# US 2023/0271847 A1 · Beta-type active zinc sulfide and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271847 A1
- Document ID: US20230271847A1
- Status: Published application
- Kind: A1
- Application number: 18/303,477
- Filed: 2023-04-19
- Published: 2023-08-31
- Earliest claimed: 2022-02-25
- Assignees: Guangdong Xinda Advanced Materials Technology Co., Ltd
- Applicants: Guangdong Xinda Advanced Materials Technology Co., Ltd
- Inventors: LIN, Ze-Peng; LIN, Hua-Xiong; LIN, Jun
- Web page: https://patentgrep.com/patent/US20230271847A1

## CPC

- C01G 9/08: Sulfides
- C01G 3/12: Sulfides
- C01P 2004/03: obtained by SEM
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/32: Spheres
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed are beta-type active zinc sulfide and a preparation method therefor. The method includes: adding an oil phase containing styrene monomers into a water phase containing a pore-forming agent, a surfactant, a Zn salt, a complexing agent, a sulfur source and a water-soluble initiator, conducting mixing and emulsification, introducing metal elements, dissolving polystyrene of microspheres prepared through reaction in tetrahydrofuran, and then conducting calcination, pickling and activation to obtain the beta-type active zinc sulfide. The zinc sulfide microspheres prepared by the present invention are beta-type, and have excellent photoelectric properties and broad application prospects.

## Claims

### Claim 1

A preparation method for beta-type active zinc sulfide, comprising the following steps:
S1, dissolving styrene monomers in an organic solvent, so as to obtain an oil phase; S2, dissolving a pore-forming agent, a surfactant, a Zn salt, a complexing agent, a sulfur source and a water-soluble initiator in water, so as to obtain a water phase, wherein the pore-forming agent is a composite pore-forming agent, the composite pore-forming agent comprises a macropore-forming agent and a mesopore-forming agent, the macropore-forming agent is selected from at least one of polyoxyethylene sorbitan fatty acid ester, polyethylene glycol octyl phenyl ether, and polyoxyethylene sorbitan fatty acid ester, and the mesopore-forming agent is cetyltrimethyl ammonium bromide (CTAB); S3, adding the oil phase into the water phase, conducting mixing and emulsification, adjusting a pH value to 8-9, introducing metal elements, heating to 50° C.-70° C., stirring and conducting reaction for 2 h-5 h, and conducting centrifugation and washing, so as to obtain porous ZnS/PS nanospheres, wherein the metal elements are selected from at least one of nickel, lanthanum, cerium, cobalt, titanium, palladium, iridium, platinum, molybdenum, and strontium, an addition amount being 0.01 wt%-0.1 wt% of a total mass of a system; S4, adding the porous ZnS/PS nanospheres prepared in S3 into a tetrahydrofuran solvent for reaction, and conducting centrifugation, washing and calcination, so as to obtain porous beta-type ZnS nanospheres; and S5, washing the porous beta-type ZnS nanospheres by using an acid pickling agent, rinsing the nanospheres by using water to become neutral after washing, and conducting activation and modification by using an activating agent, so as to obtain the beta-type active zinc sulfide, wherein the acid pickling agent is selected from at least one of sulfuric acid, nitric acid, phosphoric acid, and acetic acid, and the activating agent is selected from at least one of sodium dodecyl benzene sulfonate, sodium dodecyl sulfate, sodium dodecyl sulfonate, a silane coupling agent, a titanate coupling agent, triethanolamine, epoxidized soybean oil, isooctanol, isooctanoic acid, castor oil, glyceryl monostearate, and Span-series and Tween-series nonionic surfactants.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in S1, the organic solvent is at least one of benzene, methylbenzene, dimethylbenzene, ethylbenzene, ethyl acetate, dichloromethane, methyl acetate, chloroform and carbon tetrachloride; and a content of the styrene monomers in the oil phase is 15wt%-20wt%.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein in S2, the pore-forming agent is a mixture of the polyoxyethylene sorbitan fatty acid ester and the cetyltrimethyl ammonium bromide in a mass ratio of 5: (2-3).

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein in S2, the surfactant is selected from at least one of the sodium dodecyl benzene sulfonate, the sodium dodecyl sulfonate, the sodium dodecyl sulfate, sodium hexadecyl benzene sulfonate, sodium hexadecyl sulfonate, sodium hexadecyl sulfate, sodium octadecyl benzene sulfonate, sodium octadecyl sulfonate, and Tween-80; the Zn salt is selected from at least one of zinc nitrate, zinc sulfate, and zinc chloride; the complexing agent is selected from at least one of citric acid, sodium citrate, polyethylene glycol, ammonia water, tartaric acid, and hydrazine; the sulfur source is selected from at least one of sodium sulfide, potassium sulfide, aluminum sulfide, manganese sulfide, ammonium sulfide, thiourea, and L-cysteine; and the water-soluble initiator is selected from at least one of sodium persulfate, potassium persulfate, and ammonium persulfate.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein in S2, a mass ratio of the pore-forming agent to the surfactant to the Zn salt to the complexing agent to the sulfur source to the water-soluble initiator is (2-5): (1-3): (30-50): (10-80): (60-100): (0.5-1).

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein in S3, an emulsification condition is stirring at 12,000 r/min-15,000 r/min for 3 min-5 min.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein in S4, a solid-liquid ratio of the ZnS/PS nanospheres to the tetrahydrofuran solvent is 1:(5-10) g/ml, and a calcination condition is calcination at 500° C.-1000° C. for 1 h-6 h.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein in S5, the silane coupling agent is selected from at least one of KH550, KH560, KH570, KH580, KH590, KH602, and KH792; the titanate coupling agent is selected from at least one of isopropyl tri(isostearoyl) titanate, isopropyl tri(dioctylphosphonyl) titanate, di(dioctylphosphonyl) oxyacetate titanium, di(dioctylphosphonyl) ethylene titanate, isopropyl di(methacryloyl) isostearoyl titanate, isopropyl tri(dioctylphosphonyl) titanate, isopropyl tri(dodecylbenzenesulfonyl) titanate, and isopropyl tri(n-ethylamino-ethylamino) titanate; and a mass ratio of the porous beta-type ZnS nanospheres to the activating agent is 100: (2-5).

### Claim 9 (depends on 1)

Beta-type active zinc sulfide prepared through the preparation method according to claim 1.