# US 2023/0265273 A1 · Polyolefin composition for roofing applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265273 A1
- Document ID: US20230265273A1
- Status: Published application
- Kind: A1
- Application number: 18/015,937
- Filed: 2021-07-01
- Published: 2023-08-24
- Earliest claimed: 2020-07-24
- Assignees: Basell Poliolefine Italia S.r.l.
- Applicants: Basell Poliolefine Italia S.r.l.
- Inventors: Michele Grazzi; Claudio Cavalieri
- Web page: https://patentgrep.com/patent/US20230265273A1

## CPC

- B32B 5/022: {Non-woven fabric}
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- B32B 5/024: {Woven fabric}
- B32B 27/08: of synthetic resin
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/327: {comprising polyolefins obtained by a metallocene or single-site catalyst}
- B32B 27/36: comprising polyesters
- C08F 2/001: {Multistage polymerisation processes characterised by a change in reactor conditions without deactivating the intermediate polymer (C08F295/00, C08F297/00 take precedence)}
- C08F 2/34: Polymerisation in gaseous state
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08J 5/18: Manufacture of films or sheets
- E04D 5/06: by making use of plastics
- E04D 5/10: by making use of compounded or laminated materials, e.g. metal foils or plastic films coated with bitumen
- B32B 2250/03: 3 layers
- B32B 2250/24: All layers being polymeric
- B32B 2262/0253: Polyolefin fibres
- B32B 2262/0276: Polyester fibres
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/536: Hardness
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/546: Flexural strength; Flexion stiffness
- B32B 2307/558: Impact strength, toughness
- B32B 2307/581: Resistant to cut
- B32B 2419/06: Roofs, roof membranes
- C08J 2323/14: Copolymers of propene (C08J2323/16 takes precedence)
- C08J 2423/14: Copolymers of propene (C08J2423/16 takes precedence)
- C08L 2203/16: used for films
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2207/02: Heterophasic composition
- C08L 2314/02: Ziegler natta catalyst
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- E04D: ROOF COVERINGS; SKY-LIGHTS; GUTTERS; ROOF-WORKING TOOLS (coverings of outer walls by plaster or other porous material E04F13/00)

## Abstract

A polyolefin composition made from or containing: (A) 18-35% by weight of a copolymer of propylene with an alpha-olefin, wherein the copolymer contains 2.0-4.0% by weight of the alpha-olefin and has a melt flow rate (MFRA) ranging from 30 to 60 g/10 min; and (B) 65-82% by weight of a copolymer of propylene with an alpha-olefin, and optionally a diene, wherein the copolymer is made from or containing 20-35% by weight of the alpha-olefin, wherein the polyolefin composition is made from or containing a fraction that is soluble in xylene at 25° C. (XS(tot)) in an amount higher than 70% by weight; the amounts of (A), (B), and the fraction soluble in xylene at 25° C. (XS(tot)) are based on the total weight of the polyolefin composition; and the melt flow rate (MFR) of the polyolefin composition ranges from 0.2 to 2.0 g/10 min.

## Claims

### Claim 1

A polyolefin composition comprising:
(A) 18-35% by weight of a copolymer of propylene with an alpha-olefin of formula CH2═CHR, where R is H or a linear or branched C2-C3 alkyl, wherein
i) the copolymer contains 2.0-4.0% by weight of the alpha-olefin, the amount of the alpha-olefin is based on the total weight of (A); and
ii) the propylene copolymer has a melt flow rate (MFRA), measured according to ISO 1133, 230° C., 2.16 kg, ranging from 30 to 60 g/10 min; and
(B) 65-82% by weight of a copolymer of propylene with an alpha-olefin of formula CH2═CHR, and optionally a diene, where R is H or a linear or branched C2-C8 alkyl and wherein the copolymer comprises 20-35% by weight of the alpha-olefin, the amount of alpha olefin is based on the total weight of (B),
wherein
iii) the polyolefin composition comprises a fraction that is soluble in xylene at 25° C. (XS(tot)) in an amount higher than 70% by weight;
iv) the amounts of (A), (B), and the fraction soluble in xylene at 25° C. (XS(tot)) are based on the total weight of the polyolefin composition, the total weight being 100; and
v) the melt flow rate (MFR), measured according to ISO 1133, 230° C., 2.16 kg, of the polyolefin composition ranges from 0.2 to 2.0 g/10 min.

### Claim 2 (depends on 1)

The polyolefin composition of claim 1, wherein component (A) is a copolymer of propylene with ethylene.

### Claim 3 (depends on 1)

The polyolefin composition of claim 1, wherein the propylene copolymer (A) has a melt flow rate (MFRA) measured according to ISO 1133, 230° C., 2.16 kg ranging from 35 to 50 g/10 min.

### Claim 4 (depends on 1)

The polyolefin composition according to claim 1, wherein the propylene copolymer (A) comprises an amount of fraction soluble in xylene at 25° C. (XSA) lower than 9.0% by weight, wherein the amount of XSA being based on the weight of copolymer (A).

### Claim 5 (depends on 1)

The polyolefin composition according to claim 1, wherein component (B) comprises:
(B1) 30-60% by weight of a first copolymer of propylene with an alpha-olefin of formula CH2═CHR, and optionally a diene, where R is H or a linear or branched C2-C8 alkyl, and wherein the first propylene copolymer comprises 20-40% by weight of the alpha-olefin and a fraction soluble in xylene at 25° C. (XSB1) higher than 80% by weight, wherein the amounts of alpha-olefin and of XSB1 are based on the weight of component (B1); and
(B2) 40-70% by weight of a second copolymer of propylene with an alpha-olefin of formula CH2═CHR, and optionally a diene, where R is H or a linear or branched C2-C8 alkyl, and wherein the second propylene copolymer comprises 25-45% by weight of the alpha-olefin and a fraction soluble in xylene at 25° C. (XSB2) higher than 80% by weight, wherein the amounts of alpha-olefin and of XSB2 are based on the weight of component (B2),
wherein the amounts of (B1) and (B2) are based on the total weight of the component (B), the weight being 100.

### Claim 6 (depends on 1)

The polyolefin composition according to claim 1, wherein the alpha-olefin in components (B), (B1), and (B2) is independently selected from the group consisting of ethylene, butene-1, hexene-1,4-methy-pentene-1, octene-1, and combinations thereof.

### Claim 7 (depends on 1)

The polyolefin composition according to claim 1, comprising an amount of fraction soluble in xylene (XS(tot)) at 25° C. ranging from 70 to 90% by weight, wherein the amount of XS(tot) is based on the total weight of the polyolefin composition.

### Claim 8 (depends on 1)

The polyolefin composition according to claim 1, having the melt flow rate measured according to ISO 1133, 230° C., 2.16 kg ranging from 0.3 to 1.5 g/10 min.

### Claim 9 (depends on 1)

The polyolefin composition according to claim 1, wherein the fraction soluble in xylene at 25° C. of the polyolefin composition has an intrinsic viscosity (XS(IV)) ranging from 2.5 to 4.5 dl/g.

### Claim 10 (depends on 1)

The polyolefin composition according to claim 1, comprising:
(A) 18-35% by weight of a copolymer of propylene with ethylene
i) comprising 2.0-4.0% by weight of ethylene, wherein the amount of ethylene being based on the weight of (A) and
ii) having a melt flow rate (MFRA) measured according to ISO 1133, 230° C., 2.16 kg ranging from 30 to 60 g/10 min.; and
(B) 65-82% by weight of a copolymer of propylene with ethylene comprising 20-35% by weight of ethylene, wherein the amount of ethylene being based on the weight of (B),
wherein
iii) the polyolefin composition comprises an amount of fraction soluble in xylene at 25° C. (XS(tot)) higher than 70% by weight;
iv) the amounts of (A), (B), and the fraction soluble in xylene at 25° C. (XS(tot)) are based on the total weight of the polyolefin composition, the total weight being 100;
v) the melt flow rate (MFR) measured according to ISO 1133, 230° C., 2.16 kg of the polyolefin composition ranges from 0.2 to 2.0 g/10 min; and
vi) the fraction soluble in xylene at 25° C. of the polyolefin composition (XS(tot)) has an intrinsic viscosity (XS(IV)) ranging from 2.5 to 4.5 dl/g.

### Claim 11 (depends on 1)

The polyolefin composition according to claim 1, having one or more of the following properties:
Flexural Modulus ranging from 40 to 90 MPa, wherein the Flexural Modulus is measured according to ISO 178:2019 on injection-molded specimens;
Strength at break greater than or equal to 10.0 MPa, measured according to the method ISO 527 on injection-molded specimens;
Charpy resistance at −40° C. equal to or higher than 6.0 KJ/m2, measured according to ISO 179/1eA 2010 on injection-molded specimens;
puncture resistance greater than or equal to 170 N, measured on a 1 mm-thick extruded sheet according to method ASTM D 4833 (punch diameter: 8 mm, crosshead speed: 300 mm/min);
puncture deformation greater than or equal to 40 mm, measured on a 1 mm-thick extruded sheet according to method ASTM D 4833 (punch diameter: 8 mm, crosshead speed: 300 mm/min);
Shore D value equal to or lower than 30, measured on 1 mm-thick extruded sheets according to method ISO 868 (15 sec).

### Claim 12 (depends on 1)

A sheet or membrane comprising the polyolefin composition according to claim 1.

### Claim 13 (depends on 1)

A multilayer sheet or membrane comprising layers X, Y, and Z and having layers' structure X/Z/Y, wherein layer X and layer Y comprise a polyolefin composition according to claim 1, and layer Z is a reinforcing layer comprising a plastic material selected from the group consisting of propylene homopolymers, propylene copolymers, polyethylene, polyethylene terephthalate and combinations thereof.

### Claim 14 (depends on 12)

The sheet or membrane according to claim 12 in the form of a single-ply roofing sheet or membrane.

### Claim 15 (depends on 12)

The sheet or membrane according to claim 12 in the form of a geomembrane.