# US 2023/0257850 A1 · Novel Systems And Methods Of Reductive-Acid Leaching Of Spent Battery Electrodes To Recover Valuable Materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0257850 A1
- Document ID: US20230257850A1
- Status: Published application
- Kind: A1
- Application number: 18/014,257
- Filed: 2021-07-01
- Published: 2023-08-17
- Earliest claimed: 2020-07-01
- Assignees: Garrison Minerals, LLC
- Applicants: Garrison Minerals, LLC
- Inventors: Michael Girard Irish; Boris Andreevich Chubukov; Mac Garrison Mccreless; Aaron William Palumbo
- Web page: https://patentgrep.com/patent/US20230257850A1

## CPC

- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- C22B 26/12: Obtaining lithium
- C22B 47/0063: {with acids or salt solutions (C22B47/0072 takes precedence)}
- C25C 1/08: of nickel or cobalt
- C25C 1/24: Alloys obtained by cathodic reduction of all their ions
- C25C 7/04: Diaphragms; Spacing elements
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention describes systems and methods of a novel hydrometallurgical process to perform reductive-acid leaching and separation of constituent compounds from solid material generated from the electrodes of lithium-ion batteries, or other source material containing target high-value materials. The process method involves the initial reductive-acid leaching with sulfur dioxide and sulfuric acid of the source material which may be performed in a single or a multi-step embodiment. In a single-step embodiment, the reductive-acid leaching results in two outlet streams, a leachate solution and a bulk solid, such as graphite. In a two-step embodiment, a dilute reductive-acid leaching results in a lithium brine that may be bled as a product stream. The resulting liquor, or leachate, can be subjected to precipitation and oxidation steps to remove other compounds except, for example lithium, cobalt, and nickel. Electrowinning may then be used to separate and recover cobalt and nickel alloys among other high value compounds from a lithium brine.

## Claims

### Claim 1

A method of extracting metals comprising the steps:
depositing a first quantity of black mass derived from processed lithium-ion batteries in an acid-reduction reactor;
reductive-acid leaching said black mass through the introduction of an acid solution causing the production of:
a mother leachate containing a mixture of solubilized metals;
a quantity of bulk solid material;
increasing the pH of the mother leachate causing said solubilized metals to form metal hydroxides and further precipitating said metal hydroxides from the leachate;
oxidizing aqueous manganese (Mn) present in the leachate forming insoluble manganese dioxide (MnO2) and precipitating said MnO2 from the leachate;
electrowinning the leachate to form a quantity of cobalt/nickel alloy and extracting the cobalt/nickel alloy;
increasing the pH of the leachate precipitating cobalt, nickel and other trace metals remaining in the leachate as hydroxides;
generating a Lithium (Li) bleed stream; and
extracting said Li Brine from the bleed stream, or recycling said Li Brine back into said acid-reduction reactor with an additional quantity of black mass.

### Claim at position 2

2-61. (canceled)

### Claim 62

A method of extracting metal alloys from a source material comprising the steps:
depositing a first quantity of source material containing lithium, cobalt, nickel, manganese or graphite in an acid-reduction reactor;
reductive-acid leaching said source material through the introduction of an acid solution, wherein said acid-reduction reactor maintains a pH of at least 6, causing the production of a first Lithium (Li) brine to be further concentrated through additional application of reductive-acid leaching steps, and wherein said reductive-acid leaching said source material through the introduction of an acid solution causing the production of:
a mother leachate containing a mixture of solubilized metals;
a quantity of bulk solid material;
increasing the pH of the mother leachate causing said solubilized metals to form metal hydroxides and further precipitating said metal hydroxides from the leachate;
oxidizing aqueous manganese (Mn) present in the leachate forming insoluble manganese dioxide (MnO2) and precipitating said MnO2 from the leachate;
electrowinning the leachate to form a quantity of cobalt/nickel alloy and extracting the cobalt/nickel alloy;
increasing the pH of the leachate precipitating cobalt, nickel and other trace metals remaining in the leachate as hydroxides;
generating a Lithium (Li) bleed stream; and
extracting said Li Brine from the bleed stream, or recycling said Li Brine back into said acid-reduction reactor with an additional quantity of black mass.

### Claim at position 4

63-65. (canceled)

### Claim 66

A method of extracting metal from a feed material comprising the steps in order:
depositing a first quantity of nickel and/or cobalt rich feed material into an acid-reduction reactor;
reductive-acid leaching said feed through the introduction of an acid and reducing agent solution causing the production of:
a mother leachate containing a mixture of solubilized metals;
a quantity of bulk solid material;
increasing the pH of the mother leachate causing some of the impurity metals to form metal hydroxides and further separating said metal hydroxides from the leachate;
oxidizing aqueous manganese (Mn) present in the leachate forming insoluble manganese dioxide (MnO2) and separating said MnO2 from the leachate;
electrowinning the leachate to form a quantity of cobalt/nickel alloy and extracting the cobalt/nickel alloy;
increasing the pH of the leachate to precipitate and separate residual cobalt, nickel and other trace metals remaining from the leachate as hydroxides;
generating a lithium (Li) brine stream from the leachate

### Claim 67 (depends on 66)

The method of claim 66, wherein said acid and reducing agent solution comprises a solution of sulfur dioxide (SO2) and/or a solution sulfuric acid (H2SO4), and/or an acid solution generated by said electrowinning step.

### Claim 68 (depends on 66)

The method of claim 66, where the feed comprises black mass derived from lithium-ion batteries, a nickel or cobalt rich ore, a mixed hydroxide product (MHP), a raw or intermediate product containing nickel and/or cobalt, or a combination of the same.

### Claim 69 (depends on 66)

The method of claim 66, wherein said solubilized metals are selected from the group consisting of: lithium (Li), cobalt (Co), nickel (Ni), and manganese (Mn).

### Claim 70 (depends on 67)

The method of claim 67, wherein 0-2 mole of said SO2 is introduced into said acid-reduction reactor for each mole of Co, Ni and Mn in said feed.

### Claim 71 (depends on 66)

The method of claim 66, wherein acid-reduction reactor maintains a pH between 1-4 during leaching.

### Claim 72 (depends on 66)

The method of claim 66, further comprising the step of controlling the pH of the mother leachate by one or more of the following:
recycling downstream produced metal hydroxides to increase or maintain the pH in said acid-reduction reactor;
introducing a base compound to increase or maintain the pH in said acid-reduction reactor; and
introducing an acid compound to reduce the pH in said acid-reduction reactor; and
introducing an additional quantity of feed.

### Claim 73 (depends on 66)

The method of claim 66, wherein said step of increasing the pH of the mother leachate compromises increasing the pH of the leachate to between 4-7.

### Claim 74 (depends on 66)

The method of claim 66, wherein said step of oxidizing aqueous Mn is performed by an oxidant selected from the group consisting of: oxygen, air, SO2, ozone, permanganate, or a combination of the same.

### Claim 75 (depends on 66)

The method of claim 66, wherein the Mn remaining in said leachate after oxidation is less than 2 g/l but not less than 0.5 g/l.

### Claim 76 (depends on 66)

The method of claim 66, wherein said step of oxidizing aqueous Mn occurs prior to the step of precipitating said metal hydroxides from the leachate.

### Claim 77 (depends on 66)

The method of claim 66, wherein said step of electrowinning is performed in an electrowinning cell where a bag is configured to separate the anodes and cathodes to concentrate the acid generated at the anode, wherein the concentrated acid solution is recycled into said acid-reduction reactor.

### Claim 78 (depends on 66)

The method of claim 66, wherein the stream is recycled back into the process to concentrate said solubilized metals or change the leachate pH.

### Claim 79 (depends on 66)

The method of claim 66, further comprising a two-step reductive-acid leach of said feed, wherein said acid-reduction reactor maintains a pH of at least 6, causing selective leaching of lithium producing a second Li brine stream to be further concentrated through application of multiple reductive-acid leaching steps.

### Claim 80 (depends on 66)

The method of claim 66, further comprising the step of increasing the pH of the Li brine to precipitate remaining cobalt, nickel and other trace metals as hydroxides.

### Claim 81 (depends on 66)

The method of claim 66, wherein said quantity of bulk solid material comprises a quantity of graphite, silicon, and/or other non-solubilized material.

### Claim 82 (depends on 81)

The method of claim 81, further comprising the step of purifying said quantity of graphite.