# US 2023/0265272 A1 · High flow heterophasic polypropylene as appearance improver in polyolefin compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265272 A1
- Document ID: US20230265272A1
- Status: Published application
- Kind: A1
- Application number: 18/015,933
- Filed: 2021-07-01
- Published: 2023-08-24
- Earliest claimed: 2020-07-21
- Assignees: Basell Poliolefine Italia S.r.l.
- Applicants: Basell Poliolefine Italia S.r.l.
- Inventors: Claudio Cavalieri; Mikhail Dureev; Michele Grazzi
- Web page: https://patentgrep.com/patent/US20230265272A1

## CPC

- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08F 210/06: Propene
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2207/02: Heterophasic composition
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Heterophasic copolymers of propylene having a MFR2 (230° C./2.16 Kg) of from 3.0 to 12.0 g/10 min made from or containing: (a) from 55 to 75 wt. % of a component (A) being a copolymer of propylene with ethylene or a C4-C10 alpha-olefin, made from or containing from 0.5 to 2.0 wt. % of ethylene and/or C4-C10 alpha-olefin units and having a MFR2 (230° C./2.16 K g) ranging from 60 to 140 g/10 min; and (b) from 25 to 45 wt. % of a component (B) being a propylene-ethylene copolymer made from or containing from 25 to 45 wt. % of ethylene units and having a value of the intrinsic viscosity of the fraction soluble in xylene at room temperature (XS-IV) ranging from 5 to 9 dl/g.

## Claims

### Claim 1

A heterophasic copolymer comprising:
(a) from 55 to 75 wt. %, based on the total weight of the heterophasic copolymer, of a component (A), wherein component (A) is a copolymer of: (1) propylene and (2) ethylene or an alpha-olefin having 4-10 carbon atoms, and wherein component (A) comprises from 0.5 to 2.0 wt. %, based on the total weight of component (A), of units of ethylene and/or of C4-C10 alpha-olefin and has a MFR2 (230° C./2.16 Kg) ranging from 60 to 140 g/10 min.; and
(b) from 25 to 45 wt. %, based on the total weight of the heterophasic copolymer, of a component (B), wherein component (B) is a propylene-ethylene copolymer, and wherein component (B) comprises from 25 to 45 wt. %, based on the total weight of component (B), of ethylene units and contains a fraction that is soluble in xylene at room temperature, and wherein the fraction that is soluble in xylene at room temperature has an intrinsic viscosity (XS-IV) ranging from 5 to 9 dl/g;
wherein the percentages of components (A) and (B) are referred to the sum of components (A) and (B) and wherein the sum of components (A) and (B) equals 100;
wherein the heterophasic copolymer has a MFR2 (230° C./2.16 Kg) ranging from 3.0 to 12.0 g/10 min.

### Claim 2 (depends on 1)

The heterophasic copolymer according to claim 1, wherein the amount of component (A) ranges from 58 to 71 wt. %, based on the total weight of the heterophasic copolymer.

### Claim 3 (depends on 1)

The heterophasic copolymer according to claim 1, wherein the comonomer of component (A) is butene-1.

### Claim 4 (depends on 3)

The heterophasic copolymer according to claim 3, wherein the butene-1 content ranges from 1.0 to 1.5 wt. %, based on the total weight of component (A).

### Claim 5 (depends on 1)

The heterophasic copolymer according to claim 1, wherein the MFR2 (230° C./2.16 Kg) of component (A) ranges from 80 to 120 g/10 min.

### Claim 6 (depends on 1)

The heterophasic copolymer according to claim 1, wherein component (B) is present in an amount ranging from 29 to 42 wt. %, based on the total weight of the heterophasic copolymer.

### Claim 7 (depends on 1)

The heterophasic copolymer according to claim 1, wherein the content of ethylene units in component (B) ranges from 28 to 35 wt. %, based on the total weight of component (B).

### Claim 8 (depends on 1)

The heterophasic copolymer according to claim 1, wherein the intrinsic viscosity of the fraction soluble in xylene at room temperature (XS-IV) for component (B) ranges from 6 to 8 dl/g.

### Claim 9 (depends on 1)

The heterophasic copolymer according to claim 1, having a value of Charpy impact resistance at 23° C. ranging from 40 to 100 KJ/m2.

### Claim 10 (depends on 1)

The heterophasic copolymer according to claim 1, having a value of Charpy impact resistance at −20° C. ranging from 3.0 to 5.0 KJ/m2.

### Claim 11 (depends on 1)

A thermoplastic polyolefin composition comprising the heterophasic copolymer of claim 1.

### Claim 12 (depends on 11)

The thermoplastic polyolefin composition according to claim 11, wherein the amount of heterophasic copolymer is up to 30% by weight.

### Claim 13 (depends on 11)

An article comprising the thermoplastic polyolefin composition of claim 11.

### Claim 14 (depends on 13)

The article according to claim 13, being an automotive part.