# US 2023/0265013 A1 · Method for the Thermal Treatment of Mineral Raw Materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0265013 A1
- Document ID: US20230265013A1
- Status: Published application
- Kind: A1
- Application number: 18/014,090
- Filed: 2021-07-02
- Published: 2023-08-24
- Earliest claimed: 2020-07-02
- Assignees: S.A. Lhoist Recherche et Developpement
- Applicants: Lhoist Recherche et Développement S.A.
- Inventors: Thomas Perterer
- Web page: https://patentgrep.com/patent/US20230265013A1

## CPC

- C04B 2/104: {Ingredients added before or during the burning process}
- F27D 7/04: Circulating atmospheres by mechanical means
- F27D 11/06: Induction heating, i.e. in which the material being heated, or its container or elements embodied therein, form the secondary of a transformer
- F27D 2007/045: {Fans}
- F27M 2003/03: Calcining
- Y02P 40/40: Production or processing of lime, e.g. limestone regeneration of lime in pulp and sugar mills
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- F27M: INDEXING SCHEME RELATING TO ASPECTS OF THE CHARGES OR FURNACES, KILNS, OVENS OR RETORTS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for the thermal treatment of mineral raw materials such as limestone or dolomite is shown and described, which includes at least the following steps of a. providing a mineral bulk material and a conductive material and b. placing the mineral bulk material and the conductive material into a kiln, generating an electromagnetic field inside the kiln, thermally treating the mineral bulk material in the kiln by means of electromagnetic excitation of the conductive material in the electromagnetic field, and removing the thermally treated mineral bulk material and the conductive material from the kiln. Using the method described, even large quantities of mineral bulk material can be efficiently converted.

## Claims

### Claim 1

A method for the thermal treatment of mineral raw materials, comprising at least the steps of:
a. providing a mineral bulk material and a conductive material,
b. placing the mineral bulk material and the conductive material into a kiln,
c. generating an electromagnetic field inside the kiln,
d. thermally treating the mineral bulk material in the kiln by means of electromagnetic excitation of the conductive material in the electromagnetic field, and
e. removing the thermally treated mineral bulk material and the conductive material from the kiln.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the mineral bulk material and the conductive material are mixed before being placed into the kiln.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the mineral bulk material comprises a hydroxide and/or a carbonate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the mineral bulk material is selected from the group consisting of limestone, dolomite, magnesite, hydrated lime, carbonate ores and mixtures thereof.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the mineral bulk material has a bulk density of from 1.0 to 3.0 t/m3, in particular from 1.1 to 2.6 t/m3.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the has a melting point of at least 500° C. in particular at least 900° C. or at least 1000° C. or at least 1100° C. or at least 1200° C. or at least 1300° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the conductive material comprises at least one metal from the group consisting of iron, copper, tungsten, nickel, and cobalt, in particular iron.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the conductive material is substantially spherical.

### Claim 9 (depends on 1)

The method according to claim 1, wherein that the conductive material has a mean particle size (d50) of from 1.0 to 70.0 mm, in particular from 2.0 to 50.0 mm.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the amount of mineral bulk material in method step a. is at least 10 wt. %. in particular at least 20 wt. % or at least 30 wt. % or at least 40 wt. %. based on the total amount of mineral bulk material and conductive material, and/or the amount of mineral bulk material in method step a. is a maximum of 90 wt. %. in particular a maximum of 80 wt. % or a maximum of 70 wt. % or a maximum of 60 wt. %, based on the total amount of mineral bulk material and conductive material.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the mineral bulk material in method step d. is exposed to a temperature of from 800 to 1500° C., in particular from 850 to 1450° C. or from 900 to 1250° C.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the conductive material has a melting point which is above the temperature to which the mineral bulk material in method step d. is exposed, in particular has a melting point which is at least 50° C. in particular at least 100° C. or at least 200° C. or at least 300° C. above the temperature to which the mineral bulk material is exposed.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the electromagnetic field in method step c. has a frequency of from 50 Hz to 30 MHz, in particular from 0.1 MHz to 2 MHz.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the gas which forms during the thermal treatment is extracted from the kiln, in particular is extracted from the kiln by means of a fan.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the gas comprises carbon dioxide.

### Claim 16 (depends on 15)

The method according to claim 15, wherein at least part of the carbon dioxide extracted from the kiln is taken away for further use and/or storage.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the method comprises at least the steps of:
f. cooling the removed mineral bulk material and the conductive material, and
g. separating the conductive material from the thermally treated mineral bulk material.

### Claim 18 (depends on 17)

The method according to claim 17, wherein, after method step g., the separated conductive material is placed back into the kiln.

### Claim 19

A kiln comprising a kiln interior, a kiln wall, and a device for generating an electromagnetic field, wherein the device for generating an electromagnetic field is mounted outside the kiln interior and wherein the kiln has a wall thickness of a maximum of 50 cm.

### Claim 20 (depends on 19)

The kiln according to claim 19, wherein the kiln comprises a fan for extracting gases.

### Claim 21 (depends on 19)

The kiln according to either claim 19, wherein the kiln has an average inner diameter of 0.1 to 5 m, in particular 0.2 to 2 m, or 0.3 to 1.5 m.

### Claim 22

A use of an electromagnetically excited conductive material for the thermal treatment of a mineral raw material.

### Claim 23 (depends on 22)

The use according to claim 22, wherein the mineral raw material is a mineral bulk material and/or the electromagnetically excited conductive material.

### Claim 24 (depends on 22)

The use according to either claim 22, wherein the electromagnetically excited conductive material is used for calcining limestone and/or dolomite.

### Claim 25 (depends on 1)

The burnt lime and/or burnt dolomite which can be obtained from a method according to claim 1, wherein the mineral bulk material is selected from limestone and/or dolomite.

### Claim 26 (depends on 20)

The apparatus for the thermal treatment of a mineral raw material, comprising
a first metering installation containing a mineral bulk material,
a second metering installation containing a conductive material,
a supply system for the transport of the mineral bulk material and the conductive material,
a kiln according to claim 20,
at least one exhaust pipe connected to the kiln and the fan by means of which the extracted gas can be taken away,
at least one inlet on the kiln by means of which the mineral bulk material and the conductive material can be conveyed into the kiln by the supply system,
at least one gas-tight outlet on the kiln for removing the thermally treated mineral bulk material and the conductive material,
a discharge system for taking away the thermally treated mineral bulk material and the conductive material,
a separation system for separating the thermally treated mineral bulk material from the conductive material.
a further conveyor system for the transport of the separated conductive material to the second metering installation.

### Claim 27 (depends on 26)

The apparatus according to claim 26, wherein the inlet is a substantially gas-tight inlet.