# US 2023/0264975 A1 · Doped nickel-rich ternary material and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0264975 A1
- Document ID: US20230264975A1
- Status: Published application
- Kind: A1
- Application number: 18/139,947
- Filed: 2023-04-26
- Published: 2023-08-24
- Earliest claimed: 2020-10-26
- Assignees: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Hunan Brunp Ev Recycling Co., Ltd.
- Applicants: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Hunan Brunp Ev Recycling Co., Ltd.
- Inventors: Shaolin Du; Haijun Yu; Yinghao Xie; Xuemei Zhang; Banglai Ming; Peng Hou
- Web page: https://patentgrep.com/patent/US20230264975A1

## CPC

- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are a doped nickel-rich ternary material and a preparation method thereof. The preparation method comprises the following steps: (1) Mixing a nickel source, a cobalt source, and a manganese source in a solvent to obtain a solution A, adding oxidant and doping elements to the solution A, and stirring to obtain solution B; (2) Adding a complexing agent and nitric acid to the solution B and stirring to obtain solution C; (3) Drying the solution C to obtain aerogel D; (4) Grinding the aerogel D, and subjecting it to low-temperature pre-calcinating, and heating the aerogel to perform first calcinating to obtain precursor powder E; (5) Mixing the precursor powder E with a lithium source to obtain a mixture, and subjecting the mixture to second calcinating, grinding, and screening to obtain the doped nickel-rich ternary material.

## Claims

### Claim 1

A method of preparing a doped nickel-rich ternary material, comprising the following steps:
(1) dissolving a nickel source, a cobalt source, and a manganese source in a solvent to obtain solution A, adding an oxidant and a doping element to the solution A to obtain solution B, wherein the oxidizing agent is at least one selected from the group consisting of sodium persulfate, sodium peroxide, and ammonium persulfate;
(2) adding a complexing agent and nitric acid to the solution B to obtain solution C, wherein the complexing agent is an acrylic acid solution;
(3) drying the solution C to obtain an aerogel compound, and grinding the aerogel compound to obtain aerogel D;
(4) subjecting the aerogel D to a first calcinating, followed by a second calcinating to obtain a precursor powder E, wherein the second calcinating is carried out at a temperature of 400° C.-600° C. for 4-8 h in air or an oxygen atmosphere;
(5) mixing the precursor powder E with a lithium source to obtain a mixture, subjecting the mixture to calcinating, grinding and screening to obtain the doped nickel-rich ternary material; wherein the doping element is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in step (1), the nickel source is nickel nitrate hexahydrate, the cobalt source is cobalt nitrate hexahydrate, and the manganese source is manganese acetate tetrahydrate; a molar ratio of the nickel source to the cobalt source to the manganese source is (0.6-0.9):(0.05-0.2):(0.05-0.2).

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step (1), the doping element being added to the solution A is in the form of a nitrate, a phosphate, or a sulfate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein in step (4), the first calcinating is carried out at a temperature of 150° C.-250° C. for 1-3 h in air or an oxygen atmosphere.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in step (5), the lithium source is lithium carbonate or lithium hydroxide.

### Claim 6 (depends on 1)

A doped nickel-rich ternary material prepared by the method of claim 1, wherein the doped nickel-rich ternary material has a chemical formula of LiNixCoyMnzMiO2, M is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La, wherein 0.6≤x≤0.9, 0.05≤y≤0.2, 0.05≤z≤0.2, 0.00001≤i≤0.1, x+y+z+i=1.

### Claim 7 (depends on 2)

A doped nickel-rich ternary material prepared by the method of claim 2, wherein the doped nickel-rich ternary material has a chemical formula of LiNixCoyMnzMiO2, M is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La, wherein 0.6≤x≤0.9, 0.05≤y≤0.2, 0.05≤z≤0.2, 0.00001≤i≤0.1, x+y+z+i=1.

### Claim 8 (depends on 3)

A doped nickel-rich ternary material prepared by the method of claim 3, wherein the doped nickel-rich ternary material has a chemical formula of LiNixCoyMnzMiO2, M is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La, wherein 0.6≤x≤0.9, 0.05≤y≤0.2, 0.05≤z≤0.2, 0.00001≤i≤0.1, x+y+z+i=1.

### Claim 9 (depends on 4)

A doped nickel-rich ternary material prepared by the method of claim 4, wherein the doped nickel-rich ternary material has a chemical formula of LiNixCoyMnzMiO2, M is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La, wherein 0.6≤x≤0.9, 0.05≤y≤0.2, 0.05≤z≤0.2, 0.00001≤i≤0.1, x+y+z+i=1.

### Claim 10 (depends on 5)

A doped nickel-rich ternary material prepared by the method of claim 5, wherein the doped nickel-rich ternary material has a chemical formula of LiNixCoyMnzMiO2, M is at least one selected from the group consisting of Zr, Nb, Al, F, Mn, and La, wherein 0.6≤x≤0.9, 0.05≤y≤0.2, 0.05≤z≤0.2, 0.00001≤i≤0.1, x+y+z+i=1.

### Claim 11 (depends on 6)

The doped nickel-rich ternary material according to claim 6, wherein the doped nickel-rich ternary material has a first reversible capacity of 181-193 mAh/g.

### Claim 12 (depends on 7)

The doped nickel-rich ternary material according to claim 7, wherein the doped nickel-rich ternary material has a first reversible capacity of 181-193 mAh/g.

### Claim 13 (depends on 8)

The doped nickel-rich ternary material according to claim 8, wherein the doped nickel-rich ternary material has a first reversible capacity of 181-193 mAh/g.

### Claim 14 (depends on 9)

The doped nickel-rich ternary material according to claim 9, wherein the doped nickel-rich ternary material has a first reversible capacity of 181-193 mAh/g.

### Claim 15 (depends on 10)

The doped nickel-rich ternary material according to claim 10, wherein the doped nickel-rich ternary material has a first reversible capacity of 181-193 mAh/g.

### Claim 16 (depends on 6)

A lithium battery comprising the doped nickel-rich ternary material according to claim 6.

### Claim 17 (depends on 11)

A lithium battery comprising the doped nickel-rich ternary material according to claim 11.