# US 2023/0258180 A1 · Screw compressor with multi-layered coating of the rotor screws

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0258180 A1
- Document ID: US20230258180A1
- Status: Published application
- Kind: A1
- Application number: 18/296,163
- Filed: 2023-04-05
- Published: 2023-08-17
- Earliest claimed: 2017-05-03
- Assignees: Kaeser Kompressoren SE
- Applicants: Kaeser Kompressoren SE
- Inventors: Andreas Foerster; Gerald Weih
- Web page: https://patentgrep.com/patent/US20230258180A1

## CPC

- F04C 18/16: with helical teeth, e.g. chevron-shaped, screw type {(for non-parallel axes of movement F04C18/48)}
- F04C 18/084: {Toothed wheels}
- F04C 27/009: {Shaft sealings specially adapted for pumps}
- F04C 2230/91: Coating
- F04C 2240/20: Rotors
- F04C 2240/30: Casings or housings
- F04C 2240/50: Bearings
- F05C 2225/08: Thermoplastics
- F05C 2253/18: Filler
- F04C: ROTARY-PISTON, OR OSCILLATING-PISTON, POSITIVE-DISPLACEMENT MACHINES FOR LIQUIDS (engines F03C); ROTARY-PISTON, OR OSCILLATING-PISTON, POSITIVE-DISPLACEMENT PUMPS
- F05C: INDEXING SCHEME RELATING TO MATERIALS, MATERIAL PROPERTIES OR MATERIAL CHARACTERISTICS FOR MACHINES, ENGINES OR PUMPS OTHER THAN NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES

## Abstract

The invention relates to a screw compressor comprising a compressor housing (11) having two rotor screws (1, 2) mounted axially parallel therein, which mesh with each other in a compression space (18), can be driven by a drive and are synchronized with each other in their rotational movement, wherein the rotor screws (1, 2) each have a single-part or multi-part base body (24) with two end faces (5a, 5b, 5c, 5d) and a profiled surface (12a, 12b) extending therebetween, and shaft ends (30) projecting beyond the end faces (5a, 5b, 5c, 5d), wherein at least the profiled surface (12a, 12b) is formed in multiple layers, comprising a first, inner layer (3) and a second, outer layer (4), wherein the first, inner layer (3) and the second, outer layer (4) both comprise or are formed from a thermoplastic synthetic material, wherein particles (25) or pores (32) supporting a running-in process are embedded in the second, outer layer (4) and the thermoplastic synthetic material defines a matrix for receiving the particles (25) or for forming the pores (32).

## Claims

### Claim 1

A screw compressor comprising:
a compressor housing;
two rotor screws mounted axially parallel in the compressor housing, the two rotor screws meshing with each other in a compression space and synchronized with each other in their rotational movement; and
a drive in communication with the two rotor screws to rotate the rotor screws;
wherein each rotor screw comprises a single-part or multi-part base body with two end faces and a profiled surface extending therebetween and shaft ends projecting beyond the end faces, each shaft end comprising a bearing seat and seal seats between the bearing seat and the end face;
wherein:
each profiled surface is coated with a first layer and the first layer is coated with a second layer, wherein the first layer and the second layer both comprise a thermoplastic synthetic material; and
each of the seal seats is coated with only the first layer; and
wherein particles or pores supporting a running-in process are embedded in the second layer and the thermoplastic synthetic material defines a matrix for receiving the particles or for forming the pores, respectively.

### Claim 2 (depends on 1)

The screw compressor of claim 1, wherein the thermoplastic synthetic material for forming the first layer and the second layer is a semi-crystalline high-performance thermoplastic synthetic material.

### Claim 3 (depends on 1)

The screw compressor of claim 1, wherein the first layer forms a substantially homogeneous coating and a corrosion protection layer.

### Claim 4 (depends on 1)

The screw compressor of claim 1, wherein:
the first layer comprises a first layer thickness of 5 μm to 50 μm; and
the second layer comprises a second layer thickness of 10 μm to 120 μm.

### Claim 5 (depends on 1)

The screw compressor of claim 1, wherein the screw compressor comprises an oil-free screw compressor.

### Claim 6

A method for applying a multilayer coating to surfaces of a rotor screw of a screw compressor, the method comprising:
applying a first layer of a first thermoplastic synthetic material to a profiled surface of the rotor screw, the rotor screw comprising a single-part or multi-part base body with two end faces and the profiled surface extending therebetween and shaft ends projecting beyond the end faces, each shaft end comprising a bearing seat and seal seats between the bearing seat and the end face;
coating the first layer of synthetic material on the profile surface with a second layer of a second thermoplastic synthetic material;
applying only the first layer of the first thermoplastic synthetic material to each of the seal seats of the rotor screw;
wherein particles or pores supporting a running-in process are embedded in the second layer and the second thermoplastic synthetic material defines a matrix for receiving the particles or for forming the pores, respectively.

### Claim 7 (depends on 6)

The method of claim 6, wherein the method further comprises applying a zirconium-based nanoceramic layer to the profiled surface and each of the seal seats before applying the first layer.

### Claim 8 (depends on 6)

The method of claim 6, wherein the method further comprises pretreating the profiled surface and each of the seal seats by degreasing the profiled surface and each of the seal seats, roughening the profiled surface and each of the seal seats, cleaning the profiled surface and each of the seal seats, or combinations thereof.

### Claim 9 (depends on 6)

The method of claim 6, wherein the method further comprises baking at least one of the first layer and the second layer to form a homogenous layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein baking the at least one of the first layer and the second layer comprise baking at least one of the first and second layer at a temperature of from about 360° C. to about 420° C.

### Claim 11

A screw compressor comprising:
a compressor housing;
two rotor screws mounted axially parallel in the compressor housing, the two rotor screws meshing with each other in a compression space and synchronized with each other in their rotational movement; and
a drive in communication with the two rotor screws to rotate the rotor screws;
wherein:
each profiled surface is coated with a first layer and the first layer is coated with a second layer, wherein the first layer and the second layer both comprise a thermoplastic synthetic material; and
each bearing seat is uncoated;
wherein particles or pores supporting a running-in process are embedded in the second layer and the thermoplastic synthetic material defines a matrix for receiving the particles or for forming the pores, respectively.

### Claim 12 (depends on 11)

The screw compressor of claim 11, wherein the thermoplastic synthetic material for forming the first layer and the second layer is a semi-crystalline high-performance thermoplastic synthetic material.

### Claim 13 (depends on 11)

The screw compressor of claim 11, wherein the first layer forms a substantially homogeneous coating and a corrosion protection layer.

### Claim 14 (depends on 11)

The screw compressor of claim 11, wherein:
the first layer comprises a first layer thickness of 5 μm to 50 μm; and
the second layer comprises a second layer thickness of 10 μm to 120 μm.

### Claim 15 (depends on 11)

The screw compressor of claim 11, wherein the screw compressor comprises an oil-free screw compressor.

### Claim 16

A method for applying a multilayer coating to surfaces of a rotor screw of a screw compressor, the method comprising:
applying a first layer of a first thermoplastic synthetic material to a profiled surface of the rotor screw, the rotor screw comprising a single-part or multi-part base body with two end faces and the profiled surface extending therebetween and shaft ends projecting beyond the end faces, each shaft end comprising a bearing seat and seal seats between the bearing seat and the end face;
coating the first layer of synthetic material on the profile surface with a second layer of a second thermoplastic synthetic material; and
maintaining each bearing seat uncoated by either the first layer or the second layer;
wherein particles or pores supporting a running-in process are embedded in the second layer and the second thermoplastic synthetic material defines a matrix for receiving the particles or for forming the pores, respectively.

### Claim 17 (depends on 16)

The method of claim 16, wherein the method further comprises applying a zirconium-based nanoceramic layer to the profiled surface and each of the seal seats before applying the first layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein the method further comprises pretreating the profiled surface and each of the seal seats by degreasing the profiled surface and each of the seal seats, roughening the profiled surface and each of the seal seats, cleaning the profiled surface and each of the seal seats, or combinations thereof.

### Claim 19 (depends on 16)

The method of claim 16, wherein the method further comprises baking at least one of the first layer and the second layer to form a homogenous layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein baking the at least one of the first layer and the second layer comprise baking at least one of the first and second layer at a temperature of from about 360° C. to about 420° C.