# US 2023/0271845 A1 · Method for producing calcium carbonate and calcium carbonate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0271845 A1
- Document ID: US20230271845A1
- Status: Published application
- Kind: A1
- Application number: 18/014,356
- Filed: 2021-12-24
- Published: 2023-08-31
- Earliest claimed: 2020-12-28
- Assignees: Shiraishi Kogyo Kaisha, Ltd.
- Applicants: Shiraishi Kogyo Kaisha, Ltd.
- Inventors: Hiromitsu Sakaguchi; Sayaka Oguni; Kenichiro Eguchi; Toru Oda; Yasunori Nanri
- Web page: https://patentgrep.com/patent/US20230271845A1

## CPC

- C01F 11/181: {Preparation of calcium carbonate by carbonation of aqueous solutions and characterised by control of the carbonation conditions}
- B01D 53/14: by absorption
- B01D 53/1475: {Removing carbon dioxide}
- B01D 53/62: Carbon oxides
- B01D 53/72: Organic compounds not provided for in groups B01D53/48 - B01D53/70, e.g. hydrocarbons
- C01F 11/18: Carbonates
- C01F 11/182: {Preparation of calcium carbonate by carbonation of aqueous solutions and characterised by an additive other than CaCO3-seeds}
- C01P 2004/03: obtained by SEM
- C01P 2004/10: extending in one dimension, e.g. needle-like
- C01P 2004/30: extending in three dimensions
- C01P 2006/12: Surface area
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

To produce a calcium carbonate in a controlled form while carbon dioxide gas is efficiently used. A method for producing a calcium carbonate comprises a carbon dioxide gas absorption step of allowing an aqueous sodium hydroxide solution at a concentration of 5 to 21% to absorb carbon dioxide gas to give an aqueous sodium carbonate solution at a concentration of 4 to 24%; a hydration step of reacting calcium oxide with an aqueous sodium hydroxide solution at a concentration of 0 to less than 6% to give a lime milk that is a suspension of calcium hydroxide having a BET specific surface area of 5 to 40 m2/g; and a carbonation step of adding the aqueous sodium carbonate solution to the lime milk and performing reaction.

## Claims

### Claim 1

A method for producing a calcium carbonate, the method comprising:
a carbon dioxide gas absorption step of allowing an aqueous sodium hydroxide solution at a concentration of 5 to 21% to absorb carbon dioxide gas to give an aqueous sodium carbonate solution at a concentration of 4 to 24%;
a hydration step of reacting calcium oxide with an aqueous sodium hydroxide solution at a concentration of 0 to less than 6% to give a lime milk that is a suspension of calcium hydroxide having a BET specific surface area of 5 to 40 m2/g; and
a carbonation step of adding the aqueous sodium carbonate solution to the lime milk and performing reaction.

### Claim 2 (depends on 1)

The production method according to claim 1, wherein in the carbonation step, the lime milk is adjusted at a concentration of 1 to 24%, the aqueous sodium carbonate solution is added to the lime milk having an adjusted solid concentration, and the reaction is performed at a temperature of 9 to 80° C.

### Claim 3 (depends on 2)

The production method according to claim 2, further comprising, after the carbonation step, a solid-liquid separation step of separating a filtrate containing sodium hydroxide from calcium carbonate.

### Claim 4 (depends on 3)

The production method according to claim 3, wherein the filtrate containing sodium hydroxide is adjusted at a sodium hydroxide concentration of 5 to 21% and is reused in the carbon dioxide gas absorption step.

### Claim 5 (depends on 4)

A calcium carbonate produced by the production method according to claim 4.

### Claim 6

A method for producing a calcium carbonate, the method comprising:
a carbon dioxide gas absorption step of allowing an aqueous sodium hydroxide solution at a concentration of 5 to 21% to absorb carbon dioxide gas to give an aqueous sodium carbonate solution at a concentration of 4 to 24%;
a hydration step of reacting calcium oxide with an aqueous sodium hydroxide solution at a concentration of 0 to less than 6% to give a lime milk that is a suspension of calcium hydroxide having a BET specific surface area of 5 to 40 m2/g; and
a carbonation step of adding the aqueous sodium carbonate solution prepared in the carbon dioxide gas absorption step to the lime milk and performing reaction, wherein
in the carbonation step, the lime milk has an initial concentration of 1 to 6%, the aqueous sodium carbonate solution has a concentration of 4 to 22%, and the reaction is performed at 9 to 25° C. to yield a calcite-type calcium carbonate having a fine particle shape and having a BET specific surface area of 30 to 90 m2/g.

### Claim 7 (depends on 6)

The production method according to claim 6, wherein carbon dioxide gas unused in the carbon dioxide gas absorption step is reused in the carbon dioxide gas absorption step.

### Claim 8 (depends on 7)

The production method according to claim 7, further comprising:
after the carbonation step, a solid-liquid separation step of separating a filtrate containing sodium hydroxide from calcium carbonate; and
a washing step of washing the calcium carbonate prepared in the solid-liquid separation step with a washing liquid.

### Claim 9 (depends on 8)

The production method according to claim 8, wherein the filtrate prepared in the solid-liquid separation step and a used washing liquid after the washing step are mixed with an aqueous sodium hydroxide solution at a high concentration, or the filtrate and the used washing liquid are concentrated by heating, to give an aqueous solution containing sodium hydroxide at a concentration of 5 to 21%, and the aqueous solution is used in the carbon dioxide gas absorption step.

### Claim 10 (depends on 9)

The production method according to claim 9, wherein the filtrate prepared in the solid-liquid separation step and the used washing liquid after the washing step are adjusted to give an aqueous solution containing sodium hydroxide at a concentration of less than 6%, and the aqueous solution is used in the hydration step.

### Claim 11 (depends on 10)

A calcium carbonate produced by the production method according to claim 10.

### Claim 12

A method for producing a calcium carbonate, the method comprising:
a carbon dioxide gas absorption step of allowing an aqueous sodium hydroxide solution at a concentration of 13 to 21% to absorb carbon dioxide gas to give an aqueous sodium carbonate solution at a concentration of 15 to 24%;
a hydration step of reacting calcium oxide with an aqueous sodium hydroxide solution at a concentration of 0 to less than 6% to give a lime milk that is a suspension of calcium hydroxide having a BET specific surface area of 5 to 40 m2/g; and
a carbonation step of adding the aqueous sodium carbonate solution prepared in the carbon dioxide gas absorption step to the lime milk and performing reaction, wherein
in the carbonation step, the lime milk has an initial concentration of 11 to 19%, the aqueous sodium carbonate solution has a concentration of 15 to 24%, and the reaction is performed at 20 to 40° C. to yield a calcite-type calcium carbonate having a spindle shape and having a BET specific surface area of 4 to 20 m2/g.

### Claim 13 (depends on 12)

The production method according to claim 12, wherein carbon dioxide gas unused in the carbon dioxide gas absorption step is reused in the carbon dioxide gas absorption step.

### Claim 14 (depends on 13)

The production method according to claim 13, further comprising:
after the carbonation step, a solid-liquid separation step of separating a filtrate containing sodium hydroxide from calcium carbonate; and
a washing step of washing the calcium carbonate prepared in the solid-liquid separation step with a washing liquid.

### Claim 15 (depends on 14)

The production method according to claim 14, wherein the filtrate prepared in the solid-liquid separation step and a used washing liquid after the washing step are mixed with an aqueous sodium hydroxide solution at a high concentration, or the filtrate and the used washing liquid are concentrated by heating, to give an aqueous solution containing sodium hydroxide at a concentration of 13 to 21%, and the aqueous solution is used in the carbon dioxide gas absorption step.

### Claim 16 (depends on 15)

The production method according to claim 15, wherein the filtrate prepared in the solid-liquid separation step and the used washing liquid after the washing step are adjusted to give an aqueous solution containing sodium hydroxide at a concentration of less than 6%, and the aqueous solution is used in the hydration step.

### Claim 17 (depends on 16)

A calcium carbonate produced by the production method according to claim 16.

### Claim 18

A method for producing a calcium carbonate, the method comprising:
a carbon dioxide gas absorption step of allowing an aqueous sodium hydroxide solution at a concentration of 13 to 21% to absorb carbon dioxide gas to give an aqueous sodium carbonate solution at a concentration of 15 to 24%;
a hydration step of reacting calcium oxide with an aqueous sodium hydroxide solution at a concentration of 0 to less than 6% to give a lime milk that is a suspension of calcium hydroxide having a BET specific surface area of 5 to 40 m2/g; and
a carbonation step of adding the aqueous sodium carbonate solution prepared in the carbon dioxide gas absorption step to the lime milk and performing reaction, wherein
in the carbonation step, the lime milk has an initial concentration of 11 to 24%, the aqueous sodium carbonate solution has a concentration of 15 to 24%, and the reaction is performed at 40 to 80° C. to yield an aragonite-type calcium carbonate having a needle-like shape and having a BET specific surface area of 3 to 10 m2/g.

### Claim 19 (depends on 18)

The production method according to claim 18, wherein carbon dioxide gas unused in the carbon dioxide gas absorption step is reused in the carbon dioxide gas absorption step.

### Claim 20 (depends on 19)

The production method according to claim 19, further comprising:
after the carbonation step, a solid-liquid separation step of separating a filtrate containing sodium hydroxide from calcium carbonate; and
a washing step of washing the calcium carbonate prepared in the solid-liquid separation step with a washing liquid.

### Claim 21 (depends on 20)

The production method according to claim 20, wherein the filtrate prepared in the solid-liquid separation step and a used washing liquid after the washing step are mixed with an aqueous sodium hydroxide solution at a high concentration, or the filtrate and the used washing liquid are concentrated by heating, to give an aqueous solution containing sodium hydroxide at a concentration of 13 to 21%, and the aqueous solution is used in the carbon dioxide gas absorption step.

### Claim 22 (depends on 21)

The production method according to claim 21, wherein the filtrate prepared in the solid-liquid separation step and the used washing liquid after the washing step are adjusted to give an aqueous solution containing sodium hydroxide at a concentration of less than 6%, and the aqueous solution is used in the hydration step.

### Claim 23 (depends on 22)