# US 2023/0272134 A1 · Polyethylene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0272134 A1
- Document ID: US20230272134A1
- Status: Published application
- Kind: A1
- Application number: 18/019,232
- Filed: 2021-10-21
- Published: 2023-08-31
- Earliest claimed: 2020-10-30
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Christine Jisoo SONG; Jiwon YOON; Yi Young CHOI; Sunghyun PARK
- Web page: https://patentgrep.com/patent/US20230272134A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 4/6592: containing at least one cyclopentadienyl ring, condensed or not, e.g. an indenyl or a fluorenyl ring
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 2410/02: Anti-static agent incorporated into the catalyst
- C08F 2420/01: Cp or analog bridged to a non-Cp X neutral donor
- C08F 2420/08: Heteroatom bridge, i.e. Cp or analog where the bridging atom linking the two Cps or analogs is a heteroatom different from Si
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Provided is a polyethylene. More particularly, provided is a polyethylene which has excellent abrasion resistance and thus is suitable for fiber production.

## Claims

### Claim 1

A polyethylene polymer satisfying the following conditions of 1) to 4):
1) a melt index_(MI) of 0.5 g/10_min to 40 g/10_min, as measured at 190_°C under a load of 2.16 kg according to ASTM D1238;
2) a molecular weight distribution (MWD) of 2.3 to 2.6;
3) a crystallinity of 63% to 71%, as measured using a differential scanning calorimeter (DSC) according to ASTM F2625; and
4) a crystal relaxation temperature (Tcr) of 42° C. to 50° C., as measured using dynamic mechanical analysis (DMA).

### Claim 2 (depends on 1)

The polyethylene polymer of claim 1, wherein the melt index (MI) is 18 g/10_min to 40 g/10_min, as measured at 190_°C under a load of 2.16 kg according to ASTM D1238.

### Claim 3 (depends on 1)

The polyethylene polymer of claim 1, wherein an abrasion resistance is 0.2 mg/cm3 or less, as measured according to ASTM D5264.

### Claim 4 (depends on 1)

The polyethylene polymer of claim 1, wherein the polyethylene polymer is a copolymer of ethylene and an alpha-olefin.

### Claim 5 (depends on 4)

The polyethylene polymer of claim 4, wherein the alpha-olefin includes one or more selected from the group consisting of propylene, 1-butene, 1-pentene, 4-methyl-1-pentene, 1-hexene, 1-heptene, 1-octene, 1-decene, 1-undecene, 1-dodecene, 1-tetradecene, 1-hexadecene, 1-eicosene, norbornene, norbornadiene, ethylidene norbornene, phenyl norbornene, vinyl norbornene, dicyclopentadiene, 1,4-butadiene, 1,5-pentadiene, 1,6-hexadiene, styrene, alpha-methylstyrene, divinylbenzene, and 3-chloromethylstyrene.

### Claim 6 (depends on 1)

The polyethylene polymer of claim 1, wherein the polyethylene polymer is prepared by copolymerizing ethylene and an alpha-olefin in the presence of a catalyst composition including a metallocene compound represented by Chemical Formula 1:
wherein, in Chemical Formula 1,
B is boron,
M is a Group 4 transition metal,
R1 to R4 are each independently hydrogen, C1-20 alkyl, C3-20 cycloalkyl, or C6-20 aryl, or optionally R1 and R2 or R3 and R4 are bonded to each other to form a substituted or unsubstituted C6-60 aromatic ring,
R5 and R6 are each independently C1-20 alkyl, C3-20 cycloalkyl, or C6-20 aryl, or optionally R5 and R6 are connected to each other to form a C3-60 aliphatic ring or a C6-60 aromatic ring,
X1 and X2 are each independently C1-20 alkyl or —O(CO)R′, wherein R′ is C1-20 alkyl,
Q is a substituted or unsubstituted C2-60 hetero ring including any one or more selected from the group consisting of N, O, and S,
Y and Y′ are elements constituting Q,
Y is N, O, or S,
Y′ is N or C.

### Claim 7 (depends on 6)

The polyethylene polymer of claim 6, wherein R1 to R4 are each independently hydrogen or methyl, or optionally R1 and R2 or R3 and R4 are bonded to each other to form a benzene ring or a 1,2,3,4-tetrahydronaphthalene ring, wherein the benzene ring or the 1,2,3,4-tetrahydronaphthalene ring is unsubstituted or substituted with 1 to 4 substituents selected from the group consisting of methyl, tert-butyl, and 4-tert-butyl phenyl.

### Claim 8 (depends on 6)

The polyethylene polymer of claim 6, wherein R5 and R6 are each independently methyl or phenyl, or optionally R5 and R6 are bonded to each other to form a cyclooctane ring.

### Claim 9 (depends on 6)

The polyethylene polymer of claim 6, wherein the compound represented by Chemical Formula 1 is any one of compounds represented by the following structural formulae:
.

### Claim 10 (depends on 6)

The polyethylene polymer of claim 6, wherein the catalyst composition further includes one or more cocatalyst compounds selected from the group consisting of compounds represented by Chemical Formulae 2 to 4:
wherein, in Chemical Formula 2,
R10 is halogen or C1-20 hydrocarbyl substituted or unsubstituted with halogen; and
a is an integer of 2 or more,
wherein, in Chemical Formula 3,
D is aluminum or boron; and
R11 is halogen or C1-20 hydrocarbyl substituted or unsubstituted with halogen,
wherein, in Chemical Formula 4,
L is a neutral or cationic Lewis base;
H is a hydrogen atom;
Z is a group 13 element; and
plural As are each independently C6-20 aryl or C1-20 alkyl, of which one or more hydrogen atoms are substituted with halogen, C1-20 hydrocarbyl, C1-20 alkoxy, or phenoxy.