# US 2023/0251574 A1 · Method to enhance lithography pattern creation using semiconductor stress film tuning

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0251574 A1
- Document ID: US20230251574A1
- Status: Published application
- Kind: A1
- Application number: 17/890,766
- Filed: 2022-08-18
- Published: 2023-08-10
- Earliest claimed: 2022-02-04
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Anthony R. SCHEPIS; Daniel J. FULFORD; Mark I. GARDNER; H. Jim FULFORD; Anton J. DEVILLIERS
- Web page: https://patentgrep.com/patent/US20230251574A1

## CPC

- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G01B 11/16: for measuring the deformation in a solid, e.g. optical strain gauge
- G03F 7/092: {characterised by backside coating or layers, by lubricating-slip layers or means, by oxygen barrier layers or by stripping-release layers or means}
- G03F 7/0957: {with sensitive layers on both sides of the substrate}
- G03F 7/16: Coating processes; Apparatus therefor (applying coatings to base materials in general B05; applying photosensitive compositions to base for photographic purposes G03C1/74)
- G03F 7/70483: {Information management; Active and passive control; Testing; Wafer monitoring, e.g. pattern monitoring}
- G03F 7/70783: {Handling stress or warp of chucks, masks or workpieces, e.g. to compensate for imaging errors or considerations related to warpage of masks or workpieces due to their own weight}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- G01B 11/306: {for measuring evenness}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Aspects of the present disclosure provide a method for optimizing wafer shape. For example, the method can include receiving a wafer having a working surface for one or more devices to be fabricated thereon and a backside surface opposite to the working surface, measuring the wafer to identify bow measurement of the wafer, and forming a first stress-modification film on the backside surface. The first stress-modification film can be reactive to a first wavelength of light in that exposure to the first wavelength of light modifies an internal stress of the first stress-modification film. The method can further include exposing the first stress-modification film to a pattern of the first wavelength of light to modify the internal stress of the first stress-modification film. The pattern of the first wavelength of light corresponds to the bow measurement.

## Claims

### Claim 1

A method, comprising:
receiving a wafer having a working surface for one or more devices to be fabricated thereon, and a backside surface opposite to the working surface;
measuring the wafer to identify bow measurement of the wafer;
forming a first stress-modification film on the backside surface, the first stress-modification film reactive to a first wavelength of light in that exposure to the first wavelength of light modifies an internal stress of the first stress-modification film; and
exposing the first stress-modification film to a pattern of the first wavelength of light to modify the internal stress of the first stress-modification film, the pattern of the first wavelength of light corresponding to the bow measurement.

### Claim 2 (depends on 1)

The method of claim 1, wherein measuring the wafer to identify bow measurement of the wafer is performed prior to forming a first stress-modification film.

### Claim 3 (depends on 1)

The method of claim 1, wherein measuring the wafer to identify bow measurement of the wafer is performed subsequent to forming a first stress-modification film.

### Claim 4 (depends on 1)

The method of claim 1, wherein the working surface of the wafer is with one or more devices fabricated thereon, and the method further comprises:
forming a protection layer on the working surface of the wafer to protect the devices.

### Claim 5 (depends on 4)

The method of claim 4, wherein measuring the wafer to identify bow measurement of the wafer is performed subsequent to forming a protection layer.

### Claim 6 (depends on 4)

The method of claim 4, wherein measuring the wafer to identify bow measurement of the wafer is performed prior to forming a protection layer.

### Claim 7 (depends on 4)

The method of claim 4, wherein the wafer is flipped so that the protection layer is in contact with a wafer chuck when the first stress-modification film is formed.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
executing one or more lithographic patterning processes on the working surface of the wafer.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
removing the first stress-modification film after the lithographic patterning processes are executed.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first stress-modification film is formed while the wafer is held at a periphery.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
forming a second stress-modification film on the first stress-modification film, the second stress-modification film reactive to a second wavelength of light in that exposure to the second wavelength of light modifies an internal stress of the second stress-modification film; and
exposing the second stress-modification film to a pattern of the second wavelength of light to modify the internal stress of the second stress-modification film, the pattern of the second wavelength of light corresponding to the bow measurement.

### Claim 12 (depends on 11)

The method of claim 11, wherein measuring the wafer to identify bow measurement of the wafer is performed subsequent to forming a second stress-modification film.

### Claim 13 (depends on 1)

The method of claim 1, further comprising:
forming a stress film on the backside surface of the wafer,
wherein forming a first stress-modification film on the backside surface includes forming a first stress-modification film on the stress film.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
removing a portion of the stress film; and
replacing the removed portion with a stress layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein the stress layer has a different stress type form the stress film.

### Claim 16

A system, comprising:
a bow measurement device configured to measure a wafer to identify bow measurement of the wafer, the wafer having a working surface for one or more devices to be fabricated thereon, and a backside surface opposite to the working surface;
a stress-modification film formation device configured to form a first stress-modification film and a second stress-modification film, the first stress-modification film and the second stress-modification film reactive to first and second wavelengths of light, respectively, such that exposure to the first and second wavelengths of light modifies internal stresses of the first stress-modification film and the second stress-modification film, respectively;
a light generator configured to generate patterns of first and second wavelengths of light; and
a controller coupled to the bow measurement device, the stress-modification film formation device and the light generator, the controller configured to control the bow measurement device to measure the wafer to identify the bow measurement of the wafer, control the stress-modification film formation device to form the first stress-modification film and the second stress-modification film on the backside surface of the wafer sequentially, and control the light generator to generate and apply the pattern of first wavelength of light onto the first stress-modification film and/or the pattern of second wavelength of light onto the second stress-modification film, the pattern of first wavelength of light and the pattern of second wavelength of light corresponding to the bow measurement.

### Claim 17 (depends on 16)

The system of claim 16, further comprising:
a lithographic module coupled to the controller, the lithographic module configured to be controlled by the controller to:
form a stress film on the backside surface of the wafer;
remove a portion of the stress film; and
replace the removed portion of the stress film with a stress layer.

### Claim 18 (depends on 17)

The system of claim 17, wherein the stress layer has a different stress type from the stress film.

### Claim 19 (depends on 17)

The system of claim 17, wherein the controller is configured to control the stress-modification film formation device to form the first stress-modification film or the first and second stress-modification films on the stress film.

### Claim 20 (depends on 16)

The system of claim 16, wherein the controller is configured to first control the stress-modification film formation device to form the first stress-modification film or the first and second stress-modification films on the backside surface of the wafer and then control the bow measurement device to measure the wafer to identify the bow measurement of the wafer.