# US 2023/0265269 A1 · Enhanced aging and reduced shrinkback polymeric composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265269 A1
- Document ID: US20230265269A1
- Status: Published application
- Kind: A1
- Application number: 18/004,221
- Filed: 2021-10-04
- Published: 2023-08-24
- Earliest claimed: 2020-10-09
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Stacey A. Saba; Mohamed Esseghir; Theo Geussens; Yushan Hu; Brayden E. Glad; Andrew T. Heitsch; Buu-Dang Nguyen
- Web page: https://patentgrep.com/patent/US20230265269A1

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2203/206: use in coating or encapsulating of electronic parts
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/062: HDPE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polymeric composition includes (i) a copolymer of ethylene and an alpha olefin comonomer, the copolymer having a density of 0.945 g/cc to 0.960 g/cc, (ii) an ethylene-based polymer, and (iii) polyethylene glycol. The combination of (i) and (ii) has a High Mw Comonomer Content of 3.2 wt % or greater based on a total weight of the combined (i) and (ii) over the weight average molecular weight range of 105 g/mol to 105.5 g/mol as measured by GPC, wherein 15 wt % or greater of the total weight of the polymeric composition is the combined (i) and (ii) having a molecular weight in the range of 105 g/mol to 105.5 g/mol as measured by GPC, wherein the polymeric composition has a Relevant Comonomer Content of 0.6 wt % or greater and wherein the polymeric composition has a density of 0.945 g/cc or greater as measured according to ASTM D792.

## Claims

### Claim 1

A polymeric composition, comprising:
(i) a copolymer of ethylene and an alpha olefin comonomer, the copolymer having a density of 0.945 g/cc to 0.960 g/cc;
(ii) an ethylene-based polymer; and
(iii) polyethylene glycol,
wherein the combination of (i) and (ii) has a High Mw Comonomer Content of 3.2 wt % or greater based on a total weight of the combined (i) and (ii) over the weight average molecular weight range of 105 g/mol to 105.5 g/mol as measured by GPC,
wherein 15 wt % or greater of the total weight of the polymeric composition is the combined (i) and (ii) having a molecular weight in the range of 105 g/mol to 105.5 g/mol as measured by GPC,
wherein the polymeric composition has a Relevant Comonomer Content of 0.6 wt % or greater, and
wherein the polymeric composition has a density of 0.945 g/cc or greater as measured according to ASTM D792.

### Claim 2 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 35 wt % to 85 wt % of the copolymer based on the total weight of the polymeric composition.

### Claim 3 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 0.5 wt % to 1 wt % of the polyethylene glycol based on the total weight of the polymeric composition and the polyethylene glycol.

### Claim 4 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 15 wt % to 30 wt % of the ethylene-based polymer based on the total weight of the polymeric composition, and the ethylene based polymer is a linear low-density polyethylene having a density of 0.91 g/cc to 0.93 g/cc as measured according to ASTM D792.

### Claim 5 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 15 wt % to 19 wt % of the ethylene based polymer based on the total weight of the polymeric composition and the ethylene based polymer is a plastomer having a density of 0.90 g/cc to 0.91 g/cc as measured according to ASTM D792.

### Claim 6 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 45 wt % to 55 wt % of the ethylene-based polymer based on the total weight of the polymeric composition and the ethylene-based polymer is a high-density polyethylene having a density of 0.93 g/cc to 0.95 g/cc as measured according to ASTM D792.

### Claim 7 (depends on 1)

The polymeric composition of claim 1, wherein the polymeric composition comprises from 10 wt % to 15 wt % of the ethylene-based polymer based on the total weight of the polymeric composition and the ethylene based polymer is an elastomer having a density of 0.80 g/cc to 0.90 g/cc as measured according to ASTM D792.

### Claim 8 (depends on 1)

The polymeric composition of claim 1, wherein the combination of (i) and (ii) has a High Mw Comonomer Content of 12.0 wt % or less over the molecular weight range of 105 g/mol to 105.5 g/mol as measured by GPC.

### Claim 9 (depends on 1)

The polymeric composition of claim 1, wherein 30 wt % or less of the total weight of the polymeric composition is the combined (i) and (ii) having a molecular weight in the range of 105 g/mol to 105.5 g/mol as measured by GPC.

### Claim 10 (depends on 1)

A coated conductor comprising:
a conductor; and
the polymeric composition of claim 1 disposed at least partially around the conductor.