# US 2023/0265574 A1 · Method for recovering metals from tungsten-containing metallic material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265574 A1
- Document ID: US20230265574A1
- Status: Published application
- Kind: A1
- Application number: 17/859,278
- Filed: 2022-07-07
- Published: 2023-08-24
- Earliest claimed: 2022-02-18
- Assignees: National Tsing Hua University
- Applicants: National Tsing Hua University
- Inventors: Chih-Huang LAI; Shao-Chi LO; Tzu-Min CHENG
- Web page: https://patentgrep.com/patent/US20230265574A1

## CPC

- C25C 1/06: or iron group metals, refractory metals or manganese
- C22B 7/006: {Wet processes}
- C22B 34/36: Obtaining tungsten
- C25C 1/08: of nickel or cobalt
- Y02P 10/20: Recycling
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for recovering metals from tungsten-containing metallic materials includes the steps of: providing a cathode and the tungsten-containing metallic material as an anode in an electrolyte solution which has a neutral, acidic or basic pH value; and subjecting the tungsten-containing metallic material to an electrolysis process under a power density that is greater than 3 W/cm2 on the anode so that a passivation layer formed on the anode during the electrolysis process is broken down to permit the tungsten-containing metallic material to be continuously dissolved and oxidized, and a tungsten-containing compound is formed in the electrolyte solution.

## Claims

### Claim 1

A method for recovering metals from tungsten-containing metallic material, comprising the steps of:
providing a cathode and the tungsten-containing metallic material serving as an anode in an electrolyte solution which has a pH value of one of neutral, not greater than 2, and not less than 10; and
subjecting the tungsten-containing metallic material to an electrolysis process under a power density that is greater than 3 W/cm2 on the anode so that a passivation layer formed on the anode during the electrolysis process is broken down to permit the tungsten-containing metallic material to be continuously dissolved and oxidized, and a tungsten-containing compound is formed in the electrolyte solution.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the anode is dissolved in a dissolution rate of not less than 13 mg/min during the electrolysis process.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the pH value of the electrolyte solution in the providing step is one of neutral and not greater than 2, and the tungsten-containing compound formed during the electrolysis process includes tungsten oxide that precipitates from the electrolyte solution.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the pH value of the electrolyte solution in the providing step is not less than 10, and the tungsten-containing compound formed during the electrolysis process includes tungstate that dissolves in the electrolyte solution.

### Claim 5 (depends on 4)

The method as claimed in claim 4, further comprising, after the electrolysis process, the step of lowering the pH of the electrolyte solution to convert tungstate to tungsten oxide that precipitates from the electrolyte solution.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the step of lowering the pH of the electrolyte solution is conducted by adding an acidic electrolyte substance.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the electrolysis process is conducted under the power density ranging from 3 W/cm2 to 35 W/cm2 on the anode.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the electrolyte solution having the pH value of not greater than 2 is prepared using an inorganic acid selected from the group consisting of hydrochloric acid, sulfuric acid, nitric acid, perchloric acid, and combinations thereof.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the electrolyte solution having the pH value of 7 is prepared using a neutral electrolyte selected from the group consisting of sodium chloride, potassium chloride, potassium sulfate, and combinations thereof.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the electrolyte solution having the pH value of not lower than 10 is prepared using an inorganic base selected from the group consisting of sodium carbonate, potassium carbonate, potassium hydroxide, and combinations thereof.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein the tungsten-containing metallic material is selected from the group consisting of cemented tungsten carbide, tungsten lanthanum alloy, a doped tungsten, and combinations thereof.

### Claim 12 (depends on 3)

The method as claimed in claim 3, wherein the tungsten-containing metallic material is cemented tungsten carbide including tungsten and cobalt, the anode is dissolved during the electrolysis process in a dissolution rate of not less than 15 mg/min to produce tungsten oxide in a hydrated form having a purity of not lower than 90%, and cobalt is electrodeposited onto the cathode.

### Claim 13 (depends on 5)

The method as claimed in claim 5, wherein the tungsten-containing metallic material is cemented tungsten carbide including tungsten and cobalt, and during the electrolysis process, a cobalt compound is formed and precipitates from the electrolyte solution, the cobalt compound including one of cobalt oxide, cobalt hydroxide, and a combination thereof.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein the method further comprises, before the step of lowering the pH of the electrolyte solution, the step of collecting the cobalt compound from the electrolyte solution.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the collecting step is performed through one of a filtration process, a centrifugation process, an evaporation process, a size-exclusion chromatography process, and combinations thereof.

### Claim 16 (depends on 1)

The method as claimed in claim 1, wherein the electrolysis process is conducted at a temperature ranging from 60° C. to 80° C.