by mass, and
(2) the total content of 1,2-bonding units and 3,4-bonding units in the polymer block (b) in the block copolymer and/or the hydrogenated product thereof is 70% by mol or more.

### Claim 7 (depends on 1)

The composite fiber according to claim 1, wherein the vibration damping elastomer is a hydrogenated product of a block copolymer comprising
a polymer block (a) mainly composed of a vinyl aromatic compound, and
a polymer block (b) mainly composed of a conjugated diene-based compound, and
wherein the hydrogenation ratio of the polymer block (b) in the hydrogenated product is 80% by mol or more.

### Claim 8 (depends on 1)

The composite fiber according to claim 1, wherein the thermoplastic elastomer has a glass transition temperature of less than 45° C.

### Claim 9 (depends on 1)

The composite fiber according to claim 1, wherein the thermoplastic elastomer is at least one type selected from the group consisting of a polyamide-based elastomer and a polyester-based elastomer.

### Claim 10 (depends on 1)

A fiber structure, comprising at least a portion of the composite fiber according to claim 1.