# US 2023/0271880 A1 · Glass-based articles with sections of different thicknesses

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271880 A1
- Document ID: US20230271880A1
- Status: Published application
- Kind: A1
- Application number: 18/195,599
- Filed: 2023-05-10
- Published: 2023-08-31
- Earliest claimed: 2017-10-10
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Rohit Rai; Ljerka Ukrainczyk
- Web page: https://patentgrep.com/patent/US20230271880A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 21/005: {to introduce in the glass such metals or metallic ions as Ag, Cu}
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 2201/40: containing transition metals other than rare earth metals, e.g. Zr, Nb, Ta or Zn
- C03C 2201/50: containing alkali metals
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Glass-based articles having sections of different thicknesses where a maximum central tension in a thinner section is less than that of a thicker section. The articles comprise an alkali metal oxide having a independent nonzero concentrations that vary along at least a portion of the thickness of each section. Consumer electronic products may comprise the glass-based articles having sections of different thicknesses.

## Claims

### Claim 1

A method of manufacturing a glass-based article comprising:
exposing a glass-based substrate to a bath comprising alkali metal ions to ion-exchange the glass-based substrate for a period of time (t), the glass-based substrate comprising first section having a first thickness (h1) and a second section having a second thickness (h2), the exposing forms the glass-based article comprising:
an alkali metal oxide having a first non-zero concentration that varies in the first section from a first section surface into at least a portion of the first thickness, and the first section having a first stress profile; and
a second non-zero concentration that varies in the second section from a second section surface into at least a portion of the second thickness, and the second section having a second stress profile,
wherein the glass-based substrate comprises a diffusivity D, and 0.01561 h1/D<t<0.18 h2/D.

### Claim 2 (depends on 1)

The method of claim 1, wherein 0.07<sqrt(4Dt/h2)<0.85.

### Claim 3 (depends on 1)

The method of claim 1, wherein 0.18<sqrt(4Dt/h1)<0.67.

### Claim 4 (depends on 3)

The method of claim 3, wherein 0.25<sqrt(4Dt/h1)<0.51.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first stress profile comprises a first central tension region comprising a first maximum central tension (CT1), the second stress profile comprises a second central tension region comprising a second maximum central tension (CT2), and |CT2| is less than |CT1|.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first stress profile comprises a first depth of compression (DOC1), the second stress profile comprises a second depth of compression (DOC2), DOC1>0.15·h1, and DOC2 is in a range from 0.075·h2 to 0.15·h2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first stress profile comprises a first surface compressive stress (CS1) in a first compressive stress region of 450 MPa or more, and the second stress profile comprises a second surface compressive stress (CS2) in a second compressive stress region of 450 MPa or more.

### Claim 8 (depends on 1)

The method of claim 1, wherein a portion of the first stress profile extends from the first section surface to a knee, the knee is located at a depth from the first section surface in a range from about 2 micrometers to about 30 micrometers, and all points of the first stress profile located between the first section surface and the knee comprise a tangent having a value that is 10 MPa/micrometer or greater.

### Claim 9 (depends on 8)

The method of claim 8, wherein a portion of the first stress profile extends from the knee to a first depth of compression (DOC1), wherein all points of the first stress profile located between the knee and DOC1 comprise a tangent having a value from 0 MPa/micrometer to about 2 MPa/micrometer.

### Claim 10 (depends on 1)

The method of claim 1, wherein the glass-based substrate comprises a soda-lime silicate, an alkali-aluminosilicate, an alkali-containing borosilicate, an alkali-containing aluminoborosilicate, or an alkali-containing phosphosilicate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the glass-based substrate is a lithium-containing aluminosilicate.

### Claim 12 (depends on 11)

The method of claim 11, wherein the alkali metal ions include potassium.

### Claim 13 (depends on 1)

The method of claim 1, wherein h1 is in a range from 0.3 mm to 2.5 mm, and h2 is in a range from 0.025 mm to 2.4 mm.

### Claim 14 (depends on 1)

The method of claim 1, wherein h2 is in a range from 0.05·h1 to 0.96·h1.

### Claim 15 (depends on 1)

The method of claim 1, wherein h2 is less than h1 by at least 100 microns.

### Claim 16 (depends on 1)

The method of claim 1, wherein the alkali metal ions comprise one or more potassium, sodium, or combinations thereof.

### Claim 17 (depends on 1)

The method of claim 1, The glass-based article of claim 1, wherein the alkali metal ions comprise are selected from a group consisting of: silver, copper, zinc, titanium, rubidium, cesium, and combinations thereof.

### Claim 18 (depends on 1)

The method of claim 1, wherein the alkali metal oxide is selected from a group consisting of: silver, copper, zinc, titanium, rubidium, and cesium.

### Claim 19 (depends on 1)

The method of claim 1, wherein the alkali metal oxide comprises potassium.

### Claim 20 (depends on 1)

The method of claim 1, wherein the glass-based substrate comprises:
from 64 mol % to 68 mol % SiO2;
from 12 mol % to 16 mol % Na2O;
from 8 mol % to 12 mol % Al2O3;
from 0 mol % to 3 mol % B2O3;
from 2 mol % to 5 mol % K2O;
from 4 mol % to 6 mol % MgO; and
from 0 mol % to 5 mol % CaO,
wherein:
66 mol %<(SiO2+B2O3+CaO)≤69 mol %;
(Na2O+K2O+B2O3+MgO+CaO+SrO)>10 mol %;
5 mol %<(MgO+CaO+SrO)≤8 mol %;
(Na2O+B2O3)<Al2O3<2 mol %;
2 mol %<Na2O<Al2O3<6 mol %; and
4 mol %<(Na2O+K2O)<Al2O3≤10 mol %.