# US 2023/0271879 A1 · Chemically strengthened glass and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271879 A1
- Document ID: US20230271879A1
- Status: Published application
- Kind: A1
- Application number: 18/174,179
- Filed: 2023-02-24
- Published: 2023-08-31
- Earliest claimed: 2022-02-28
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Yusuke FUJIWARA; Yoichi TAKATO; Yusuke KOBAYASHI
- Web page: https://patentgrep.com/patent/US20230271879A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/095: containing rare earths
- C03C 10/0027: {containing SiO2, Al2O3, Li2O as main constituents}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to a chemically strengthened glass, satisfying: a ratio ICS (≥400)/ICS being more than 0.13 in a stress profile, the ICS representing an integrated value of compressive stress in a region from a surface of the glass to a depth where the compressive stress becomes 0 in the stress profile, and the ICS (≥400) representing an integrated value of compressive stress in a region from a depth of 400 μm from the surface of the glass to the depth where the compressive stress becomes 0 in the stress profile.

## Claims

### Claim 1

A chemically strengthened glass, satisfying:
a ratio ICS (≥400)/ICS being more than 0.13 in a stress profile, the ICS representing an integrated value of compressive stress in a region from a surface of the glass to a depth where the compressive stress becomes 0 in the stress profile, and the ICS (≥400) representing an integrated value of compressive stress in a region from a depth of 400 μm from the surface of the glass to the depth where the compressive stress becomes 0 in the stress profile.

### Claim 2 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the ICS (≥400) is 9,200 MPa·μm or more.

### Claim 3 (depends on 1)

The chemically strengthened glass according to claim 1, having a stress layer depth DOL where the compressive stress becomes 50 MPa of 400 μm or more.

### Claim 4 (depends on 1)

The chemically strengthened glass according to claim 1, having a negative maximum slope of the stress profile at a position deeper than 50 μm from the surface of −0.50 (MPa/μm) or more.

### Claim 5 (depends on 1)

The chemically strengthened glass according to claim 1, having a value DOC/t being 0.170 or more, the DOC representing a depth of a compressive stress layer, and the t representing a sheet thickness of the glass.

### Claim 6 (depends on 1)

The chemically strengthened glass according to claim 1, having a maximum tensile stress CTmax of 40 MPa or more.

### Claim 7 (depends on 1)

The chemically strengthened glass according to claim 1, having a compressive stress CS600 at a depth of 600 μm from the surface of 15 MPa or more.

### Claim 8 (depends on 1)

The chemically strengthened glass according to claim 1, having a negative maximum slope of the stress profile at a depth of 0 to 20 μm from the surface of −10 (MPa/μm) or less.

### Claim 9 (depends on 1)

The chemically strengthened glass according to claim 1, wherein the stress profile has a local maximum, and the compressive stress value at the local maximum is 50 MPa or more.

### Claim 10 (depends on 9)

The chemically strengthened glass according to claim 9, wherein the local maximum positions within a range of 0.05 t to 0.13 t in a depth from the surface, t representing a sheet thickness of the glass.

### Claim 11 (depends on 9)

The chemically strengthened glass according to claim 9, satisfying:
a relationship of ms>md, the ms representing an absolute value of an average slope of the stress profile in a region from the surface to the local maximum; and the and representing an absolute value of an average slope of the stress profile from the local maximum to the depth where the compressive stress becomes 0.

### Claim 12 (depends on 1)

The chemically strengthened glass according to claim 1, having a ratio CS400/CS0 being 0.10 or more, the CS400 representing a compressive stress at a depth of 400 μm from the surface, and CS0 representing a surface compressive stress.

### Claim 13 (depends on 1)

The chemically strengthened glass according to claim 1, having a ratio CS600/CS0 being 0.03 or more, the CS600 representing a compressive stress at a depth of 600 μm from the surface, and CS0 representing a surface compressive stress.

### Claim 14 (depends on 1)

The chemically strengthened glass according to claim 1, having a ratio CS400/CS0 being 0.32 or more, the CS400 representing a compressive stress at the depth of 400 μm from the surface, and CS0 representing a surface compressive stress.

### Claim 15 (depends on 1)

The chemically strengthened glass according to claim 1, having a crack generation rate evaluated in accordance with a strength test method of ISO 20567-1 Test Method B of 10% or less.

### Claim 16 (depends on 1)

The chemically strengthened glass according to claim 1, having a sheet thickness of the glass of 1.4 to 7 mm.

### Claim 17 (depends on 1)

The chemically strengthened glass according to claim 1, being used for an on-vehicle sensor.

### Claim 18

A method for manufacturing a chemically strengthened glass, comprising:
performing a first ion exchange of exchanging ions by bringing a lithium-containing aluminosilicate glass having a sheet thickness of 1.4 to 7 mm into contact with a first inorganic salt composition containing sodium at a temperature of 430° C. or higher for 10 hours or longer.

### Claim 19 (depends on 18)

The method for manufacturing a chemically strengthened glass according to claim 18, wherein the chemically strengthened glass has a compressive stress CS400 at a depth of 400 μm from a surface of the glass of 60 MPa or more.

### Claim 20 (depends on 18)

The method for manufacturing a chemically strengthened glass according to claim 18, further comprising, after the first ion exchange, performing a second ion exchange of exchanging ions by bringing the lithium-containing aluminosilicate glass into contact with a second inorganic salt composition containing lithium.

### Claim 21 (depends on 20)

The method for manufacturing a chemically strengthened glass according to claim 20, wherein the second inorganic salt composition comprises lithium and potassium.

### Claim 22 (depends on 20)

The method for manufacturing a chemically strengthened glass according to claim 20, wherein a mass ratio of lithium to a total amount of sodium and lithium contained in the second inorganic salt composition is larger than a mass ratio of lithium to a total amount of sodium and lithium contained in the first inorganic salt composition.