# US 2023/0265541 A1 · method for recovering rare-earth in cerium-based rare-earth polishing powder waste by two-step acid leaching gradient separation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265541 A1
- Document ID: US20230265541A1
- Status: Published application
- Kind: A1
- Application number: 18/132,979
- Filed: 2023-04-11
- Published: 2023-08-24
- Earliest claimed: 2020-12-02
- Assignees: Beijing University of Technology
- Applicants: Beijing University of Technology
- Inventors: Qijun Zhang; Yufeng Wu; Minwei Song
- Web page: https://patentgrep.com/patent/US20230265541A1

## CPC

- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C22B 59/00: Obtaining rare earth metals
- C22B 1/24: Binding; Briquetting {; Granulating}
- C22B 3/065: {Nitric acids or salts thereof}
- C22B 3/10: Hydrochloric acid {, other halogenated acids or salts thereof}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/001: {Dry processes}
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 7/007: {by acid leaching}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method of recovering rare-earth in cerium-based rare-earth polishing powder waste by two-step acid leaching gradient separation, characterized by: firstly, using a one-step acid leaching treatment on cerium-based rare-earth polishing powder waste to obtain a rare-earth leaching liquor which is rich in La; secondly, the leaching residue is then processed through alkali activation and transformation process, water washing and impurity removal process, secondary acid leaching process, filtration, and recovery to obtain high purity CeO2 products; thirdly, the acid leaching liquor obtained through first acid leaching and second acid leaching process is finally precipitated by oxalic acid, filtered and calcined at high temperature to obtain rare-earth oxide mixed products, which achieves the gradient separation and recovery of rare-earths from cerium-based rare-earth polishing powder waste. The total recovery efficiency of rare-earth of this invention reaches 97% or higher, with high efficiency of rare-earth recovery, wide process applicability, and low environmental pollution.

## Claims

### Claim 1

A method of separating and recycling rare-earth in cerium-based rare-earth polishing powder waste by two-step acid leaching, comprising the following specific steps:
(1) Ball milling pretreatment: the cerium-based rare-earth polishing powder waste is ball-milled to a particle size below 160 mesh to obtain ball-milled waste;
(2) First acid leaching: put the ball milled waste obtained in step (1) into a container and add an acid solution for a first acid leaching reaction, keep heating and stirring during the first acid leaching reaction, separate solid and liquid after the first acid leaching reaction to obtain leaching residue and leaching liquor 1, a molar concentration of the acid solution is 5-8 mol/L, a solid-liquid ratio of the ball milled waste to the acid solution is 1:4-1:8 kg/L, leaching temperature is 70-80° C., and leaching time is 1-2 hours;
(3) Alkali roasting: mix the leaching residue obtained in step (2) with alkali to obtain a mixture and roast the mixture to obtain a roasted mixture, a mass ratio of the leaching residue to alkali is 1:1-1:3, roasting temperature is 450-650′C, and roasting time is 0.5-1.5 hours;
(4) Water leaching: put the roasted mixture obtained in step (3) in water to conduct water leaching, a solid-liquid ratio of the roasted mixture to water is 1:4-1:9 kg/L, water leaching temperature is 80-90′C, water leaching time is 2-3 hours, and stirring speed is 300-500 rpm, after the water leaching is completed, separate solid from liquid, and water leaching residue is obtained by filtration;
(5) Second acid leaching: mix the water leaching residue obtained in step (4) with an acid solution to carry out secondary acid leaching reaction, separate solid from liquid after the second acid leaching reaction is completed, and conduct filtration to obtain CeO2 product and leaching liquor 2, a molar concentration of the acid solution is 5-8 mol/L, a solid-liquid ratio of the water leaching residue to the acid solution is 1:2.5-1:6 kg/L, leaching temperature is 70-80° C., and leaching time is 2-3 hours;
(6) Precipitation of rare-earths with oxalic acid: mix the leaching liquor 1 obtained in step (2) and the leaching liquor 2 obtained in step (5) to obtain a mixed solution, and add an oxalic acid solution with a mass concentration of 100 g/L to the mixed solution to precipitate rare-earths, a volume ratio of the mixed solution to the oxalic acid solution is 5:1-3:1, stir and add ammonia with a mass percentage concentration of 25%, until the pH value of the solution reaches 1.8-2.0, and precipitate at 80-90° C. for 2-3 hours, conduct filtration to obtain rare-earth oxalate;
(7) Calcination: the rare-earth oxalate obtained in step (6) is calcined in a muffle furnace at 950° C. for 0.5-1 hour to obtain rare-earth oxide product; wherein:
in step (2), the acid solution is hydrochloric acid solution or nitric acid solution;
in step (2), the stirring speed is 300-500 rpm;
in step (3), the alkali in the alkali roasting process is Na2O2 or K2O2;
in step (5), the acid solution is hydrochloric acid solution or nitric acid solution.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in step (5), the stirring speed is 300-500 rpm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in step (5), when the solid is separated from the liquid after the second acid leaching reaction, the CeO2 product obtained is washed 4-8 times with a hydrochloric acid solution to remove impurities, a mass concentration of the hydrochloric acid solution is 2-5%.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the leaching liquor 1 obtained in step (2) is evaporated and concentrated until the molar concentration of HCl or HNO reaches 5-8 mol/L, a concentrated leaching liquor 1 is then incorporated into the secondary acid leaching reaction of step (5) to partially or completely replace the hydrochloric acid solution or nitric acid solution.