# US 2023/0264179 A1 · Preparation Method and Use of Cobalt Nanoparticle/Boron Nitride Composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0264179 A1
- Document ID: US20230264179A1
- Status: Published application
- Kind: A1
- Application number: 18/147,243
- Filed: 2022-12-28
- Published: 2023-08-24
- Earliest claimed: 2022-02-23
- Assignees: China University of Petroleum (East China)
- Applicants: China University of Petroleum (East China)
- Inventors: Pengcheng Dai; Yan Feng; Yang Li; Xuebo Zhao; Dehong Yang; Hongyu Gan; Yubin Tian
- Web page: https://patentgrep.com/patent/US20230264179A1

## CPC

- B01J 23/80: with zinc, cadmium or mercury
- B01J 37/10: in the presence of water, e.g. steam
- B01J 27/24: Nitrogen compounds
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/51: Spheres
- B01J 37/009: {Preparation by separation, e.g. by filtration, decantation, screening}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/343: {of ultrasonic wave energy}
- C02F 1/722: {Oxidation by peroxides}
- C02F 1/725: {by catalytic oxidation}
- C02F 2101/30: Organic compounds
- C02F 2101/306: {Pesticides}
- C02F 2101/308: {Dyes; Colorants; Fluorescent agents}
- C02F 2101/345: {Phenols}
- C02F 2101/36: containing halogen
- C02F 2101/38: containing nitrogen
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- Y02W 10/37: using solar energy
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present disclosure belongs to the technical field of sewage treatment, and relates to a preparation method and use of a cobalt nanoparticle/boron nitride composite. The preparation method includes the following steps: dissolving 2-methylimidazole and boric acid in deionized water, and stirring to obtain a solution A; dissolving Co(NO3)2·6H2O and Zn(NO)3·6H2O in deionized water, and conducting ultrasonic dispersion to obtain a solution B; transferring the solution B into the solution A, and stirring to form a clear and transparent solution; transferring the clear and transparent solution into a container lined with Teflon, and conducting a reaction; subjecting an obtained product to cooling, filtration, washing, and drying sequentially to obtain a precursor of the composite; and conducting roasting on the precursor in an ammonia gas atmosphere to obtain the cobalt nanoparticle/boron nitride composite with a spherical superstructure.

## Claims

### Claim 1

A preparation method of a cobalt nanoparticle/boron nitride composite, comprising the following steps:
S1, preparation of a solution A: dissolving 2-methylimidazole and boric acid at a molar ratio of (0.5-1):(1-2) in deionized water, and stirring for 15 min to obtain the solution A;
S2, preparation of a solution B: dissolving Co(NO3)2·6H2O and Zn(NO)3·6H2O at a molar ratio of (0.5-1):(1-2) in deionized water, and conducting ultrasonic dispersion for 15 min to obtain the solution B;
S3, preparation of a precursor: transferring the solution B into the solution A, and stirring for 15 min to form a clear and transparent solution; transferring the clear and transparent solution into a container lined with Teflon, and conducting a reaction at 150° C. for 6 h to 18 h; subjecting an obtained product to cooling, filtration, washing, and drying sequentially to obtain the precursor of the composite; and
S4, conducting roasting on the precursor obtained in step S3 at 800° C. to 1,200° C. for 2 h to 5 h in an ammonia gas atmosphere to obtain the cobalt nanoparticle/boron nitride composite with a spherical superstructure.

### Claim 2 (depends on 1)

The preparation method of a cobalt nanoparticle/boron nitride composite according to claim 1, wherein in step S1, 10 mL to 20 mL of the deionized water is used for every 15 mmol of the 2-methylimidazole, and wherein in step S2, 10 mL to 20 mL of the deionized water is used for every 2.6 mmol of the Zn(NO3)2·6H2O.

### Claim 3 (depends on 1)

The preparation method of a cobalt nanoparticle/boron nitride composite according to claim 1, wherein in step S3, the cooling, filtration, washing, and drying specifically comprises: cooling the clear and transparent solution to a room temperature, and conducting filtration to collect a solid product; washing the solid product 3 to 5 times with deionized water; and drying a washed solid product in an oven at 50° C. to 80° C. for 6 h to 12 h.

### Claim 4 (depends on 1)

The preparation method of a cobalt nanoparticle/boron nitride composite according to claim 1, wherein in step S3, the container is a stainless steel autoclave lined with the Teflon.

### Claim 5 (depends on 1)

A method for degradation of an organic pollutant in water by catalytic activation of a persulfate using a cobalt nanoparticle/boron nitride composite prepared by the preparation method according to claim 1, comprising the following steps:
(1) adding the composite to sewage containing the organic pollutant and stirring for 10 min to 30 min to obtain mixed sewage, wherein the organic pollutant and the composite have a mass concentration ratio of 1:(4-10); and
(2) adding the persulfate to the mixed sewage, and conducting a reaction by stirring at 10° C. to 40° C. for 1 min to 30 min to degrade the organic pollutant in the sewage, wherein the composite and the persulfate have a mass concentration ratio of 1:(15-30).

### Claim 6 (depends on 5)

The method for degradation of an organic pollutant in water by catalytic activation of a persulfate using the cobalt nanoparticle/boron nitride composite according to claim 5, wherein the sewage has a pH value of 3 to 11.

### Claim 7 (depends on 5)

The method for degradation of an organic pollutant in water by catalytic activation of a persulfate using the cobalt nanoparticle/boron nitride composite according to claim 5, wherein the organic pollutant is one or a combination of two or more selected from the group consisting of 2-chlorophenol, 3-chlorophenol, 4-chlorophenol, bisphenol A, atrazine, and rhodamine B.

### Claim 8 (depends on 5)