# US 2023/0265264 A1 · Polyolefin formulation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265264 A1
- Document ID: US20230265264A1
- Status: Published application
- Kind: A1
- Application number: 18/043,793
- Filed: 2021-10-25
- Published: 2023-08-24
- Earliest claimed: 2020-10-30
- Assignees: Dow Global Technologies LLC; Rohm and Haas Company
- Applicants: Dow Global Technologies LLC; Rohm and Haas Company
- Inventors: Xindi Yu; Paul M. Mwasame; Decai Yu; Sukrit Mukhopadhyay; Yuanqiao Rao; Timothy J. Person; Dachao Li; Junsi Gu; Jeffrey M. Cogen
- Web page: https://patentgrep.com/patent/US20230265264A1

## CPC

- C08K 5/07: Aldehydes; Ketones
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- C09D 123/06: Polyethylene
- H01B 3/441: {from alkenes}
- B32B 15/085: comprising polyolefins
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/202: Conductive
- B32B 2307/206: Insulating
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A crosslinkable polyolefin formulation comprises (A) a polyethylene polymer and (B) an arylketone of formula (I) as defined herein; products made therefrom; methods of making and using same; and articles containing same.

## Claims

### Claim 1

A coated conductor comprising a conductive core and an insulation layer at least partially covering the conductive core, wherein at least a portion of the insulation layer comprises a crosslinkable polyolefin formulation comprising (A) a polyethylene polymer and (B) an arylketone of formula (I):
wherein each of R1 to R6 is a hydrogen atom (H); or wherein R1 and R2, or R3 and R4, or R4 and R5, or R5 and R6, are bonded together with the carbon atoms in formula (I) to which they are bonded to form a fused 6-membered aryl ring and each of the remaining four of R1 to R6 is H; or wherein R2, R3, and R4 are bonded together in such a way with the carbon atoms in formula (I) to which they are bonded and the closest bridgehead carbon atom in formula (I) to form two fused 6-membered aryl rings and each of R1 R5, and R6 are H; and wherein one of RA and RB is a group of formula —C(═O)—R7 and the other of RA and RB is H, or wherein RA is a group of formula —C(═O)—R7 and RB and R1 are bonded together with the carbon atoms in formula (I) to which they are bonded to form a fused 6-membered aryl ring and R2 to R6 are as defined above; wherein R7 is an unsubstituted (C1-C40)alkyl group; wherein the (A) polyethylene polymer comprises from 51 to 100 weight percent (wt %) ethylene-derived constituent units and from 49 to 0 wt %, respectively, of alpha-olefin-derived constituent units, based on weight of the (A) polyethylene polymer; and wherein the crosslinkable polyolefin formulation comprises from 30.0 to 99.9 wt % of the (A) polyethylene polymer based on total weight of the crosslinkable polyolefin formulation and from 0.1 to 3.0 wt % of the (B) arylketone based on total weight of the crosslinkable polyolefin formulation.

### Claim 2 (depends on 1)

The coated conductor of claim 1 wherein the (B) arylketone is an arylketone of formula (Ia) or (Ib):
wherein R1 to R7 and RB are independently as defined for formula (I).

### Claim 3 (depends on 1)

The coated conductor of claim 1 wherein the (B) arylketone is an arylketone of formula (Ia-1), (Ia-2), or (Ia-3):
wherein each R7 independently is as defined for formula (I).

### Claim 4 (depends on 1)

The coated conductor of claim 1 wherein the (B) arylketone is an arylketone of formula (Ib-1):
wherein R7 independently is as defined for formula (I).

### Claim 5 (depends on 1)

The coated conductor of claim 1 wherein R7 is an unsubstituted (C1-C5)alkyl group or an unsubstituted (C6-C40)alkyl group.

### Claim 6 (depends on 1)

The coated conductor of claim 1 wherein the (A) polyethylene polymer comprises 100 wt % of ethylene-derived constituent units and is (A1) a low-density polyethylene homopolymer; or wherein the (A) polyethylene polymer comprises from 51 to 99.9 wt % ethylene-derived constituent units and from 49 to 0.1 wt % alpha-olefin-derived constituent units and is (A2) an ethylene/alpha-olefin copolymer.

### Claim 7 (depends on 1)

The coated conductor of claim 1 further comprising at least one additive wherein each additive is independently selected from the group consisting of: (C) an organic peroxide; (D) an anti-scorch agent; (E) an antioxidant; (F) a filler; (G) a flame retardant; (H) a hindered amine stabilizer; (I) a tree retardant; (J) a methyl radical scavenger; (K) a crosslinking coagent; (L) a nucleating agent; (M) a colorant; and a combination of any two or more of additives (C) to (M).

### Claim 8 (depends on 1)

A cured coated conductor comprising a conductive core and an insulation layer at least partially covering the conductive core, wherein at least a portion of the insulation layer comprises a crosslinked polyolefin product, wherein the cured coated conductor is made by a method comprising subjecting the coated conductor of claim 1 to a curing condition in such a way so as to crosslink the (A) polyethylene polymer, thereby making the crosslinked polyolefin product.

### Claim 9 (depends on 8)

A method of transmitting electricity, the method comprising applying a voltage across the conductive core of the coated conductor of claim 8 so as to generate a flow of electricity through the conductive core.

### Claim 10 (depends on 1)

The coated conductor of claim 1 wherein the crosslinkable polyolefin formulation has an improvement (increase) in electrical breakdown strength value eta, η, of at least +5 percent (%) relative to that of the (A) polyethylene polymer that is free of a voltage stabilizer; wherein the electrical breakdown strength values eta, η, are determined for a failure probability value of 63.2% using Weibull statistics according to the Electrical Breakdown Strength Test Method and Weibull Statistics Method described in the description.