# US 2023/0271864 A1 · Process for enriching phosphorus and recovering blue iron ore by using biofilm method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271864 A1
- Document ID: US20230271864A1
- Status: Published application
- Kind: A1
- Application number: 18/005,971
- Filed: 2021-05-24
- Published: 2023-08-31
- Earliest claimed: 2020-11-30
- Assignees: Suzhou University of Science and Technology
- Applicants: Suzhou University of Science and Technology
- Inventors: Yang PAN; Xingyu ZHANG; Yong HANG; Min NI; Yue CHEN
- Web page: https://patentgrep.com/patent/US20230271864A1

## CPC

- C02F 3/308: {Biological phosphorus removal}
- B01D 9/0036: {Crystallisation on to a bed of product crystals; Seeding}
- B01D 9/0059: {General arrangements of crystallisation plant, e.g. flow sheets}
- C01B 25/375: {of iron}
- C02F 3/006: {Regulation methods for biological treatment}
- C02F 1/5245: {using basic salts, e.g. of aluminium and iron}
- C02F 3/04: using trickle filters
- C02F 3/1263: {Sequencing batch reactors [SBR]}
- C02F 3/1268: {Membrane bioreactor systems}
- C02F 3/282: {using anaerobic sequencing batch reactors}
- C02F 2001/5218: {Crystallization}
- C02F 2209/04: Oxidation reduction potential [ORP]
- C02F 2209/22: O2
- C02F 2209/44: Time
- C02F 2305/06: Nutrients for stimulating the growth of microorganisms
- Y02W 10/10: Biological treatment of water, waste water, or sewage
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A process for enriching phosphorus and recovering vivianite by a biofilm method includes the following steps: 1) an aerobic phosphorus absorption stage; 2) an anaerobic phosphorus release stage; 3) a cyclic enrichment stage; 4) a seed crystal forming stage; and 5) a crystal forming stage. Phosphorus is enriched by the biofilm method and recovered with vivianite as a recovery product, which solves the problem of phosphorus removal from municipal sewage and improves the economic value; by preparing high dissolved oxygen at the aerobic stage, a high-concentration phosphorus recovery solution can be obtained with a relatively low carbon-phosphorus ratio and relatively high enrichment times, and the consumption of carbon sources can be reduced; since the oxidation-reduction potential is controlled to be less than −100 mv by the biofilm method at the anaerobic phosphorus release stage, the oxidation-reduction potential does not need to be adjusted again during the recovery of vivianite,

## Claims

### Claim 1

A process for enriching phosphorus and recovering vivianite by a biofilm method, specifically comprising the following steps:
1) an aerobic phosphorus absorption stage: under an aerobic condition, controlling dissolved oxygen of phosphorus-containing wastewater in a biofilm reactor to be greater than 4 mg/L, and discharging the wastewater after aerobic phosphorus absorption for a period of hydraulic retention time;
2) an anaerobic phosphorus release stage: under an anaerobic condition, feeding liquid in a phosphorus recovery device into the biofilm reactor as base liquid, adding a carbon source at a preset carbon-phosphorus ratio through a carbon source dosing device, and discharging the phosphorus-containing solution to the phosphorus recovery device after anaerobic phosphorus release for another period of hydraulic retention time;
3) a cyclic enrichment stage: performing multiple rounds of operation, each round comprising one cycle of the aerobic phosphorus absorption phase according to step 1) and one cycle of the anaerobic phosphorus release phase according to step 2) so that the base liquid reaches a phosphorous-rich solution with a preset concentration, and recovering the phosphorous-rich solution to the phosphorus recovery device;
4) a seed crystal forming stage: further discharging the phosphorus-rich solution in the phosphorus recovery device to an up-flow reactor, adding a ferrous ion solution to the up-flow reactor, and continuously operating a backflow system to fully mix the ferrous ion solution and the phosphorus-rich solution in the up-flow reactor to form ferrous phosphate seed crystals; and
5) a crystal forming stage: continuously feeding the phosphorus-rich solution and the ferrous ion solution into the up-flow reactor at a preset speed, and continuously operating the backflow system to circularly crystallize the phosphorus-rich solution and the ferrous ion solution in the up-flow reactor, so that the ferrous phosphate seed crystals form ferrous phosphate crystals with a preset particle size.

### Claim 2 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein in step 1), the period of hydraulic retention time at the aerobic phosphorus absorption stage is from 2 to 10 hours; and in step 2), the period of hydraulic retention time at the anaerobic phosphorus release stage is from 1 to 6 hours.

### Claim 3 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein in step 1), the dissolved oxygen in the biofilm reactor ranges from 4 mg/L to 8 mg/L, and after the aerobic phosphorus absorption, the phosphorus storage capacity of a phosphorus-accumulating biofilm in the biofilm reactor is greater than or equal to 100 mg-P/g-SS.

### Claim 4 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein an enrichment time of the phosphorus-rich solution in step 3) is 10 to 30 times.

### Claim 5 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein the preset carbon-phosphorus ratio in step 2) is 15 g/g to 40 g/g, and the concentration of the phosphorus-rich solution obtained in step 3) is 60 mg/L to 300 mg/L.

### Claim 6 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein step 3) further comprises storing the phosphorus-rich solution in the phosphorus recovery device to a phosphorus storage device under the anaerobic condition, and step 4) further comprises discharging the phosphorus-rich solution from the phosphorus storage device to the up-flow reactor.

### Claim 7 (depends on 6)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 6, wherein oxidation-reduction potentials in the phosphorus recovery device and the phosphorus storage device range from −450 mv to −100 mv.

### Claim 8 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein the ferrous ion solution is a ferrous sulfate solution or a ferrous chloride tetrahydrate solution.

### Claim 9 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein in step 5), the up-flow reactor further comprises an overflow weir at the upper end of the up-flow reactor, and wastewater produced in the up-flow reactor is discharged from the overflow weir.

### Claim 10 (depends on 1)

The process for enriching phosphorus and recovering vivianite by a biofilm method according to claim 1, wherein in step 5), the ferrous phosphate crystals have an average particle size greater than or equal to 100 μm.