# US 2023/0271886 A1 · ELECTRO-CONDUCTIVE B4C-TiB2 COMPOSITE CERAMIC AND PREPARATION METHOD THEREOF

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271886 A1
- Document ID: US20230271886A1
- Status: Published application
- Kind: A1
- Application number: 18/301,214
- Filed: 2023-04-15
- Published: 2023-08-31
- Earliest claimed: 2022-05-06
- Assignees: Anhui University of Technology
- Applicants: Anhui University of Technology
- Inventors: Songlin RAN; Jun ZHAO; Xing JIN; Dong WANG; Xiang DING
- Web page: https://patentgrep.com/patent/US20230271886A1

## CPC

- C04B 35/563: based on boron carbide
- C04B 35/645: Pressure sintering
- C04B 35/5611: {based on titanium carbides}
- C04B 35/58071: {based on titanium borides}
- C04B 35/62605: {Treating the starting powders individually or as mixtures}
- C04B 35/62802: {Powder coating materials}
- C04B 35/62828: {Non-oxide ceramics}
- C04B 2235/3813: Refractory metal borides
- C04B 2235/3821: Boron carbides
- C04B 2235/3843: Titanium carbides
- C04B 2235/421: Boron
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/661: Multi-step sintering
- C04B 2235/666: Applying a current during sintering, e.g. plasma sintering [SPS], electrical resistance heating or pulse electric current sintering [PECS]
- C04B 2235/77: Density
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/85: Intergranular or grain boundary phases
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

An electro-conductive B4C—TiB2 has a microstructure in which large B4C grains are coated by small TiB2 grains. The composite ceramic includes 10˜30% by volume of TiB2. A method for preparing the electro-conductive B4C—TiB2 composite ceramic includes: (1) weighing B4C, TiC, and amorphous B powder; (2) mixing evenly and drying thoroughly the powders; and (3) loading the mixed powder into a graphite mold; and placing the graphite mold in a spark plasma sintering furnace for sintering under vacuum, where the sintering is performed at 2000° C. and 50 MPa for 5˜20 min.

## Claims

### Claim 1

An electro-conductive B4C—TiB2 composite ceramic, wherein the electro-conductive B4C—TiB2 composite ceramic has a microstructure in which B4C grains are coated by TiB2 grains; a grain size of the B4C grains is larger than that of the TiB2 grains; and a TiB2 volume percentage in the electro-conductive B4C—TiB2 composite ceramic is 10˜30%;
wherein the electro-conductive B4C—TiB2 composite ceramic is prepared through steps of:
(1) weighing a B4C powder, a TiC powder, and an amorphous B powder according to a preset weight ratio;
wherein a particle size of the B4C powder is 3.0˜20.0 μm; a particle size of the TiC powder is 0.05˜3.0 μm; and a particle size of the amorphous B powder is 0.5˜1.0
(2) mixing the B4C powder, the TiC powder and the amorphous B powder evenly followed by drying to obtain a mixed powder; and
(3) loading the mixed powder into a graphite mold; and transferring the graphite mold to a spark plasma sintering (SPS) furnace followed by sintering under vacuum.

### Claim 2 (depends on 1)

The electro-conductive B4C—TiB2 composite ceramic of claim 1, wherein in step (3), the sintering is performed at 2000° C. and 50 MPa for 5˜20 min.

### Claim 3 (depends on 1)

The electro-conductive B4C—TiB2 composite ceramic of claim 1, wherein a molar ratio of TiC to B is 1:6.6; and a weight ratio of the B4C powder to the TiC powder to the amorphous B powder is 21-69:14-36:16-43.

### Claim 4

A method for preparing an electro-conductive B4C—TiB2 composite ceramic, comprising:
(1) weighing a B4C powder, a TiC powder, and an amorphous B powder according to a preset weight ratio;
wherein a particle size of the B4C powder is 3.0˜20.0 μm; a particle size of the TiC powder is 0.05˜3.0 μm; and a particle size of the amorphous B powder is 0.5˜1.0 μm;
(2) mixing the B4C powder, the TiC powder and the amorphous B powder evenly followed by drying to obtain a mixed powder; and
(3) loading the mixed powder into a graphite mold; and transferring the graphite mold to a spark plasma sintering (SPS) furnace followed by sintering under vacuum.

### Claim 5 (depends on 4)

The method of claim 4, wherein in step (3), the sintering is performed at 2000° C. and 50 MPa for 5˜20 min.

### Claim 6 (depends on 4)

The method of claim 4, wherein a molar ratio of TiC to B is 1:6.6; and a weight ratio of the B4C powder to the TiC powder to the amorphous B powder is 21-69:14-36:16-43.