# US 2023/0265244 A1 · Polyether ether ketone and method for producing polyether ether ketone

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265244 A1
- Document ID: US20230265244A1
- Status: Published application
- Kind: A1
- Application number: 18/024,240
- Filed: 2021-09-02
- Published: 2023-08-24
- Earliest claimed: 2020-09-02
- Assignees: Idemitsu Kosan Co., Ltd.
- Applicants: Idemitsu Kosan Co.,Ltd.
- Inventors: Koichi SUGA; Minoru SENGA; Hiromu KUMAGAI; Yuko MURAKAMI
- Web page: https://patentgrep.com/patent/US20230265244A1

## CPC

- C08G 65/4012: {Other compound (II) containing a ketone group, e.g. X-Ar-C(=O)-Ar-X for polyetherketones}
- C08G 65/40: from phenols (I) and other compounds (II), e.g. OH-Ar-OH + X-Ar-X, where X is halogen atom, i.e. leaving group
- C08G 65/4093: {characterised by the process or apparatus used}
- C08G 65/46: Post-polymerisation treatment, e.g. recovery, purification, drying
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided is a polyether ether ketone, comprising a repeating unit represented by the following formula (1), the polyether ether ketone having a crystallization temperature Tc of 255° C. or more, and satisfying one or both of the following conditions (A) and (B): (A) a fluorine atom content a is less than 2 mg/kg; and (B) a chlorine atom content b is 2 mg/kg or more.

## Claims

### Claim 1

A polyether ether ketone, comprising a repeating unit represented by the following formula (1), having a crystallization temperature Tc of 270° C. or more, and satisfying one or both of the following conditions (A) and (B):
(A) a fluorine atom content a is less than 2 mg/kg; and
(B) a chlorine atom content b is 2 mg/kg or more.

### Claim 2 (depends on 1)

The polyether ether ketone according to claim 1, wherein a raw material of the polyether ether ketone comprises 4,4′-dichlorobenzophenone.

### Claim 3 (depends on 1)

The polyether ether ketone according to claim 1, having a melt flow index of 100 g/10 min or less.

### Claim 4 (depends on 1)

The polyether ether ketone according to claim 1, having a reduced viscosity ηsp/c of 0.40 dl/g to 1.50 dl/g.

### Claim 5

A method for producing a polyether ether ketone, which comprises reacting 4,4′-dichlorobenzophenone and hydroquinone under a condition in which a highest temperature of a reaction mixture is 260° C. to 280° C.

### Claim 6 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, further comprising increasing a temperature of the reaction mixture to 150° C. or more, followed by holding of the temperature.

### Claim 7 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, further comprising increasing a temperature of the reaction mixture to 150° C. or more, followed by repetition of an increase of the temperature and holding of the temperature a plurality of times.

### Claim 8 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, further comprising holding the reaction mixture at 180° C. to 220° C. for 0.5 hour to 2 hours.

### Claim 9 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, further comprising holding the reaction mixture at 230° C. to 270° C. for 0.5 hour to 2 hours.

### Claim 10 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, further comprising holding the reaction mixture at 280° C. to 320° C. for 1 hour to 8 hours.

### Claim 11 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein a time period from a time point at which a temperature of the reaction mixture reaches 150° C. to a time point at which the temperature reaches the highest temperature is 2.0 hours to 10 hours.

### Claim 12 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein the polyether ether ketone to be produced has a crystallization temperature Tc of 255270° C. or more.

### Claim 13 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein the polyether ether ketone to be produced has a melt flow index of 100 g/10 min or less.

### Claim 14 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein the polyether ether ketone to be produced has a reduced viscosity ηsp/c of 0.40 dl/g to 1.00 dl/g.

### Claim 15

(canceled)

### Claim 16 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein the reaction mixture contains only one kind of solvent as a solvent.

### Claim 17 (depends on 5)

The method for producing a polyether ether ketone according to claim 5, wherein the reaction mixture is free of any of sodium fluoride, potassium fluoride, rubidium fluoride, or cesium fluoride.