# US 2023/0258747 A1 · Composite Hard Masks For Ultra-Thin Magnetic Sensors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0258747 A1
- Document ID: US20230258747A1
- Status: Published application
- Kind: A1
- Application number: 17/671,413
- Filed: 2022-02-14
- Published: 2023-08-17
- Earliest claimed: 2022-02-14
- Assignees: Headway Technologies, Inc.
- Applicants: Headway Technologies, Inc.
- Inventors: Tom Zhong; Min Li; Ruhang Ding; Hiroshi Omine; QingJun Qin; Richard Zhou; Yunqing Cai; Yewhee Chye; Minghui Yu
- Web page: https://patentgrep.com/patent/US20230258747A1

## CPC

- G01R 33/093: {using multilayer structures, e.g. giant magnetoresistance sensors (thin magnetic films H01F10/00)}
- B24B 37/042: {operating processes therefor}
- B24B 37/048: {of sliders and magnetic heads of hard disc drives or the like}
- G01R 33/0052: {Manufacturing aspects; Manufacturing of single devices, i.e. of semiconductor magnetic sensor chips (devices based on galvano-magnetic effect or the like H10N50/85)}
- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- G03F 7/16: Coating processes; Apparatus therefor (applying coatings to base materials in general B05; applying photosensitive compositions to base for photographic purposes G03C1/74)
- G03F 7/36: Imagewise removal not covered by groups G03F7/30 - G03F7/34, e.g. using gas streams, using plasma
- G03F 7/427: {using plasma means only}
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 10/3272: {by use of anti-parallel coupled [APC] ferromagnetic layers, e.g. artificial ferrimagnets [AFI], artificial [AAF] or synthetic [SAF] anti-ferromagnets}
- H01F 41/308: {lift-off processes, e.g. ion milling, for trimming or patterning}
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A composite hard mask is disclosed. In some embodiments, a first sacrificial hard mask layer comprising an amorphous carbon or silicon nitride and a second sacrificial hard mask layer comprising a silicon nitride, silicon oxide, metal, metal oxide, or metal nitride, wherein the first and second sacrificial hard mask layers are not made of the same material.

## Claims

### Claim 1

A composite hard mask, comprising:
a first sacrificial hard mask layer comprising an amorphous carbon or silicon nitride; and
a second sacrificial hard mask layer comprising a silicon nitride, silicon oxide, metal, metal oxide, or metal nitride,
wherein the first and second sacrificial hard mask layers are not made of the same material.

### Claim 2 (depends on 1)

The composite hard mask of claim 1, wherein the first sacrificial hard mask layer is an amorphous carbon masking layer.

### Claim 3 (depends on 1)

The composite hard mask of claim 1, wherein the first sacrificial hard mask layer is a silicon nitride masking layer.

### Claim 4 (depends on 1)

The composite hard mask of claim 1, wherein the second sacrificial hard mask layer comprises Ti, Ta, NiCr, NiFe, TaOx, SmOx, Al2O3, SiO2, or SiN.

### Claim 5 (depends on 1)

The composite hard mask of claim 1, wherein the second sacrificial hard mask layer is made from material that can be removed without affecting the first sacrificial hard mask layer.

### Claim 6 (depends on 1)

The composite hard mask of claim 1, wherein the first sacrificial hard mask layer comprises amorphous carbon and the second sacrificial hard mask layer comprises SiO2, NiFe, NiCr, SiN, Ti, TaOx, or SmOx.

### Claim 7 (depends on 1)

The composite hard mask of claim 1, wherein the first sacrificial hard mask layer comprises SiN and the second sacrificial hard mask layer comprises Al2O3, or SiO2.

### Claim 8 (depends on 1)

The composite hard mask of claim 1, wherein a thickness of the first sacrificial hard mask layer is 10 to 150 Angstroms.

### Claim 9 (depends on 1)

The composite hard mask of claim 1, wherein a thickness of the second sacrificial hard mask layer is 20 to 800 Angstroms.

### Claim 10 (depends on 1)

The composite hard mask of claim 1, wherein a thickness of the first sacrificial hard mask layer is less than a thickness of the second sacrificial hard mask layer.

### Claim 11 (depends on 1)

A film stack structure, comprising:
the composite hard mask of claim 1.

### Claim 12 (depends on 11)

The film stack structure of claim 11, further comprising a bottom electrode.

### Claim 13 (depends on 12)

The film stack structure of claim 12, further comprising a seed layer, an anti-ferromagnetic (AFM) pinning layer, a ferromagnetic pinned layer, a coupling layer, a reference layer, a spacer or barrier layer, a ferromagnetic free layer, and a capping layer sequentially formed on the bottom electrode.

### Claim 14 (depends on 13)

The film stack structure of claim 13, wherein the pinned layer, the coupling layer, and the reference layer 106 form a synthetic anti-parallel (SyAP) layer.

### Claim 15 (depends on 13)

The film stack structure of claim 13, wherein the composite hard mask is formed on the capping layer.

### Claim 16 (depends on 11)

A method of forming a MR sensor, comprising:
providing the film stack structure of claim 11.

### Claim 17 (depends on 16)

The method of claim 16, further comprising sequentially coating a bottom anti-reflective coating (BARC) and a photoresist layer on the composite hard mask.

### Claim 18 (depends on 17)

The method of claim 17, further comprising a MR junction photopatterning including patterning the photoresist layer and transferring a photoresist pattern through the BARC.

### Claim 19 (depends on 18)

The method of claim 18, further comprising patterning the first and second hard mask layers by dry reactive ion etching (RIE), ion beam etching (IBE), or a combination of both methods.

### Claim 20 (depends on 19)

The method of claim 19, further comprising forming a MR junction after patterning of the first and second hard sacrificial mask layers.

### Claim 21 (depends on 20)

The method of claim 20, wherein forming the MR junction includes ion beam etching (IBE) to pattern the MR junction.

### Claim 22 (depends on 21)

The method of claim 21, wherein ion beam etching (IBE) to pattern the MR junction stops between a seed layer and a capping layer of the film stack structure.

### Claim 23 (depends on 21)

The method of claim 21, wherein ion beam etching (IBE) to pattern the MR junction stops at or within a spacer or barrier layer of the film stack structure.

### Claim 24 (depends on 20)

The method of claim 20, further comprising depositing a layer of insulating material after forming the MR junction.

### Claim 25 (depends on 24)

The method of claim 24, further comprising ion beam etching (IBE) after depositing the layer of insulating material to open up sidewalls around the MR junction and expose the photoresist layer.

### Claim 26 (depends on 25)

The method of claim 25, further comprising removing the BARC and the photoresist layer.

### Claim 27 (depends on 26)

The method of claim 26, further comprising applying a chemical mechanical polishing (CMP) process to planarize a wafer surface after removing the BARC and the photoresist layer.

### Claim 28 (depends on 27)

The method of claim 27, wherein the first sacrificial hard mask layer is configured to serve as a CMP stop layer.

### Claim 29 (depends on 28)

The method of claim 28, further comprising applying an etch back process to remove the first sacrificial hard mask layer.