# US 2023/0264945 A1 · Roughness selectivity for mems movement stiction reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0264945 A1
- Document ID: US20230264945A1
- Status: Published application
- Kind: A1
- Application number: 18/308,950
- Filed: 2023-04-28
- Published: 2023-08-24
- Earliest claimed: 2020-11-04
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Hsi-Cheng HSU; Kuo-Hao LEE; Jui-Chun WENG; Ching-Hsiang HU; Ji-Hong CHIANG; Lavanya SANAGAVARAPU; Chia-Yu LIN; Chia-Chun HUNG; Jia-Syuan LI; Yu-Pei CHIANG
- Web page: https://patentgrep.com/patent/US20230264945A1

## CPC

- B81B 3/0005: {Anti-stiction coatings}
- B81B 3/001: {Structures having a reduced contact area, e.g. with bumps or with a textured surface}
- B81C 1/00968: {Methods for breaking the stiction bond}
- B81B 2201/0235: Accelerometers
- B81B 2201/0242: Gyroscopes
- B81B 2201/0257: Microphones or microspeakers
- B81B 2201/0264: Pressure sensors
- B81B 2203/0118: Cantilevers
- B81C 2201/112: Depositing an anti-stiction or passivation coating, e.g. on the elastic or moving parts
- B81C 2201/115: Roughening a surface
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)

## Abstract

A micro-electromechanical-system (MEMS) device may be formed to include an anti-stiction polysilicon layer on one or more moveable MEMS structures of a device wafer of the MEMS device to reduce, minimize, and/or eliminate stiction between the moveable MEMS structures and other components or structures of the MEMS device. The anti-stiction polysilicon layer may be formed such that a surface roughness of the anti-stiction polysilicon layer is greater than the surface roughness of a bonding polysilicon layer on the surfaces of the device wafer that are to be bonded to a circuitry wafer of the MEMS device. The higher surface roughness of the anti-stiction polysilicon layer may reduce the surface area of the bottom of the moveable MEMS structures, which may reduce the likelihood that the one or more moveable MEMS structures will become stuck to the other components or structures.

## Claims

### Claim 1

A method, comprising:
forming a polysilicon layer over a substrate of a device wafer of a micro-electromechanical-system (MEMS) device;
increasing a surface roughness of a first portion of the polysilicon layer relative to a surface roughness of a second portion of the polysilicon layer such that the surface roughness of the first portion is greater relative to the surface roughness of the second portion;
etching through a plurality of portions of the first portion and through a plurality of associated portions of the substrate to form a plurality of moveable MEMS structures; and
bonding the device wafer and a circuitry wafer of the MEMS device after forming the plurality of moveable MEMS structures.

### Claim 2 (depends on 1)

The method of claim 1, wherein the surface roughness of the second portion in root means square roughness (Rq) is less than approximately 30 nanometers.

### Claim 3 (depends on 1)

The method of claim 1, wherein increasing the surface roughness of the first portion comprises:
forming an oxide layer on the polysilicon layer,
wherein the oxide layer oxidizes a top surface of the first portion; and
etching the oxide layer on the first portion,
wherein oxidization of the top surface and etching the oxide layer on the first portion increases the surface roughness of the first portion.

### Claim 4 (depends on 1)

The method of claim 1, wherein forming the polysilicon layer comprises:
forming the polysilicon layer to a thickness equal to or less than approximately 10,000 angstroms.

### Claim 5 (depends on 1)

The method of claim 1, wherein increasing the surface roughness of the first portion comprises:
increasing the surface roughness of the first portion to decrease a likelihood of stiction between the plurality of moveable MEMS structures and a passivation layer on the circuitry wafer.

### Claim 6 (depends on 1)

The method of claim 1, wherein increasing the surface roughness of the first portion comprises:
increasing the surface roughness of the first portion to decrease surface area on a bottom of the plurality of moveable MEMS structures.

### Claim 7 (depends on 1)

The method of claim 1, wherein increasing the surface roughness of the first portion comprises:
increasing the surface roughness of the first portion to a particular surface roughness such that the MEMS device satisfies a threshold quantity of drop test cycles.

### Claim 8

A method, comprising:
etching through a plurality of portions, of a first portion of a polysilicon layer over a substrate of a device wafer of a micro-electromechanical-system (MEMS) device, and a plurality of associated portions, of the substrate of the device wafer, to form a plurality of MEMS structures,
wherein a surface roughness of the first portion of the polysilicon layer is greater than a surface roughness of a second portion of the polysilicon layer; and
bonding the device wafer and a circuitry wafer of the MEMS device after etching through the plurality of portions of the first portion and the plurality of associated portion so the substrate.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
bonding the device wafer and a capping wafer of the MEMS device; and
wherein forming the polysilicon layer comprises:
forming the polysilicon layer after bonding the device wafer and the capping wafer.

### Claim 10 (depends on 8)

The method of claim 8, further comprising:
bonding the device wafer and a capping wafer of the MEMS device; and
wherein forming the polysilicon layer comprises:
forming the polysilicon layer after bonding the device wafer and the capping wafer.

### Claim 11 (depends on 10)

The method of claim 10, wherein bonding the device wafer and the capping wafer of the MEMS device comprises:
fusion bonding the device wafer and the capping wafer.

### Claim 12 (depends on 8)

The method of claim 8, further comprising:
forming one or more germanium bonding pads on the first portion and on the one or more second portions prior to bonding the device wafer and the circuitry wafer.

### Claim 13 (depends on 12)

The method of claim 12, wherein bonding the device wafer and the circuitry wafer comprises:
forming a eutectic bond between the one or more germanium bonding pads and one or more metal bonding pads of the circuitry wafer.

### Claim 14

A method, comprising:
increasing a surface roughness, of a first portion of a polysilicon layer of a substrate of a device wafer of a micro-electromechanical-system (MEMS) device, relative to a surface roughness, of a second portion of the polysilicon layer, such that the surface roughness of the first portion is greater relative to the surface roughness of the second portion;
forming a plurality of moveable MEMS structures using the first portion and the substrate; and
bonding the device wafer and a circuitry wafer of the MEMS device after forming the plurality of moveable MEMS structures.

### Claim 15 (depends on 14)

The method of claim 14, wherein the plurality of moveable MEMS structures is formed via etching the first portion and the substrate.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
depositing an oxide layer on the polysilicon layer,
wherein forming the plurality of moveable MEMS structures is based on depositing the oxide layer on the polysilicon layer.

### Claim 17 (depends on 14)

The method of claim 14, wherein forming the polysilicon layer comprises:
forming the polysilicon layer to a thickness equal to or less than approximately 10,000 angstroms.

### Claim 18 (depends on 14)

The method of claim 14, further comprising:
bonding the device wafer and a capping wafer of the MEMS device; and
wherein forming the polysilicon layer comprises:
forming the polysilicon layer based on bonding the device wafer and the capping wafer.

### Claim 19 (depends on 14)

The method of claim 14, further comprising:
forming one or more germanium bonding pads on the first portion and the second portion.

### Claim 20 (depends on 19)

The method of claim 19, wherein forming the one or more germanium bonding pads comprises:
forming a germanium layer on the first portion and on the second portion prior to bonding the device wafer and the circuitry wafer; and
removing one or more portions of the germanium layer on the first portion to form one or more germanium bonding pads.